moviez
Hazard to Self
**




Posts: 73
Registered: 25-8-2024
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 12-11-2025 at 20:36
Ni + HNO3 = something red?


Hi folks, I’m trying to make a small amount of Nickel nitrate and I reacted a few grams of nickel strips with 35% HNO3 solution (azeotrope HNO3 : H2O =1:1). To my surprise it ended up with a brick red solution (see picture).

The nickel is battery-grade (>99% per manufacturer but I’m not sure now). They attract to magnets well. Nitric acid is from JSP (I’ve used some from the same bottle before, and there was no issue).

I’ve tried a few things but they don’t make sense so far. I’ve boiled the solution to drive off dissolved NO2, and diluted the solution with more water, but the solution remains red.

I still have a few things to try:
(1) add a small amount of H2O2
(2) perform qualitative identification tests such as Prussian blue test for iron and see what other potential metals are there
(3) repeat this experiment again with even more diluted nitric acid

I’m wondering if anyone had seen this before? Even if my starting materials aren’t as pure as they advertised, it shouldn’t be this bad. Any inputs are highly appreciated.

IMG_3159.jpeg - 108kB

[Edited on 13-11-2025 by moviez]




Please check out the science contents on my YouTube: https://youtube.com/@thegoldenbearshow
View user's profile View All Posts By User
moviez
Hazard to Self
**




Posts: 73
Registered: 25-8-2024
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 12-11-2025 at 20:47


Here is a video of this reaction

Attachment: ScreenRecording_11-12-2025 20-15-19_1.mov (5.4MB)
This file has been downloaded 83 times




Please check out the science contents on my YouTube: https://youtube.com/@thegoldenbearshow
View user's profile View All Posts By User
Radiums Lab
Hazard to Others
***




Posts: 301
Registered: 18-3-2025
Location: India
Member Is Offline

Mood: Experiencing the elegance of science.

[*] posted on 12-11-2025 at 21:42


I think this Fe+3 impurities. As you know your solution should end up in an emerald green colour.



Water is dangerous if you don't know how to handle it, elemental fluorine (F₂) on the other hand is pretty tame if you know what you are doing.
View user's profile View All Posts By User
Radiums Lab
Hazard to Others
***




Posts: 301
Registered: 18-3-2025
Location: India
Member Is Offline

Mood: Experiencing the elegance of science.

[*] posted on 12-11-2025 at 21:46


This has a less chance but you might have Co nitrate too which is magenta in colour.



Water is dangerous if you don't know how to handle it, elemental fluorine (F₂) on the other hand is pretty tame if you know what you are doing.
View user's profile View All Posts By User
moviez
Hazard to Self
**




Posts: 73
Registered: 25-8-2024
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 12-11-2025 at 23:33


Quote: Originally posted by Radiums Lab  
I think this Fe+3 impurities. As you know your solution should end up in an emerald green colour.


My first thought was iron impurities as well. I’ll do some confirmatory tests and update here.

The chance of cobalt impurity is low since cobalt is much more expensive than nickel, and they usually don’t come in the same ores. But I’ll check cobalt as well.




Please check out the science contents on my YouTube: https://youtube.com/@thegoldenbearshow
View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 574
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 12-11-2025 at 23:56


A lot of pure nickel battery tabs from eBay/China are actually just nickel plated steel. I'm guessing 99% of their users wouldn't tell the difference.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 13-11-2025 at 07:35


Your solution looks remarkably much like a solution you get when you dissolve pure iron in HNO3, which I did a few years ago. Most likely Deathunter88's post gives the best explanation.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
moviez
Hazard to Self
**




Posts: 73
Registered: 25-8-2024
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 13-11-2025 at 19:24


Quote: Originally posted by Deathunter88  
A lot of pure nickel battery tabs from eBay/China are actually just nickel plated steel. I'm guessing 99% of their users wouldn't tell the difference.


You’re probably correct. I thought they were pure nickel since they were attracted to magnets, but apparently iron with a thin nickel coating does the same.




Please check out the science contents on my YouTube: https://youtube.com/@thegoldenbearshow
View user's profile View All Posts By User
moviez
Hazard to Self
**




Posts: 73
Registered: 25-8-2024
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 13-11-2025 at 19:25


Quote: Originally posted by woelen  
Your solution looks remarkably much like a solution you get when you dissolve pure iron in HNO3, which I did a few years ago. Most likely Deathunter88's post gives the best explanation.


Thank you for the input. When the nitric acid was added, it indeed turned green momentarily (which is probably from the nickel coating) and then turned blood-red color right after.




Please check out the science contents on my YouTube: https://youtube.com/@thegoldenbearshow
View user's profile View All Posts By User
moviez
Hazard to Self
**




Posts: 73
Registered: 25-8-2024
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 17-11-2025 at 21:21


Update:

Thank you all for the input. These are, indeed, just iron strips coated with a thin layer of nickel. See below for the thiocyanate test and Prussian blue test.

After the metal strips were dissolved in nitric acid, the mixture was diluted to ~300 ppm (by weight, so 0.0003 grams of metal ions per mL) before performing these tests. I didn’t do a quantitative analysis, but just based on the results, we can say the metal is mostly just iron.



IMG_3182.jpeg - 318kB




Please check out the science contents on my YouTube: https://youtube.com/@thegoldenbearshow