Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
 Pages:  1  ..  21    23  
Author: Subject: New Energetic Materials - Current Research
dettoo456
Hazard to Others
***




Posts: 291
Registered: 12-9-2021
Member Is Offline


[*] posted on 1-1-2024 at 11:43


High modulus, pyrolized polyacrylonitrile (carbon fiber) can be used to drastically enhance CMDB (and likely other types of) propellant burning rates. And carbon black is slightly energetic on its own - coal fires. Other than that, metal fuels are the closest thing to an elemental EM you’ll find.

Carbon fiber propellant catalyst pdf:
https://patentimages.storage.googleapis.com/4b/c9/f1/f77511a...
View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 11-2-2024 at 11:06
Ag2BTA


Anyone here with information about the disilver salt of bistetrazolylamine? I found this substance mentioned in "laser ignition of energetic materials" by S Rafi Ahmad and Michael Cartwright 10 years ago:

The copper and silver salt of bis tetrazolyl amine CuBTA (46) and Ag2BTA (47) have been trialled as primary explosives (...) the performance of these materials is a little unpredictable, and they should be treated with extreme care - particulary the silver bistetrazolamine. There is insufficient data in the literature to fully characterize their properties as primer compositions."



[Edited on 11-2-2024 by Nemo_Tenetur]
View user's profile View All Posts By User
dettoo456
Hazard to Others
***




Posts: 291
Registered: 12-9-2021
Member Is Offline


[*] posted on 11-2-2024 at 20:09


I couldn’t find any info on the silver salt, but the 5,5’-bis(tetrazolyl)amine is light sensitive on its own (much less energetic as compared to a detonation).

https://doi.org/10.1016/j.chemosphere.2019.125008

Laser sensitive EMs are pretty common though, laser initiation systems far less so.
View user's profile View All Posts By User
Nemo_Tenetur
Hazard to Self
**




Posts: 79
Registered: 13-12-2023
Location: Germany
Member Is Offline


[*] posted on 12-2-2024 at 01:46
EP 2 679 567 A2


There is an european patent filed in 2012, but the information is pretty sparse.

Impact sensitivity greater than one Joule, friction sensitivity greater than 20 Newton, decomposition temperature 360 degree centigrade (sic!)
Detonation was observed with 200 mW @ 532 nm wavelenght.
The chromium (III) salt is even more thermally stable, but deflagrates only.

The synthesis is also described and easy, so I´ll give it a try next time.







Attachment: EP2679567A2 BTA.pdf (141kB)
This file has been downloaded 529 times
View user's profile View All Posts By User
Mush
National Hazard
****




Posts: 643
Registered: 27-12-2008
Member Is Offline

Mood: No Mood

[*] posted on 16-10-2025 at 14:59


Recent Progress on Synthesis, Characterization, and Performance of Energetic Cocrystals: A Review

Molecules 2022, 27(15), 4775; https://doi.org/10.3390/molecules27154775

Abstract
In the niche area of energetic materials, a balance between energy and safety is extremely important. To address this “energy–safety contradiction”, energetic cocrystals have been introduced. The investigation of the synthesis methods, characteristics, and efficacy of energetic cocrystals is of the utmost importance for optimizing their design and development. This review covers (i) various synthesis methods for energetic cocrystals; (ii) discusses their characteristics such as structural properties, detonation performance, sensitivity analysis, thermal properties, and morphology mapping, along with other properties such as oxygen balance, solubility, and fluorescence; and (iii) performance with respect to energy contents (detonation velocity and pressure) and sensitivity. This is followed by concluding remarks together with future perspectives.
Keywords:
energetic materials; cocrystallization; detonation performance; characterizations of ECCs

The Study of Co-Crystallization of Trinitrophenol (TNP) and Ammonium Nitrate (AN) As a Potential Method for Enhanced Stability
DOI: https://doi.org/10.51584/IJRIAS.2025.100500035

Received: 16 April 2025; Accepted: 28 April 2025; Published: 05 June 2025
ABSTRACT

