Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Cesium hexafluorozirconate - Cs2[ZrF6]
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 12-10-2022 at 07:45
Cesium hexafluorozirconate - Cs2[ZrF6]


Hello! I made cesium hexafluorozirconate. first, I started with zirconium metal. I was surprised because it dissolved very easily in hydrofluoric acid(conc.). the reaction was fast like the Al&HCl reaction.

I made a reaction in 50ml PP plastic test tube. also, I put this test tube in water, because the reaction was very exothermic. then I added a solution of cesium sulfate tetrahydrate. nothing happened, I think because the solution was hot. then I put this test tube in the freezer. after 10-15 minutes I saw a white precipitate. then I filtered it and washed it with distilled water several times.

here is the result:
IMG-2609.jpg - 2.3MB

[Edited on 12-10-2022 by vano]




View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1931
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 14-10-2022 at 09:11


Have you analysed the product and what was the yield? The reason I ask is that zirconium is one of the metals to form very stable complexes with sulphate ions and these complexes mask some of the reaction of zirconium. You should check the stability values for zirconium and fluoride verses sulphate. You might have a trisulphatozirconate IV complex :)
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 14-10-2022 at 11:06


thank you! I didn't think that. I know that Zr, Nb, and such metals alkali fluoro complexes are insoluble or not much soluble in water, so I just precipitated it. ill try to find exactly what it is.

wet powder of the compound must turn the glass opaque after some time, if it is fluoro complex, isn't it?

[Edited on 14-10-2022 by vano]




View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1931
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 15-10-2022 at 00:58


Etches glass, Yep that sounds more like a fluoro complex. I don't know how soluble the sulphato-complexes are.
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 15-10-2022 at 10:12


one chemist found info for me about sulfatozirconate complexes of alkali metals in an old book. so according to the source, alkali metal sulfatozirconate will precipitate for example if you add a large exec of sodium chloride in an acidic solution of zirconium sulfate(which contains exec sulfate anion) Na2[ZrO(SO4)2]*3H2O will precipitate.

also, hydroxytrisulfatezirconate which is in solution loose bisulfate and turns into zyrconyldisulfate anion.


Screenshot 2022-10-15 220650.png - 8kB

[Edited on 15-10-2022 by vano]




View user's profile View All Posts By User