sodium acetate electrolysis
Is it possible to electrolyse anhydrous sodium acetate in a copper crucible? My friend gave me some sodium but it is almost gone. I dont want to mess
w/ molten NaOH. Sodium acetate melts @ =/= 330 C and is easily obtained.
|
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
and it decomposes at a slightly higher temperature, giving mostly sodium carbonate.
|
|
|
octave
Harmless
Posts: 39
Registered: 4-11-2007
Member Is Offline
Mood: Working.
|
|
Would it be possible to form sodium oxide also as a byproduct?
|
|
|
nodrog19
Harmless
Posts: 38
Registered: 29-5-2008
Member Is Offline
Mood: No Mood
|
|
I didnt realize you could melt lye over an alcohol burner, so thats how Ill do it.
|
|
|
raiden
Harmless
Posts: 38
Registered: 4-2-2008
Member Is Offline
Mood: Curious
|
|
| Quote: | Originally posted by nodrog19
I didnt realize you could melt lye over an alcohol burner, so thats how Ill do it. |
Be careful, hot lye will eat through pretty much anything.
|
|
|
nodrog19
Harmless
Posts: 38
Registered: 29-5-2008
Member Is Offline
Mood: No Mood
|
|
now you tell me!!
just kidding.
why would it turn blue?
|
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
iron or steel contains work with NaOH, especially if you add a few percent Na2CO3.
|
|
|