This study explores the co-crystallization of trinitrophenol (TNP) and ammonium nitrate (AN) using a slow solvent evaporation method at a 1:1 molar ratio. The co-crystal formation and its potential for improved explosive stability were investigated. Characterization techniques including Fourier-Transform Infrared Spectroscopy (FTIR), X-ray Diffraction (XRD), and Differential Scanning Calorimetry (DSC) were employed. FTIR analysis revealed new peaks corresponding to functional group interactions between TNP and AN, indicating co-crystal formation. XRD confirmed the presence of new diffraction peaks not observed in the individual components, further supporting co-crystallization. DSC analysis demonstrated a significant shift in thermal behaviour compared to TNP and AN. The co-crystal exhibited a glass transition, melting point, and decomposition temperature distinct from the single components. These observations suggest interactions between TNP’s -OH groups and Ammonium NH4+ ions, leading to the formation of a more stable ammonium picrate co-crystal. The altered thermal profile indicates a potential improvement in the co-crystal’s stability compared to the individual explosives.

Synthesis of environmentally friendly energetic cocrystal derived from commodity
10.1039/d4cc04037f
Abstract

Ammonium nitrate (AN) is a green oxidizer in the field of energetic materials. However, hygroscopicity and phase transitions have prevented AN from being put into practical use. To address these two drawbacks, a cocrystallization technique was applied to AN in this study. An AN/glycine (Gly) cocrystal was newly prepared and characterized; both AN/Gly and AN/sarcosine exhibited decreased hygroscopicity and did not exhibit a phase transition.
chemicals


Enhancement of the burning performance of ammonium nitrate via cocrystallization
Abstract
Ammonium nitrate (AN) is a low-cost oxidizer with a low environmental impact; however, its low burning rate limits its application. In this study, a cocrystallization technique was used to enhance the burning performance of AN. An AN/4- amino-1,2,4-triazole (4ATA) cocrystal (molar ratio = 1:1) was prepared, and its crystal structure was investigated using single-crystal X-ray diffraction. The friction sensitivity test proved to be sufficiently safe for the treatment of the cocrystal. 5-Amino-1H-tetrazole/strontium nitrate was blended with the AN/4ATA cocrystal or with a simple mixture of AN and 4ATA to evaluate the burning behavior using the deflagration test. The test results showed enhanced burning performance for the composition containing the AN/4ATA cocrystal compared to that containing the mixture of AN and 4ATA. The hygroscopicity test revealed that cocrystallization suppressed the hygroscopicity and also resulted in the phase stabilization of AN, as confirmed from sealed cell-differential scanning calorimetry analysis.

"In our previous
studies, we prepared novel cocrystals of 1Htetrazole/
sodium perchlorate (SP), 1,2,4triazole/SP, 3amino1,2,4
triazole/SP, and 4amino1,2,4triazole (4ATA)/SP. All four
cocrystals showed higher burning performances than the
corresponding mixtures of parent materials 13)15). To the
best of our knowledge, the series of studies undertaken by
our research group are the only ones that focus on the effect
of cocrystallization on the burning performance of a
mixture of fuel and oxidizer."

Three Insensitive Energetic Co-crystalsof 1-Nitronaphthalene, with 2,4,6-Trinitrotoluene (TNT),2,4,6-Trinitrophenol (Picric Acid) and D-MannitolHexanitrate (MHN)
Central European Journal of Energetic Materials, 2015, 12(1), 47-62

Abstract: Co-crystallization is proposed as an effective method to alter the physicochemical
properties of energetic materials, e.g. density, sensitivity and solubility.
As reported in this paper, it was found that 1-nitronaphthalene could form cocrystals
with TNT, picric acid and MHN in a 1:1 molecular ratio. The sensitivity
and thermal stability of the 1-nitronaphthalene co-crystals was greatly improved
compared with that of pure TNT, picric acid and MHN. In addition, the melting
points of TNT, picric acid and MHN were lowered through co-crystallization with
1-nitronaphthalene. The electrostatic potential surface of 1-nitronaphthalene,
calculated by the DFT method, showed that the electron-rich 1-nitronaphthalene
has a tendency to be a proton donor and to co-crystallize with other energetic
materials. The structures of the co-crystals of 1-nitronaphthalene with TNT and
picric acid were characterized by single crystal X-ray diffraction (SXRD). The
1-nitronaphthalene/MHN co-crystal was studied by powder X-ray diffraction
(PXRD), differential scanning calorimetry (DSC) and FTIR.

