[*] posted on 4-5-2013 at 21:39
Over-the-counter Tetrahydrofuran


I found a product hidden in the depths of my garage called "Christy's PVC Pipe Cement". Looking at the MSDS, it turns out that much of it is composed of tetrahydrofuran, about 38-50%. The stuff is also reasonably cheap. I think that you could fractionally distill it to obtain the pure THF. I really don't know if this would be pure enough to use in a Grignard reaction... maybe. You would probably have to take steps to dry it as well. Anyway, I still think it would be cheaper to get THF this way than by ordering it online.

The link to the product: http://www.homedepot.com/p/Christy-s-8-fl-oz-PVC-Pipe-Cement...



[Edited on 5-5-2013 by ParadoxChem126]




View user's profile Visit user's homepage View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 4-5-2013 at 22:28


The primer may be promising as well; it doesn't have the sticky PVC resin:

http://www.homedepot.com/catalog/pdfImages/34/342c06be-e1cb-...

MEK, acetone, THF and cyclohexanone might be a challenge to separate; I'm guessing THF and acetone will come off close together, followed by MEK and hex? Sodium bisulfite might be useful to precipitate the remaining ketones, or other adducts or adsorbants (particular size molecular sieves?).

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 5-5-2013 at 05:55


http://hpd.nlm.nih.gov/cgi-bin/household/brands?tbl=brands&a...
http://hpd.nlm.nih.gov/cgi-bin/household/brands?tbl=chem&...

.
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 5-5-2013 at 10:22


try pvc and cpvc pipe dope primer:

http://www.sciencemadness.org/talk/viewthread.php?tid=3173#p...

[Edited on 5-5-2013 by Magpie]




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
DH2
Harmless
*




Posts: 8
Registered: 13-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 13-5-2013 at 18:20


Tetrahydrofuran should be easy to find in pure form. I have seen it sold to repair rafts. It's also sold as "conformal coating remover":

http://www.techspray.com/download-tds-document.php?pId=99