This part came out of a Haake Rheometer. As far I can see it’s a single Machined aluminium part but with three really distinctly different
surfaces, I’ve photographed the two surfaces that are unique (the third being being what is just common al machined surface.
The shiny one almost appears like an applied foil and the darker grey one is very thick.
Does anyone have an insight into these surfaces?
|
|
|
Fulmen
International Hazard
   
Posts: 1800
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
The shiny surface looks like regular machined aluminum to me, possibly anodized. The dark one could be anything but I'm guessing some sort of paint.
We're not banging rocks together here. We know how to put a man back together.
|
|
|
wg48temp9
National Hazard
  
Posts: 789
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
It looks like a casting. The grey coloured surface looks like an as cast surface meaning no treatment or coating.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
|
Mateo_swe
National Hazard
  
Posts: 591
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
I would also guess a casted part that were machined on a lathe.
If one zooms in on the rim of the shiny top surface (not the bottom widest flange), one can see the tool markings left from each turn on the lathe.
Aluminium parts sometimes are anodized but i would guess its just bare aluminium surfaces where its shiny.
If the shiny parts were anodized i dont think you would see the faint tool markings, also anodized surfaces looks great but every scratch made after
anodization is highly visible.
|
|
|