[Edited on 16-10-2025 by Mush]
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 13-11-2025 at 00:03


Recently I have been looking at furazan derivatives again. There are a number of procedures for diaminofurazan (DAF) from hydroxylamine hydrochloride and glyoxal which does not require a pressure reactor. The dehydration/cyclization step is done either in a high boiling polar solvent such as ethylene glycol, or in concentrated aqueous urea solution with reflux for 12 hours. I have not had much success with the EG processes, but I suspect there is some additive in my EG that is the culprit. The H2O/urea system works fine but I have noticed a fairly large amount of white crystalline sublimate that collects in the condenser.
This compound puzzles me. It is non-flammable, water soluble and does not melt on application of heat from either above or below but rather sublimates. When heated from below on a piece of Al foil this creates a sort of Liedenfrost effect that makes it skate around on the foil without melting.
I initially thought it might be hydroxylamine freebase, maybe as an adduct with water, but that doesn't track with the non-flammability.
Does anyone have an idea as to what it might be?
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 14-11-2025 at 09:34


Quote: Originally posted by Microtek  
Does anyone have an idea as to what it might be?


No idea, but you could check its pH in water, then see if it reduced AgNO3 solution. Or just throw it in a nitration bath and see what happens :D

Is this regarding the dinitramino analogue of DNAF?
View user's profile Visit user's homepage View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 21-11-2025 at 02:47


Quote: Originally posted by Microtek  
Does anyone have an idea as to what it might be?


Just a thought, probably thinking too exotic. Ammonium carbonate would likely act like that.
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 21-11-2025 at 03:14


Ammonium carbonate is probably the most likely. It is a very substantial amount and may provide insight into why the yield is not so good for these preparations (especially if calculated from hydroxylamine basis).

And, yes, I am considering nitrogen rich salts of furazan derivatives such as dinitraminofurazan or dinitraminoazoxyfurazan. I found a reference to the coupling of DAF to DAAF using just Oxone rather than H2O2/H2SO4 that worked quite well, and since it should be fairly straight forward to nitrate DAAF, it seemed natural to invetigate the salts.
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 21-11-2025 at 04:37


TODO is another possibility. 4H-[1,2,3]triazolo[4,5-c][1,2,5]oxadiazole 5-oxide. d. 1.934 g/cm3, VOD 9250 m/s, DP 43.1 GPa free acid decomposes at 89C though.

Supposedly DAF can be nitrated simply in 70% HNO3, involves a gay solvent extraction, but that's just with ethyl acetate.

From supporting info of ACS Appl. Energy Mater. 2020, 3, 9401−9407.

3,4-Dinitraminofurazan (6)

3,4-Diaminofurazan 5 (1 g, 10 mmol) was added in portions to a vigorously stirred 70% HNO3 (8 g, 5.6 mL, d = 1.42 g cm−3) at 25 °C. After that, the reaction mixture was stirred at ambient temperature for 2 h (as the reaction progressed, 3,4-diaminofurazan was completely dissolved). The solution was poured out into ice water (60 mL) and extracted with ethyl acetate (2 × 60 mL). The combined organic phases were washed with water (2 × 60 mL), dried over magnesium sulfate and concentrated under reduced pressure without heating. The obtained product (1.4 g, 76%) was identical to the 3,4-dinitraminofurazan synthesized by Tang et al.17 and was used without further purification.

