Melting MgO with electric arc is EASY !!
With an electric welder I made an arc which melted MgO rods like plastic ....
<iframe sandbox width="760" height="465" src="http://www.youtube.com/embed/AHAUHIOD_5Y" frameborder="0" allowfullscreen></iframe>
|
|
|
vmelkon
National Hazard
  
Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline
Mood: autoerotic asphyxiation
|
|
That's neat. Perhaps you can make a MgO crucible.
|
|
|