metalresearcher
National Hazard
  
Posts: 819
Registered: 7-9-2010
Member Is Offline
Mood: Reactive
|
|
Make Phosphorus from Ca phosphate and Mg powder ?
The topic about the guy "Kobold vor NH4" who got burns on his arm with an attempt making phosphorus using phosphate with magnesium powder triggered me
to verify whether it is possible to make P4 using phosphate and Mg powder. I have Ca phosphate and Mg powder.
Reaction which I expect: Ca3(PO4)2 + 5 Mg => 3 CaO + 5 MgO
310 121
The ratio should be 310 : 121. So I mixed 3.1 g phosphate with 1.2g Mg powder and set fire to about 1g of the mixture with a burner. It reacted slowly
and not sustainable (I had to keep the burner to heat the mixture). Indeed the bright yellow flames billowing white P2O5 smoke appeared.
Then I put another gram in a test tube with a stopper and a glass tube into water. Just above the surface to avoid suckback.
When heating, red color appeared in the bottom of the test tube and smoke (P4 vapor + P2O5 ?) appeared in the tube and got into the water.
Then I added the rest of the mixture and it reacted again upon heating.
The reddish color appears to be not only red glow, but also the red calcium color.
Conclusion: P4 can be made this way with a more robust distillation kit (e.g. stainless steel tubes) and no violent reactions took place. I used
gloves as I was prepared for a similar event as "Kobold vor NH4" experienced, but it did not happen.
Video: https://www.metallab.net/jwplayer/video.php?f=/forums/Calciu...
|
|
|
papaya
National Hazard
  
Posts: 615
Registered: 4-4-2013
Member Is Offline
Mood: reactive
|
|
Look what I've found !
Sodium tripolyphosphate + MgAL:
https://www.youtube.com/watch?v=kCA7Ne24cm4
Also many different things are possible like with borax: https://www.youtube.com/watch?v=3IAv6Ohjuh8
Carbonates :https://www.youtube.com/watch?v=3n8Cgl_deEM
As one can see under right conditions all of them can react self-sustainingly, when thermodynamics are favorable of coarse.
|
|
|
simply RED
Hazard to Others
 
Posts: 209
Registered: 18-8-2005
Location: noitacoL
Member Is Offline
Mood: booM
|
|
Be careful with those things, accidental phosphide and phosphine poisoning may occur.
When logic and proportion have fallen sloppy dead...
|
|
|
Kobold vor NH4
Hazard to Self

Posts: 56
Registered: 27-8-2019
Location: The sewer underneath your house
Member Is Offline
|
|
Hmm I speculate that it did not react as mine did because the Mg had to replace the Ca from the molecule, maybe that is less exothermic compared to
the magnesium already being attached and ready to "fly off" once the other oxygen is removed. Maybe. I should calculate it to make sure though.
|
|
|
zed
International Hazard
   
Posts: 2312
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
This is unlikely to produce elemental Phosphorus.
But, if it actually does.... Please post in the Phosphorus Link, in General Chemistry.
|
|
|
Kobold vor NH4
Hazard to Self

Posts: 56
Registered: 27-8-2019
Location: The sewer underneath your house
Member Is Offline
|
|
Why do you say that zed? I may try a variation of metalresearcher's experiment, A.K.A using Ca3(PO4)2 instead of decomposing H2NH4PO4. Maybe even a
metal that is lower on the reactivity series might work better, such as Cu or Fe phosphate with aluminium powder
"I don't need no excuse for being what I am"
-----Frank Zappa
|
|
|
BJ68
Hazard to Others
 
Posts: 118
Registered: 12-3-2012
Member Is Offline
Mood: No Mood
|
|
Other way:
" A. R o s s e 1 und L. F r an k: Darstellung von Phosphor
aus den Phosphaten der Alkalien und alkalischen Erden mittels
Aluminium als Reductionsmittel und Einwirkung des Aluminiums auf Sulfate und Chloride"
https://zenodo.org/record/1425728/files/article.pdf
Attention: If there is calcium sulfate in the mixture, it will explode....
Bj68
|
|
|
PirateDocBrown
National Hazard
  
Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline
Mood: No Mood
|
|
The more hydrogen, the more phosphine. Dry your reagents out.