Potassium 5-oxido-[1,2,3]triazolo[4,5-c][1,2,5]oxadiazol-4-ide (2a)

3,4-Dinitraminofurazan 6 (1.9 g, 10 mmol) was added in portions to a vigorously stirred and cooled (15 °C) solution of 93% H2SO4 (1050 mg, 10 mmol, d = 1.83 g·cm–3) in Ac2O (20 mL). After that, the reaction mixture was stirred for 30 min at ambient temperature. The solution was poured into
ice water (200 mL) and stirred for 30 min until Ac2O was completely hydrolyzed. Then AcOK (3 g, 30 mmol) was added in portions while stirring. The solution was extracted with ethyl acetate (2 × 200 mL), and the combined organic extracts were washed with H2O (100 mL). Water fractions
S4 were combined, and water was evaporated in vacuo. Acetonitrile (100 ml) was added to the brown residue and the suspension was vigorously stirred for 5 min. Then the precipitate (mainly inorganic salts) was filtered off. The solvent was evaporated in vacuo and the residue was recrystallized from MeOH to give K salt 2a (1.05 g) identical to that described previously.1 The mother liquor was concentrated under reduced pressure and the crude product was purified by flash chromatography (ethyl acetate/methanol, 5:1) to give an additional amount of the K salt as light yellow solid (200 mg). Overall yield: 1.25 g (74%); 13C NMR (125.8 MHz, d6-DMSO): δ = 160.9 (С-3a, C-6a) ppm; 14N NMR (36.1 MHz, d6-DMSO): δ = –3 (N-5, ∆ν1/2 = 15 Hz), –20 (2N, N-1, N-3, ∆ν1/2 = 540 Hz), –129 (2N, N-4, N-6, ∆ν1/2 = 600 Hz) ppm; elemental analysis calcd (%) for C2KN5O2: C 14.55, H 0.00, N 42.41; found C 14.83, H 0.00, N 42.15.

4H-[1,2,3]triazolo[4,5-c][1,2,5]oxadiazole 5-oxide (1)

To a suspension of K salt 2a (0.5 g, 3 mmol) in MeOH (10 mL) ion-exchange resin (Amberlite IR 120, H-form, 1.4 g) was added and the mixture was vigorously stirred for 2 h at room temperature. The ion-exchange resin was filtered off and the solvent was evaporated in vacuo. Diethyl ether (20
mL) was added to the residue. The white solid that formed was filtered off and washed with diethyl ether (5 mL). The filtrate was concentrated under reduced pressure to give pale beige viscous oil that crystallized in a few hours. Yield: 362 mg (95%); light beige solid; m.p. 89 °C (decomp.); 13C
NMR (150.9 MHz, d6-DMSO): δ 160.9 (С-3a, C-6a) ppm; 14N NMR (43.4 MHz, d6-DMSO): δ = –5 (N-5, ∆ν1/2 = 13 Hz), –20 (2N, N-1, N-3, ∆ν1/2 = 275 Hz), –121 (2N, N-4, N-6, ∆ν1/2 = 300 Hz) ppm; 13C NMR (125.8 MHz, d6-acetone): δ = 155.2 (С-3a, C-6a) ppm; 14N NMR (36.1 MHz, d6
acetone): δ = –5 (2N, N-1, N-3, ∆ν1/2 = 615 Hz), –38 (N-5, ∆ν1/2 = 50 Hz), –150 (2N, N-4, N-6, ∆ν1/2 = 600 Hz) ppm; IR (KBr): ν˜ 1092, 1337, 1466, 1500, 3057 cm-1; MS (EI, 70 eV) m/z : 97 [M-NO]+, 83 [M-N2O]+; HRMS (ESI) m/z [M-H]– calcd for C2HN5O2: 126.0047, found: 126.0050; elemental analysis calcd (%) for C2HN5O2: C 18.91, H 0.79, N 55.12; found C 19.17, H 0.73, N 53.41.
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 2-12-2025 at 09:22


I found a chinese (!) paper about new methods of preparing DAF (https://www.energetic-materials.org.cn/hnclen/article/abstra...). The full-text is publicly available, but in chinese. Here is an AI-translated excerpt. Beware of potential translation errors:

"2.2.1 Preparation of Supported Solid Base Catalyst

The activated carbon support was boiled in 30% nitric acid at 90 °C for 4 hours, washed with water until neutral, and dried. Then, 100 g of activated carbon was immersed in a potassium hydroxide solution overnight. The moisture was evaporated to dryness using a rotary evaporator. Under nitrogen protection, the sample was dried at 130 °C for 2 hours, then calcined by raising the temperature to 500 °C and holding for 4 hours to obtain the supported solid base catalyst. The KOH loading was 5% (mass fraction).

