I'm a beginning chemist and I'm interested in the best way to extract calcium carbonate from eggshells. My current method is to clean out the egg
gunk inside the eggs by hand, stick the eggshells in the toaster oven for a few minutes, then grind them up in a mortar and pestle. This method works
fine except for removing the egg gunk by hand which is really a pain and probably not very efficient. I'm wonder if anyone here can suggest a better
method to remove the egg gunk, maybe a solvent that doesn't dissolve the egg shells? Also, I know it is possible to by calcium carbonate over the
counter, but at the moment I'm interested in what useful chemicals I can make for free from things most people have at home.
EDIT: Hints as to how I could figure this out myself are also appreciated.
Thanks in advance,
-javagamer
[Edited on 25-9-2008 by javagamer]
|
|
Magpie
lab constructor
   
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Perhaps you could burn out the organic matter. My wife says that our self-cleaning oven literature claims it gets to 875F (468C). Probably would
leave some carbon residue, however.
Or you could dissolve the CaCO3 in an acid (HCl) , filter saving the filtrate, then neutralize with baking soda. Then add further CO2 from a bubbler
using vinegar and baking soda. This should precipitate out fairly pure CaCO3.
[Edited on 25-9-2008 by Magpie]
|
|
javagamer
Harmless
Posts: 22
Registered: 25-9-2008
Member Is Offline
Mood: No Mood
|
|
I read somewhere that CaCO3 dissolves in vinegar, but I heard elsewhere that it reacts with vinegar and I'll be left with something else. Can someone
clear this up for me?
|
|
bfesser
Resident Wikipedian
   
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
CaCO<sub>3</sub>(s) + 2 CH<sub>3</sub>COOH(aq.) -> Ca(CH<sub>3</sub>COO)<sub>2</sub>(aq.) +
H<sub>2</sub>O(l) + CO<sub>2</sub>(g)
Calcium carbonate (base) reacts with the acetic acid in vinegar to form calcium acetate, water, and carbon dioxide. It's an acid-base reaction.
Google/Wiki it.
[Edited on 9/25/08 by bfesser]
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
CaCO3 (solid) + 2 AcOH (liq) => Ca(OAc)2 (in solution) + CO2 (gas)
So vinegar dissolves CaCO3 by reactive with it. If an inorganic carbonate is insoluble in water then generally anything that dissolves it does so by
reacting with it.
Heating the shells to 500-600 C in air will remove the organics, CaCO3 doesn't break down very fast below 800C, but there's other stuff than just
CaCO3 in the shells. If you calcine the shells like that, then grind them, finally soaking them in colddistilled/deionised water for a hour so so and
pour off the water - repeat several times - you'll get pretty pure CaCO3. Magnesium and phosphate are the major impurities, followed by sodium,
potassium. Washing with water will remove the Na, K, and some Mg.
Attachment: Elemental and Ultrastructural Analysis of the Eggshell.pdf (634kB) This file has been downloaded 1176 times
|
|
bfesser
Resident Wikipedian
   
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
not_important, your equation is not_balanced.
|
|
javagamer
Harmless
Posts: 22
Registered: 25-9-2008
Member Is Offline
Mood: No Mood
|
|
not_important: Doesn't calcium carbonate react with water? I heard a simple qualitative way to check whether you have calcium carbonate or calcium
oxide is to add a little to water, the more bubbles you get the more calcium carbonate you have.
|
|
chemkid
Hazard to Others
 
Posts: 269
Registered: 5-4-2007
Location: Suburban Hell
Member Is Offline
Mood: polarized
|
|
That is not true. Calcium carbonate does not react with water. CaO reacts with water however there should be no effervescence (bubbling):
CaO + H2O --> Ca(OH)2
This is true of most alkali and alkali earth oxides.
Calcium carbonate will effervesce with acid. But calcium carbonate is not a base in some regards. This has to do with the different theories of acids
and bases. (Bronsted, Lewis etc.)
All carbonates (or a lot of them) react like this:
H+ + CO3(2-) --> H2CO3
H2CO3 dissociates....
H2CO3 --> H20(aq) + CO2 (g)
The carbon dioxide is insoluble and comes off as a gas.
Chemkid
[Edited on 27-9-2008 by chemkid]
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
What chemkid said. Adding CaO to a not too large excess of water will boil the excess water. Calcium carbonate just sits there. Egg and sea shells
are mostly calcium carbonate, as is coral and marble rock; if it was very reactive rain would make some building and statues interesting to be around,
and imagine the ocean if CaCO3 reacted with plain water to give CO2.
|
|
kclo4
National Hazard
  
Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline
Mood: No Mood
|
|
Quote: | I know it is possible to by calcium carbonate over the counter, but at the moment I'm interested in what useful chemicals I can make for free from
things most people have at home. |
Chalk is a pretty good source of Calcium Carbonate. Most people have this at home also. 
just so you know
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
While many people may have 'chalk' at home, they may may not have calcium carbonate. Children's and blackboard chalk is often gypsum in part or
whole, other 'chalks' can be talc or magnesium carbonate. Be sure to test you chalk before attempting to do a demonstration of the reaction of chalk
and acid, it can be a bit embarrassing to add the acid and just have the mixture sit there inertly.
[Edited on 28-9-2008 by not_important]
|
|