Well, HCl/H2O2 will sure dissolve Platinum, but the reaction doesn't seem to be very robust.
The H2O2 liberates Chlorine, but the H2O2 needs constant replacement, as Platinum decomposes it.
Folks sometimes use the process to dissolve finely divided spent catalysts, or to leech the Platinum out of Platinized Carbon.
For dissolving Chunks of Platinum, perhaps messy Aqua Regia is the was to go. It's something I have to do soon, and I lack enthusiasm. Clouds of
toxic red gas.... Yuk! Still, it does produce the product I need, straightaway, and in its pure form. Chloroplatinic acid.
Thought Electrolysis with HCl might also work. Or, reaction with elemental Chlorine.... But, each has its drawbacks, and Aqua Regia is tried and
true. Additionally, Nurdrage has provided a decent Youtube video.
Oh yeah, Gold? Gold is easier. Some of the More Arcane Precious Metals, aren't touched by any reagent we have discussed. You can fuse them with
Molten Alkali Salts though.
Well, I can't provide a link. This odd Southern guy, does interesting work, but perhaps he has rubbed Youtube, the wrong way. One day, you are a
star.... The next day, you are gone.
[Edited on 27-2-2021 by zed]
|
|
|
Panache
International Hazard
   
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
I find aqua regia dissolution of precious metals are best performed using a behive type setup. Basically your metal and aqua regia are in a beaker.
This has a larger inverted beaker on top. Both sitting in a tray with water...
[Edited on 28-2-2021 by Panache]
|
|
|
ChemTalk
Hazard to Self

Posts: 65
Registered: 13-12-2018
Location: United States
Member Is Offline
Mood: colloidal
|
|
>> This odd Southern guy, does interesting work, but perhaps he has rubbed Youtube, the wrong way. One day, you are a star.... The next day, you
are gone
Who was that?
|
|
|
Panache
International Hazard
   
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
Quote: Originally posted by Panache  | Quote: Originally posted by Lion850  | | Concentrated HCl with I2 dissolved in it dissolves gallium (fast!) and also tin (slower, but faster than HCl on its own). If I had a bit of gold to
spare I would try, but I don't have. |
So i just tried straight i2 ar rt with gold...no reaction. Sealed the tube and heated no reaction. I reacon addinghcl will do sweet fa.
Illletyou know |
Ahh yeah i was completely wrong...no metallic gold.
So iodine and hcl most definitely dissolves gold.
|
|
|
zed
International Hazard
   
Posts: 2312
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
So, Panache. You are suggesting to place this project in a shallow pan of water... and to heat the whole thing? One large beaker, inverted over a
smaller beaker containing Aqua Regia and Metal?
Thereby, trapping the noxious fumes, in the water bath?
I like the simplicity.
|
|
|
Lion850
National Hazard
  
Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline
Mood: Great
|
|
Quoting Panache:
Ahh yeah i was completely wrong...no metallic gold.
So iodine and hcl most definitely dissolves gold.
Unquote
Hi Panache very interesting, can you please give more details? Did the gold go into solution with no ppt? Gold monoiodide is yellow-greenish according
to Wikipedia; did you see these colors? Do you know the weights of reagents involved?
|
|
|
zed
International Hazard
   
Posts: 2312
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Alright, that Precious Metals poster, is still on Youtube. Not excluded.... yet. And, maybe he isn't a Southern Guy.
Not Gold, but a very interesting procedure. Fusion of Platinum Group metals, in molten Alkali. Precipitation via Barium Salt.
https://www.youtube.com/watch?v=gV2N2Jqpo6w
[Edited on 2-3-2021 by zed]
|
|
|
Panache
International Hazard
   
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
Firstly zed, yes it's fantastic, you can even use your kitchen sink as the pan of water and run a constant water stream down the drain. I once did a
larger one in a 20L pp bucket, over the bucket i had a shallow wider bucket and then over this a towel and the entire thing ran under the shower, once
they get bigger they really don't need any heating.
And lion 850, ahh you're australian.
So i grabbed i guess enough gold plated pins to cover the bottom of a 50ml beaker, i then added i guess about quarter this volume in iodine. The pins
were very fine. i then sealed the top with some silicon film and warmed the underside melting the iodine. not much happen. I let it cool and added
some hcl conc. It began working upon the copper (the pins were gold plated over copper) but i saw no attack of any gold surfac. After about 30minutes
i got bored left it for three days snd then when i looked again there was no gold left on any of the pins but srangely there were pins left, well
partly.
I rinsed them well to ensure that the observation was correct.
And yes absolutely a ppt had formed and it was yellowish green. i haven't filterred it yet, prtobably wont. as it would also contain copper nickel al
compounds also.
With this Au(!) iodide, does it dissolve other metals liberating gold netal?
|
|
|
pneumatician
Hazard to Others
 