2.2.2 Synthesis of 3,4-Diaminofurazan Under Supported Solid Base Catalysis

15 g of 3,4-diaminoethanedioxime was dissolved in 187.5 g of distilled water and transferred into an autoclave. Then, 52.5 g of the supported solid base catalyst was added. After purging the air in the system with nitrogen, the autoclave was sealed and heated to 150 °C for 4 hours. The pressure change inside the autoclave was recorded.

After completion of the reaction, the mother liquor was allowed to cool naturally to room temperature, where a white solid precipitated. The solid was filtered and washed with water to obtain the product, with a yield of 91.2%.
m.p.: 179–180 °C.
IR (KBr, cm⁻¹): 3435, 3322 (—NH₂), 1646, 1589 (C—NH—O).
¹H NMR (DMSO): δ 5.8 (4H, NH₂)."

If true, this would be a sufficiently high yield that DAF-based materials could become interesting from more than an academic perspective.

[Edited on 2-12-2025 by Microtek]
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 10-12-2025 at 10:22


I had some DAF from ages ago, so I treated 1 gram with TCCA in acetonitrile (1:2 molar eq. in 50 mL solutions). This is the literature route to the bicyclic "difurazanotetrazocine", so 2 furazan rings joined through two azo bridges. I mistakenly added the TCCA slowly to the DAF whereas as published it should be done the other way around, this may be important.

The lit runs a 2hr soxhlet extraction with hexane, this sounds like a pain in the arse so I just evaporated the acetonitrile and digested the remains with NaOH/water and filtered the orange suspension. It seems to have worked.

You have to be careful with this stuff, it flashes violently on ignition, a fair comparison on the vehemicity scale would liken it to NHN or dinitrobenzenediazonium perchlorate. It detonates easily and strongly under the hammer and when briskly rubbed with the hammer on rusty steel. I wouldn't be surprised if C4N8O2 has initiating properties.

Testing the mp it was way off, lit gives 54C mine kind of beads up a bit at 100C then more major melting at over 200C. This may be the result of adding the TCCA to DAF instead of DAF to TCCA. May also be because I didn't extract it with hexane. I checked the lit for higher oligomers and found the props for the tetramer and its mp was 212C.

Both the dimer and tetramer have similar densities and heats of formation thus would be expected to have similar detonation properties. The tetramer has published values of 8550m/s and 31.9GPa. No sensitivity data for the tetramer but the dimer is 4 cm with 2.5 kg weight where HMX was 25 cm.


[Edited on 10-12-2025 by Axt]

Difurazanotetrazocine.jpg - 14kB
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 10-12-2025 at 23:57


It might also form polymers and I wouldn't be surprised if the higher homologues were favoured when an excess of DAF was present. Regardless, the potential for a metal free primary is interesting. I might have to look into that. At the moment I'm building a proper pressure reactor to see if I can make the above referenced procedure work. While the reported yields are not that much higher ( ca. 50% vs ca. 70 % total from glyoxal), the major expense is the hydroxylamine which is usually used in large excess such as 10 equivalents when doing the one-pot synthesis.

Another possibility is to perform the dehydration of DAG without solvent (https://revues.imist.ma/index.php/morjchem/article/view/7392). This gives a melt that solidifies on cooling and must then be worked up to remove impurities. Reported yields are around 70 %. I tried it one a 1 gram scale and got around 50%, though I didn't use nearly as much ethyl acetate as the authors. I suppose Soxhlet extraction would be a viable way to conserve solvent.
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2025 at 01:31


Have you entertained the thought of the microwave preparation:

One pot synthesis of DAF from glyoxime: An aqueous solution
of sodium hydroxide (100 ml 7.5 M) was added to glyoxime
(17.6 g, 0.2 mol) and mixture was kept under stirring. Subsequently,
hydroxylamine hydrochloride (27.8 g, 0.4 mol) was added, and
the contents were irradiated in the microwave oven at the power of
300 W for 2–3 min. During this period, a break of 30 s was given
when the reaction mixture started boiling. The flask was taken out of
the microwave oven after 3 min when the vigorous reaction started.
The reaction was allowed to subside at room temperature.
The reaction mixture was further irradiated in microwave oven for
30 min with a break of 30 s, whenever required (see above), using a
power of 800 W and was cooled to get a solid product. After washing
with water, DAF (14g, 70 %) was isolated.

