Chemgineer
Hazard to Others
 
Posts: 240
Registered: 25-5-2021
Member Is Offline
|
|
Aluminium chloride
I tried to electrolyse a solution of aluminium chloride, I got 1 amp to flow but then it immediately dropped to 0.2amp and when I tried to raise the
voltage to broiing it back up I popped a capacitor in my power supply.
Is it a bad idea to carry out electrolysis of this salt?
Sorry I seem to have put this in the wrong section.
[Edited on 9-8-2024 by Chemgineer]
|
|
|
Rainwater
National Hazard
  
Posts: 993
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
Electrolysis of aqueous AlCl3 results in a build up of a passivation layer of AlOx and Al(OH)3 on the cathode.
This layer has to be physically removed from my experience.
Gaseous Cl2 with ether escape or be dissolved into the solution and in my situation attack more of the aluminum anode
I use this process to convert scrap aluminum into refractory bricks.
It requires routine beatings in order to be considered a continuous process.
"You can't do that" - challenge accepted
|
|
|
Chemgineer
Hazard to Others
 
Posts: 240
Registered: 25-5-2021
Member Is Offline
|
|
Thanks, so the fact my power supply broke was probably just coincidence then, it has been in a corrosive environment for months.
|
|
|
Rainwater
National Hazard
  
Posts: 993
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
Lets assume there is no short circuit, hydrogen contamination or other obvious cause for the failure.
make sure your vcc is greater that the unloaded voltage of your electrolysis cell.
Meaning that as your reaction runs, the cell can turn into a battery amd due to Murphy law, produce more voltage than your power supply is outputting,
without a diode in series, this can reverse polarity your filtering caps,
Its a rarely encountered issue, because the extra voltage potential will dissipate over time and your cell can not charge more than voltage applied.
Unless you change the conditions, such as adding reagents.
Then the extra umph from the fresh chemicals will cause all sorts of electrical phenomenon until the system becomes heterogeneous.... homogeneous
..... damnit im tryin to sound fancy but cant spell the dam word. Till everything mixes throughly
"You can't do that" - challenge accepted
|
|
|
Chemgineer
Hazard to Others
 
Posts: 240
Registered: 25-5-2021
Member Is Offline
|
|
That's really interesting, I think you are probably right. In future I won't go near max voltage to hopefully avoid it happening again.
|
|
|
Sir_Gawain
National Hazard
  
Posts: 530
Registered: 12-10-2022
Location: southeast
Member Is Offline
|
|
What is the end goal of the electrolysis, i.e. what chemicals are you trying to produce?
|
|
|
Chemgineer
Hazard to Others
 
Posts: 240
Registered: 25-5-2021
Member Is Offline
|
|
I don't see much information about aluminium chlorate or perchlorate and I wondered why, so just on a small scale I thought i'd electrolyse a small
sample to find out the problems. I found them!
|
|
|
Rainwater
National Hazard
  
Posts: 993
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
http://www.chlorates.exrockets.com/chlorate.html doesnt have anything about alumnium. At a wild guess you would react alumnium with perchloric
acid so im out. That stuff to nasty for me. It can make your lab go boom boom boom.
[Edited on 11-8-2024 by Rainwater]
"You can't do that" - challenge accepted
|
|
|