Dissolving Uranium metal in nitric acid.


Hello! today I made some uranyl nitrate. I just dissolved the metal in conc. nitric acid. because I made a small amount (<2g), I made a reaction in the vial. Here are videos&photos. (unfortunately, I couldn't upload the video here. If you want you can watch the dissolving process here.



IMG-2336.jpg - 1.4MB

IMG-2338.jpg - 1.6MB




View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 27-9-2022 at 06:21


longer video:
https://www.youtube.com/shorts/Cl5I_udG25c