It's out of India and half the stuff out of India is retarded but it looks plausible, its written descriptively not vaguely. It's from the paper "Microwave mediated fast synthesis of diaminoglyoxime and 3,4-diaminofurazan: key synthons for the synthesis of high energy density materials". 2005.

I've never tried it. The only "microwave mediated" prep I've tried was sulphanilic acid via microwaving aniline and sulphuric acid which went surprisingly well. I've also tried microwaving ethylene glycol with urea for ethyleneurea but this was a total failure.
View user's profile Visit user's homepage View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2025 at 10:27


Difurazanotetrazocine (DFT), 40 mg in a single layer of foil was negative to DDT, just flashed with a pop.

100 mg of DFT lightly pressed over 600 mg hand pressed PETN was positive with full detonation. Below compares the DFT initiated charge with a commercial #8. The #8 should be around 800 mg PETN with ASA primary and reinforcing cap.



DFT detonator vs numer 8 sm.jpg - 1.4MB
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 12-12-2025 at 06:41


I tried that exact preparation many years ago but found that once the mixture started boiling, cooling for 30 s at room temp removed so little heat from the mix that it started boiling again in a matter of seconds when replaced in the oven. That means you will have to babysit the reaction for maybe 4-6 hours. Perhaps if more heat can be removed during the cooling intervals such as with a water bath, it might be workable.

DFT seems very interesting, I think I have to experiment with it myself.
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 12-12-2025 at 08:17


Yeh I got to reading the old furazan pre-pub thread https://www.sciencemadness.org/talk/viewthread.php?tid=5813 I don't remember doing any of it, being 18 years old, but I mention the same result of the microwave prep as you. It just boils the instant power is reapplied. I guess you could run it slowly on defrost mode (so auto intermittent mode) and run it to dry and extract the result. I even seem to have had some obsession with DFT back then (I have a fetish for small symmetric molecules, they are pretty) but it was never tried. There was no mention of it being an actual primary explosive.

I think it would be worth trying adding DAF to sodium dichloroisocyanurate in water instead of TCCA in acetonitrile similar to the azotriazole reaction on route to BLG-1. The TCCA reaction is very easy but avoiding the need for acetonitrile would be great.
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 13-12-2025 at 05:05


Another possibility might be using Oxone for the oxidative coupling, though it might give DAAF instead. I don't know if the azoxy version of DFT would be stable enough to exist, but this might also be a possibility.
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 13-12-2025 at 13:30


Yeh I did stir some DAF in oxone and received a high yield of DAAF, it will respond with a weak snap to a very strong hammer blow. The reduced azo (non-oxy) bridged compound is meant to be just as insensitive. I've been trying to find reference to the sensitivity of the larger azofurazan macrocycles but have not found anything. I'll attach the article on DFT that mentions its sensitivity. I referred to this back in the 19yo thread but mentioned it's too old to be available online, its online now.

"DFT is a dangerous primary explosive with a drop height of approximately 4 cm (2.5 kg. Type 12, HMX=25 cm). We believe the sensitivity is due to the boat configuration as the azo-group's n-electrons are orthogonal to the x-electrons in the furazan rings, and thus no stabilization through delocalization can occur."

They do refer to an attempt at oxidising the DFT to azoxy but received only a low yield of monoazoxy compound and gave up. I have seen reference to oxidation of the tetramer to tetraazoxy yes very dense very powerful but it required oleum/persulphate ie. super Caro's acid.

I tried sodium dichlorisocyanurate (1.2 g DAF, 10.2 g SDCIC, 10. g 90% acetic acid / molar ratio 1:4:16) It turns orange instantly but left stirred for an hour then digested with 12 g NaOH whereby the solution turned dark brown. Filtering this leaves the same orange highly sensitive DFT. Its annoyingly fine and difficult to filter, I digested my filter paper with NaOH in the process.

