madbee
Harmless
Posts: 2
Registered: 17-11-2003
Location: europa
Member Is Offline
Mood: No Mood
|
|
Another metal of Palladium
Hi,
Exist there for a catalysis of hydrogenation another metal with the characteristics of palladium even if other metals do not generate as much
hydrogen
The Tungsten can it replace it! Or gold, silver,or other ?
Regards.
|
|
|
vulture
Forum Gatekeeper
   
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Raney nickel?
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
|
unionised
International Hazard
   
Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
It depends what you want to do.
Ni is a fairly good hydrogenation catalyst.
|
|
|
Organikum
resurrected
   
Posts: 2344
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
Nickel can be made a hell of a hydrogenation catalyst - all sugar reductions for example are done with those. Just heating precipated Ni at 800°C
under a stream of hydrogen is fairly out of reach I fear.
There had been rumors on tungstencarbide having similar properties to Pd/Pt, but I never heard something on this again.
Catalytic hydrogenation is art. This is by no way easy to do - with or without pressure.
|
|
|
madbee
Harmless
Posts: 2
Registered: 17-11-2003
Location: europa
Member Is Offline
Mood: No Mood
|
|
Hum... . .
Thank you for all information I will look at the track of the tungstencarbide !
|
|
|
If_6_was_9
Unregistered
Posts: N/A
Registered: N/A
Member Is Offline
|
|
See
http://www.geocities.com/dritte123/Nipat.html
http://www.geocities.com/dritte123/PSPF.html
|
|
|