Assuming extremely cheap electricity, what are some electrolyses you would run for profit?


Assuming extremely cheap electricity, what are some electrolyses you would run for profit?

Curious about the options. Thank you.
View user's profile View All Posts By User
bariumbromate
Hazard to Others
***




Posts: 106
Registered: 4-2-2025
Location: australia
Member Is Offline

Mood: nitrating

[*] posted on 5-6-2025 at 14:33


mabey copper and sulfuric acid from copper sulfate or chlorates



View user's profile View All Posts By User
MrDoctor
Hazard to Others
***




Posts: 251
Registered: 5-7-2022
Member Is Offline


[*] posted on 5-6-2025 at 15:05


sulfuric acid from elemental sulfur (sulfurous acid electrolysis), just because acid can be so expensive but its so useful to use all the time over other acids. So not for profit, but cost-savings.

selling alkali metals would probably be an easy one, doing something like electrolyzing alkali chloride at room temp from propylene carbonate, although idk if that cell requires a split circulated design using a mercury, or gallium membrane, its recommended but, possibly not required.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3954
Registered: 8-2-2015
Member Is Online


[*] posted on 5-6-2025 at 17:58
Assuming extremely cheap electricity


I would use the electricity to mine bitcoins etc. then buy Merck



CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 999
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 6-6-2025 at 02:57


Not some but almost all of them. First, I would open an electroplating company because, besides the revenue, it would give me access to a good part of the regulated chemicals. Then, I would branch out the company to electrosynthesis to make stuff that is otherwise too expensive to buy from, say, Merck et al. or to import from India, China or thereabouts. I would include my hobby electrosyntheses as "research" and have fun and profit at the same time.



Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
MrDoctor
Hazard to Others
***




Posts: 251
Registered: 5-7-2022
Member Is Offline


[*] posted on 6-6-2025 at 03:51


isnt turbostratic "flash graphene" worth something? you can convert almost any carbon-containing material into it with a flash reactor (rubber tyres in particular which normally cost money to dispose of), which at scale would pretty much just be like an auto-loading revolver but with short quartz tubes for chambers. flash graphene is supposed to exfoliate all by itself since the layers arent well connected, if nothing else it can radically alter the strength of concrete with a very minor addition comparable to a coloring additive, allowing for, with some creative engineering, using something like 30% less cement for the same overall strength. Im just going off the top of my head but its significant. turbostratic graphene made to a certain quality or refinement has loads of uses, its pretty much good to go as-is for any application where tiny flakes are acceptable, rather than singularly huge 2D sheets, idk if TSG can be fused, but even amateurs like myself can utilize it and do cool stuff with it.

[Edited on 6-6-2025 by MrDoctor]
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 6-6-2025 at 04:52


Aluminium is the traditional answer.
View user's profile View All Posts By User
chempyre235
Hazard to Others
***




Posts: 224
Registered: 21-10-2024
Location: Between Nb and Tc
Member Is Offline

Mood: Quite distracted

[*] posted on 6-6-2025 at 07:23


Here are a few suggestions that might be helpful:

  • Sulfuric acid
  • Hydroxylamine
  • Sodium nitrite
  • Formic acid
  • Chlorates and perchlorates
  • Periodates and derivatives (IBX and DMP)
  • Sodium metal
  • Magnesium metal
  • Potassium hydroxide
  • Hydrazine salts
  • Sodium hydride (for making NaBH4, NaBH3CN, and LiAlH4)

View user's profile View All Posts By User
Mister Double U
Hazard to Self
**




Posts: 66
Registered: 21-2-2025
Member Is Offline


[*] posted on 6-6-2025 at 10:09


Iron metal might be worth it.
A group from MIT is working on it - so steel making can be carbon neutral in the future:
https://news.mit.edu/2024/mit-spinout-boston-metal-makes-ste...
View user's profile View All Posts By User
MrDoctor
Hazard to Others
***




Posts: 251
Registered: 5-7-2022
Member Is Offline


[*] posted on 7-6-2025 at 00:54


iron filings arent cheap, or at least not readily found for cheap, here, if we are talking about stuff just anyone can manage, that, from common carbon-steel is absolutely doable, i opted to make some rather than buy, theres a trick to harvesting a lot without it re-dissolving that is probably manageable at scale
View user's profile View All Posts By User
Varungh
Hazard to Self
**




Posts: 70
Registered: 23-6-2025
Location: India
Member Is Offline

Mood: Bad mood

[*] posted on 24-12-2025 at 09:03


Making bleach(single cell electrolysis of table salt) it is cheap to get bulk NaClO solution. use MMO or just buy Graphite rods and set up a big 10l bucket for 2 days. Calculate concentration and sell.