[Edited on 13-12-2025 by Axt]

Attachment: azo, azoxyfurazans and difurazanotetrazocine (TCCA oxidation).pdf (648kB)
This file has been downloaded 69 times

View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 30-12-2025 at 00:44


I tried nitrating DAF as follows:

1.8 g DAF was added in small portions to fuming nitric acid (10 ml double distilled, free of NOx) at 0 C. Stirring was continued at this temp for two hours.

At this point the mix was poured on crushed ice. Nothing precipitated so the soln was extracted with 3 times 8 ml ethyl acetate. The combined extracts were evaporated in an air stream without heating. A small amount of gas evolution was observed during this procedure. I couldn't get the products to crystallize and the mix seemed fairly unstable, so I resolved to form salts directly. I did this by dissolving the product liquid in ethanol and then added this to ethanolic solutions of bases.
I began with simple KOH, the idea being that I could then react this with acid, extract into ethyl acetate and precipitate with other bases as needed. A large amount of orange precipitate was instantly formed when the two solutions were combined, but I had the suspicion that some of the crystals might be KNO3 if some of the nitric acid had been extracted into the ethyl acetate, or if decomposition of the nitrated product had produced HNO3 during evaporation.
To see if there was something other than HNO3, I added some of the product solution to an ethanolic solution of hydrazine hydrate. This also gave an instant precipitate that was slightly darker in colour than the potassium salt.
I also wanted to try the carbohydrazide salt whic I haven't seen mentioned in the litteraure. Carbohydrazide is not soluble in ethanol, but I dissolved some in a small amount of water and then added an equal amount of ethanol. This did not cause the CHZ to crystallize, so I added the purpoted DNAF solution to the CHZ soln, and after about half of the DNAF soln had been added, a large amount of beige precipitate had formed.

All of the salts were isolated and are air drying at time of writing.
On re-reading the "Taming DNAF" paper, I saw that they worry about over-nitrating the DAF substrate by substituting one of the nitramine hydrogens. This substance is obviously much less stable than DNAF. They resolve this problem by using a very small amount of WFNA (2 ml per 1 g of DAF), running the reaction at -10 C and only for 30 minutes.
This means that I likely have made a mixture of di- and tri-nitramines which may explain the instability.
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 1-2-2026 at 01:13


After working this past month on optimizing the preparation of DAF, I have done a few more runs of DNAF and its salts.

I first suspended 1 g DAF (10 mmol) in H2SO4 (96 %, 5 ml) and then added a mix of HNO3 (62 %, 2.24 g, 22 mmol) and H2SO4 (96 %, 2 ml) dropwise with stirring. I kept temp at 7-8 C using a salt/ice bath. After end of addition, I stirred another 30 minutes. At this point, some foam had formed, but there was no active off-gassing. The mix was poured on ice, and the clear solution was extracted with 3x10 ml ethylacetate. A little of the extract was combined with hydrazine hydrate. No precipitate formed, but after evaporating the solvent and excess hydrazine, a waxy crystalline substance remained. In a flame it melt and then burns with a hissing flame. It may be a hydrate, I will try drying it at some point.
The rest of the extracts were combined with CHZ-nitrate solution. This resulted in an immediate off white precipitate which was isolated.
The dried product puffs off at 198 C without melting. The yield was about 90 % from DAF.
I haven't done any sensitivity or performance tests yet.

I also tried the nitration using acetic anhydride and fuming nitric acid. My nitric had developed some NOx staining, and I think this may have caused some of the DAF to be oxidized (to DAAF probably) based on a marked orange colouring of the reaction. The advantage of not using H2SO4 is that the CHZ soln can be added directly when the mix has been diluted with water. This is problematic with the mixed acid nitration since CHZ-sulfate is only slightly soluble in water (about 25 g/L in hot water), and might compete with the precipitation of the product.
It might not be a big issue since the CHZ-DNAF salt has an extremely low solubility.

