Schwerter's solution


I mixed up a small batch from a recipe I found laying about : 20 grains potassium dichromate dissolved in 30 mL 35% nitric acid. The K2Cr2O7 is from an ebay source, the acid is AR from Allworld Scientific, the water is distilled water from the grocery store.

I'm trying to figure out how I'm misusing it. I should get a bright to dark red glob with a similar stain on fine, sterling, and coin silver.

I get a red to almost brown drop on all silver samples used, and the stain is white on .999 and sterling, and grey on coin. How should the drop be removed to inspect the stain?

I found it odd that measurement types are mixed (english with metric). Should I have K2Cr2O7 in the solution?
View user's profile View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 858
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 13-4-2010 at 14:10


What you have in solution is potassium trichromate in equillibrium with potassium dichromate.

Am I answering your question? Your post seems a little vague, what exactly are you asking for?
View user's profile View All Posts By User
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 13-4-2010 at 19:31


What is Schwerter's solution ?
See Silver testing , here _
http://en.wikipedia.org/wiki/Potassium_dichromate

How to
http://shorinternational.com/TestGoldMakeSolution.htm
http://www.lacywest.com/t_goldt.htm
http://www.testforsilver.com/index.php?main_page=product_inf...

Schwerter's solution indications
Brass - Dark Brown
Copper - Brown
Nickel - Blue
Palladium - None
Gold - None
- Silver Pure - Bright Red
- Silver .925 - Dark Red
- Silver .800 - Brown
- Silver .500 - Green
Lead - Yellow
Tin - Yellow

_________

@ ldanielrosa

" the acid is AR "
Aqua Regia is Nitric acid plus Hydrochloric acid
Schwerter's is made only with Nitric acid and Dichromate.

Perhaps Lambda-Eyde can say now why your .999 silver
( if you are certain that's what it is ) turns white.
For the same reason coins will turn grey since they are less pure.

" K2Cr2O7 is from an ebay source "
so what is the assay of what purports to be K2Cr2O7 ?

.
View user's profile View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 13-4-2010 at 19:43


Quote: Originally posted by franklyn  

" the acid is AR "
Aqua Regia is Nitric acid plus Hydrochloric acid
Schwerter's is made only with Nitric acid and Dichromate.


AR = analytical reagent

You don't buy aqua regia since it degrades, so I can only image the above is what the OP means.

I'd just dab the drop off with paper towel. nothing fancy.




Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
ldanielrosa
Hazard to Others
***




Posts: 124
Registered: 25-4-2007
Member Is Offline

Mood: transparent

[*] posted on 14-4-2010 at 02:27


" Should I have K2Cr2O7 in the solution?" Sorry, I was thinking ahead of the typing. I meant should I have _more_ in the solution.

Yes, analytical reagent. The store carried this, but not technical grade so it was less expensive.

I'll try dabbing it next time, thanks.
View user's profile View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 14-4-2010 at 19:45


Nitric and K2Cr2O7:

http://en.wikipedia.org/w/index.php?title=Special%3ASearch&a...

Didn't anyone do any research on this? See also:

http://survivetheflu.tripod.com/moneywise/id51.html

for the procedure

[Edited on 15-4-2010 by chemrox]




"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User

  Go To Top