Burn Rates for Rocket Fuel


I'm going to be doing an experiment either tomorrow or before the week is out, measuring burn rates for different solid rocket fuel mixtures and ratios. The oxidizer I'll be using will be KNO3 and ordinary sugar for the fuel(sucrose). The end goal is to build some efficient home-made rockets, but for now I'm just interested in getting some numbers.

So I was wondering if people had some suggestions for the different ratios I could try and also burn catalysts to add. For example, the standard test I'll be doing will be using the standard mixture in 6:4 , 3:4, and 10:4 ratios to see which burns the fastest.

Some folks have told me you can use different additives to also alter the burn rate, but I couldn't get any solid info on it. Like the wikipedia page says you can add aluminum and iron oxide, but im pretty sure that makes thermite when ignited..

So any suggestions, hints tips etc? Thanks in advance <3
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 1-7-2015 at 17:18


You can add aluminum OR iron oxide, not both. I prefer Fe2O3 2% by weight with the 60/40 ratio.