Jango
Harmless
Posts: 7
Registered: 23-11-2010
Location: Oxfordshire, England
Member Is Offline
Mood: No Mood
|
|
Electrilysis of Iron(III) Chloride?
If I electrolysed Iron(III) Chloride solution, what would I get at the anode and cathode?
I guess I would get Fe at the cathode and Cl2 at the anode, but I'm not sure if Fe is too reactive to be made at the cathode. What about Zinc Chloride
as well? Would I make Zn at the cathode?
|
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Hmmm imagine what if I were to Google "iron plating" or "zinc plating", what might I learn?
|
|
|
cyanureeves
National Hazard
  
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
what will you use for anode?if you use silver youll get silver chloride in your solution. it will look like milk.maybe youll get fe just in your
solution as well and some form of fe on cathode.you ought to try it.it could be a coolway to galvanize with zinc.either way youll definitely get cl
for sure.i could never get the zinc to stick permanently on cathode with home made zinc chloride made with hcl. i havent tried nitrating zinc then
adding nacl to see if i can get zinc chloride that way.
|
|
|
Jango
Harmless
Posts: 7
Registered: 23-11-2010
Location: Oxfordshire, England
Member Is Offline
Mood: No Mood
|
|
Thanks for your replies, and yes, I did check Google first, but I didn't get any good answers...
I was thinking of using an iron or graphite cathode for both, and a graphite anode of course.
|
|
|
12AX7
Post Harlot
   
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Fe or Fe(II) will form at the cathode, the latter particularly at low voltages.
Speaking of iron plating, does anyone know which additives create a flat, smooth deposit?
Tim
|
|
|
cyanureeves
National Hazard
  
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
hey jango. it can be done. i just read a patent that said a ferrous salt can be used along with boric acid.yep!cockroach killer boric acid. except it
says to use iron anode.
|
|
|