[*] posted on 9-6-2010 at 08:50
NHN


Would anyone here care to share an opinion concerning the possible use of Nickel Hydrazinium Nitrate (NHN) in so called bullet hit squibs, used in the movie sfx ?
The lack of sensitivity to shock and friction of this compound would definitly be a bonus.
Through my work as film armourer, I am in frequent practical contact with movie special effects operations; A "squib" with a lower sensitivity than the usual primaries will make some movie set workers happier.
Your learned comments wellcome.
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 831
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 11-6-2010 at 10:02


They might be safer from an energetic materials standpoint, but the question is whether the released cloud of nickel would pose a problem. Nickel is after all a known allergen, so it may not be a good idea to inhale it in dust form.
View user's profile View All Posts By User
mnick12
Hazard to Others
***




Posts: 404
Registered: 30-12-2009
Location: In the lab w/ Dr. Evil
Member Is Offline

Mood: devious

[*] posted on 11-6-2010 at 13:39


Well I did not know it was a allergen, but Nickel is a known carcinogen.
I think there is a thread that talks about nickel hydrazine nitrate here it is http://www.sciencemadness.org/talk/viewthread.php?tid=1778 hope that helps
View user's profile View All Posts By User