Author: Subject: Odd behaviour of a pickling gel
Panache
International Hazard
*****




Posts: 1248
Registered: 18-10-2007
Member Is Offline

Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein

[*] posted on 9-2-2021 at 04:23
Odd behaviour of a pickling gel


So i was at friend house. He had some Avesta Classic Pickling gel 122 (un2922).
I asked for some, he obliged and decanted some into a glass coke bottle. I got home and put it on the shelf.
Fast forward a few months and my friend gives me.the remainder in the original packaging as he has no.use for it. I go to recombine the two portions and.in the coke botttle.the cloudy pickle has clarified and some rather large very clear and colourless crystals have grown.
The pickle is 20% nitric, 2-5%HF
Any ideas?

20210209_232144.jpg - 518kB 20210209_232120.jpg - 423kB
View user's profile View All Posts By User
UC235
International Hazard
*****




Posts: 531
Registered: 28-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 9-2-2021 at 17:09


Well, mistake #1 was putting HF in glass.

More directly related is that since it's a gel, it clearly contains things aside from HF and HNO3 that could be forming the crystals.
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1189
Registered: 2-8-2018
Member Is Offline


[*] posted on 9-2-2021 at 23:42


The gel probably absorbed the silicon fluoride and solidified to a degree