Edit: I have done a few tests of CHZ-DNAF. Firstly, I tested impact sensitivity by hammering on a cheap anvil. It required sustained full power strikes, but I was eventually able to set it off in this manner. I would say that it is considerably less sensitive than RDX.
I also compressed 1.000 g into the usual 7 mm ID brass tube with reinforcing block. I used my vice, but wasn't able to get the density to more than 1.70 g/cc. This is not so great, but might be caused by less than ideal crystal morphology. I do not have access to methods to measure crystal density, so it is possible that it is simply not much higher.
Finally, I made a plate dent test (20 mm Al block witness plate using the aforementioned 1.000 g in 7 mm tube at 1.70 g/cc). The dent was 4.2 mm deep placing it at 98 % HMX, 102 % RDX at their respective maximum achievable densities in my setup. This is quite decent at this relatively low density.

[Edited on 2-2-2026 by Microtek]
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 3-2-2026 at 14:34


Are you saying you did receive a precipitate from pouring the water/nitration mixture directly into carbohydrazide solution?

I've tried the prep I posted above, just stirring DAF into 70% HNO3 for 2 hrs at room temp until it dissolved, then poured this yellow solution into a CHZ solution but there was no precipitate. I neutralised it with NH3 but still nothing bar a little sediment that settled out, not enough to bother filtering. I might try again but follow the script to see if it works at all.

What Al grade witness plate are you using?

Interesting though, there's very little that can beat RDX while being less sensitive than it.
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 3-2-2026 at 23:51


Yes, after nitration in Ac2O/HNO3, the mix was diluted with water and then combined directly with carbohydrazide dissolved in acetic acid. The acetic acid was probably not necessary since the nitration mix contained that in abundance.
The product from the Ac2O nitration is not as thermally stable as that from mixed acids, puffing off at 180 C. I haven't done any experiments to improve the stability, and it is definitely possible that it stems from nitrosamine compounds (or something else entirely) from the dissolved NOx. Maybe boiling for a while could decompose any unstable impurities.

The Al is ordinary extruded AW-6060. I get it in 20x40x2000 mm bars and then saw small blocks off as needed.



[Edited on 4-2-2026 by Microtek]
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 979
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 5-2-2026 at 03:14


I tried again, 5 g DAF was stirred in room temp. 68% HNO3 for 2-3 hrs until it dissolved, then either evaporated out directly or poured into 200mL water and extracted with ethyl acetate. The ethyl acetate extract seemed to stay very wet with at least 20 mL water/HNO3 coming over with it I attempted to dry with CaCl2 but it was just too much.

Neither dried to dry crystals rather the ethyl acetate extract stayed slightly waxy, and that evaporated from HNO3 was oily. It dissolved readily in water but neither off these extracts produce precipitates when combined with carbohydrazide (1g extract with 1 molar eq. CHZ in 50 mL water).

The extracts are energetic, deflagrating similar to RDX and responding to the hammer in a similar fashion. Melting point for the obviously impure EA extract was low 60-70C.

EA extract dissolved readily into acetonitrile, there was an initial pale yellow precipitate on addition of 80% hydrazine hydrate for which I accidently added 2x to much (4 molar eq.), but it turned into a yellow solution with small orangish brown oily precip. Currently evaporating out the acetonitrile.

All in all, its pretty ugly.



dinitraminofurazan.jpg - 702kB
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 992
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 5-2-2026 at 23:40


I have never isolated the free acid. When I tried evaporating the ethyl acetate extracts the first time I nitrated DAF (and my product was probably contaminated with a lot of the dinitramide derivative) it started bubbling ominously even a room temp, so I stopped concentrating any further and just added the protonated bases in ethanol. Subsequently, I just haven't bothered to evaporate before precipitating the salts. I did find that the CHZ salt doesn't precipitate from ethyl acetate unless the CHZ is protonated first. I have used both CHZ nitrate and acetate which I would dissolve in a small amount of water and then dilute with ethanol.
When this is added to the ethyl acetate extracts (still wet and probably containing some HNO3) with rapid stirring, immediate precipitation is observed. Over the course of a few seconds the precipitate seems to mostly redissolve but as more CHZ-NO3 soln is added, the precipitate persists. The hydrazine salt seems to not precipitate as easily, and I had to evaporate to dryness (room temp airstream) to get the somewhat waxy salt. I did use straight hydrazine hydrate in this case, not a hydrazine salt.