In2O very easy preparation method.


Hi. Today i made indium(I) oxide from indium (III) oxalate. I dont have high quality photos, because i used very small amount of compound. But it is interesting and also very simple reaction. Oxide in photo looks black, but actually it is nice brown powder.

received_4311021075593163.jpeg - 239kB received_2946833505559367.jpeg - 239kB




View user's profile View All Posts By User