Posts: 416
Registered: 27-5-2013
Location: Magonia
Member Is Offline
Mood: ■■■■■■■■■■ INRI ■■■■■■■■■■ ** Igne Natura Renovatur Integra **
|
|
if you know how, with only HCL, Gold CAN BE dissolved. PERIOD ;-)
|
|
|
Panache
International Hazard
   
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
ok, ill bite, what do you know? I find it difficult to believe you need only hcl, i mean one would need at least a beaker and water (because HCL is a
gas at stp.....)
|
|
|
pneumatician
Hazard to Others
 
Posts: 416
Registered: 27-5-2013
Location: Magonia
Member Is Offline
Mood: ■■■■■■■■■■ INRI ■■■■■■■■■■ ** Igne Natura Renovatur Integra **
|
|
Quote: Originally posted by Panache  |
ok, ill bite, what do you know? I find it difficult to believe you need only hcl, i mean one would need at least a beaker and water (because HCL is a
gas at stp.....)
|
oh yes, period, I asume you are right... of course you need a table, a pair of hands, a bottle to contain the hcl, a company producing hcl if you not
make your own and etc etc etc ad infinitum, ok? right? but the point here is Gold dissolved with only hcl, in water or gas, in a beaker and etc etc
etc, ok? right? :-D
ok, after all this ironic mumbo-jumbo... what is Gold?
ok, right, a metal, produced in the big bang, star dust and more and more mumbo-jumbo...
Stop! Gold is a COMPACT BODY, right?
so, et dividant dissolvere, I need to say ironic free something more??
in some thread here a guy "dissolved" Gold with chlorine only.
Sapere aude!
|
|
|
clearly_not_atara
International Hazard
   
Posts: 2912
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
possibility #979831: gold in hydrochloric acid, ozone generator bubbles (slowest possible method)
|
|
|
pneumatician
Hazard to Others
 
Posts: 416
Registered: 27-5-2013
Location: Magonia
Member Is Offline
Mood: ■■■■■■■■■■ INRI ■■■■■■■■■■ ** Igne Natura Renovatur Integra **
|
|
With ONLY HCL, no more, no less!
https://www.youtube.com/watch?v=oevJf2aYHjo
|
|
|
clearly_not_atara
International Hazard
   
Posts: 2912
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
^my post wasn't responding to you so much as providing a humorous way to dissolve gold, but, what I would suppose is, you can dissolve Au in "pure"
hydrochloric acid (HCl@H2O) using a membrane-cell setup (no membrane likely = gold all over cathode), but this isn't actually simple to set up in
practice
|
|
|
densest
Hazard to Others
 
Posts: 359
Registered: 1-10-2005
Location: in the lehr
Member Is Offline
Mood: slowly warming to strain point
|
|
(4) works quite well. Here, 35% H2O2 is (relatively) inexpensive and is used in gallons for swimming pool treatment. Swimming pool chlorinator tablets
Trichloro-S-Triazinetrione are a good chlorine source.The reaction seems to work at near neutral pH.
I tried various methods without HNO3 in order to simplify subsequent reduction. Also 35%H2O2 was -much- easier to obtain OTC locally with no hazmat
shipping.
Want to be Auric Goldfinger? (Ian Fleming reference) Spill a beaker of aqua regia + gold on your hands. Instant Purple of Cassius! I got to the sink
before the acid did any significant damage, but the gold precipitated in my skin -instantly-. Lasted for weeks.
Another reaction with H2O2 and gold plated copper: H2O2 and CH3COOH happily dissolve copper and leave gold behind. 3% H2O2 and 5% acetic acid work
albeit slowly leaving pretty blue-green cupric acetate and little gold flakes.
|
|
|