sublimation of CuI + I2 to get...


In the equation:
4KI + 2CuSO4 => 2CuI(precipitate) + I2(aq) + 2K2SO4(aq)
To end up with a pure I2 product it would be necessary to sublime the CuI+I2 (after fine filtering the I2 out of soln.
Can anyone shed light on the validity of this method (which avoids the sublimation step):
1Filter out the CuI precipitate as per usual
2Then add HCl to the remaining soln (ie: I2+ K2SO4) until the Ph is 1.
3Then add H2O2 and the I2 will crash out of soln
View user's profile View All Posts By User
Axt
National Hazard
****




Posts: 973
Registered: 28-1-2003
Member Is Offline

Mood: No Mood

[*] posted on 10-12-2004 at 09:22


Quote:
Originally posted by johnnyBbad
1Filter out the CuI precipitate as per usual
2Then add HCl to the remaining soln (ie: I2+ K2SO4) until the Ph is 1.
3Then add H2O2 and the I2 will crash out of soln


Why use copper?, it can be precipitated straight from KI solution:

2KI + 2HCl + H2O2 --> I2 + 2KCl + 2H2O

It's what I use.
View user's profile Visit user's homepage View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3320
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 10-12-2004 at 09:40


This was the method we used in lab to titrimetrically determine the copper concentration in ore.

2Cu2+ + 5I- ---> 2CuI + I3-

Followed by titration of the triiodide anion with sodium thiosulfate. I never noticed (solid) elemental iodine formed, the solution just went a nasty brown color, i.e. iodine formed complexed with the iodide in solution to form triiodide. I wouldn't call this a good procedure to iodine by a long shot just look at the potential for losses, and CuI is fairly insoluble unless you have excess ammonia or potassium iodide in solution (more losses) so you'd have a hard time getting anything back from that ...
Quote:
....incredibly unstable, risking the potential hazard of explosion and a horrible oder of rotten eggs and mayonaise that will sink into your house and not leave for weeks.
What?



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 10-12-2004 at 16:25


You certainly wouldn’t get any back if you used ammonia. NI<sub>3</sub>… How would KI affect this reaction?
View user's profile View All Posts By User
johnnyBbad
Harmless
*




Posts: 5
Registered: 10-12-2004
Member Is Offline

Mood: heightened mood

[*] posted on 11-12-2004 at 18:24


thanks AXt.. I had my wires crossed a little there..your clear and concise response has clarified someth:cool:ing for me..beautifully