Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Making Bismuth(III) Oxide
toothpick93
Harmless
*




Posts: 44
Registered: 26-2-2013
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2015 at 05:06
Making Bismuth(III) Oxide


i've been filming a few videos lately to do with pyrotechnics and fire and came accross dragon eggs which are a very simple composition which requires Bismuth Trioxide as the main component I did not have so instead of buying it I decided to make it (in a bit too deep here I think). I must not have looked deep enough but the videos I watched of Nitric acid reacting with bismuth was slow and needed heating to accomplish anything so I added my bismuth into the acid and geez it reacted vigorously, I was prepared for something like that I just did not expect it.

I came back the next morning and the solution went from clear to pretty much a saturated solution with what looks to be most of the crystals falling out of the solution, is this a mixture of Bismuth Nitrate and Bismuth Oxynitrates? When i add the crystals to water the solution turns a cloudy white and then when I add the cloudy solution to Sodium Hydroxide a white precipitate falls out of the solution. Is this Bismuth(III) Oxide? Is the Bismuth nitrate hydrolyzing on contact with the water to the oxynitrates and then reacting with the NaOH to form the insoluble Bismuth Oxide?

Bismuth in Nitric Acid
20151102_174323.jpg - 209kB

Bismuth solution in water
20151102_174459.jpg - 149kB

White precipitate after adding sodium hydroxide
20151102_174245.jpg - 182kB
View user's profile Visit user's homepage View All Posts By User
woelen
Super Administrator
*********




Posts: 8149
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 2-11-2015 at 08:11


Your water contains a lot of bismuth nitrate in solution, excess HNO3 and the solid is basic bismuth nitrate, mixed with hydroxde.

If you want to make your oxide, simply dissolve the bismuth in nitric acid and when all of the metal has disappeared, then boil down the liquid. At a certain point you get a wet paste. Keep heating, drive off water vapor and vapor of nitric acid. Keep heating further and stronger, you get nitric oxide (brown fumes). After prolonged heating, when the formation of brown fumes ceases, you will have a pale yellow solid, which is quite pure Bi2O3. Pure Bi2O3 is yellow, not white.

It is a pity that you added NaOH to your solution of bismuth. Now you contaminated your product. The precipitate almost certainly contains quite some sodium ions as well, it most likely will be impure bismuth hydroxide/nitrate with trapped sodium ions.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2015 at 09:09


I've made bismuth trioxide by accident when attempting to melt bismuth powder. Instead of melting, the high surface area makes it react with oxygen and turn into yellow Bi<sub>2</sub>O<sub>3</sub>.
View user's profile Visit user's homepage View All Posts By User
Amos
International Hazard
*****




Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline

Mood: No

[*] posted on 2-11-2015 at 09:19


Woelen, if the OP strongly boils the solution dry(with the precipitate still in it), will the basic nitrate lose water and nitrogen dioxide, and the hydroxide decompose as well to form Bi2O3? Or do you think these compounds will be unresponsive to strong heating? If it works, the sodium compounds should be able to be removed simply by washing with water.

[Edited on 11-2-2015 by Amos]




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8149
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 2-11-2015 at 14:02


If the OP boils down the solution, then he'll end up with sodium nitrate and bismuth oxide. On further heating it will be amazingly hard to get rid of the nitrate. It will partially decompose to nitrite but only at very high temperatures. Rinsing with water will not really help. The sodium ions will be trapped inside the particles of the Bi2O3 and will only partially leach out.

For pyrotechnic purposes, however, the heated product will be useful, I'm quite sure that the crackling effect in dragon's eggs still works fine with the material which has some sodium ions and nitrate ions left in it.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
toothpick93
Harmless
*




Posts: 44
Registered: 26-2-2013
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2015 at 15:28


I understand boiling it down to decompose it is the most easiest way but I do not have access to a hot plate to be able to boil down without breaking anything. I figured using sodium hydroxide was the easiest way for me at least, I can at least try wash the solid Bi2O3 with a lot of hot water to get rid of as much sodium nitrate as possible
View user's profile Visit user's homepage View All Posts By User
toothpick93
Harmless
*




Posts: 44
Registered: 26-2-2013
Member Is Offline

Mood: No Mood

[*] posted on 20-11-2015 at 03:29


I decided to use Potassium Hydroxide over Sodium Hydroxide for the reaction. This is the white precipitate I was left with. I thought Bismuth(III) Oxide is supposed to be yellow? Is it ok that it is white?

20151118_220826.jpg - 164kB
View user's profile Visit user's homepage View All Posts By User
HeYBrO
Hazard to Others
***




Posts: 290
Registered: 6-12-2013
Location: 'straya
Member Is Offline

Mood: :)

[*] posted on 20-11-2015 at 03:44


Quote: Originally posted by toothpick93  
I decided to use Potassium Hydroxide over Sodium Hydroxide for the reaction. This is the white precipitate I was left with. I thought Bismuth(III) Oxide is supposed to be yellow? Is it ok that it is white?



Why don't you try it in the composition you're interested in? If it doesn't work try again with the suggestions posted by woelen et al.
View user's profile View All Posts By User
toothpick93
Harmless
*




Posts: 44
Registered: 26-2-2013
Member Is Offline

Mood: No Mood

[*] posted on 20-11-2015 at 05:42


I'm certain it is Bismuth Trioxide, what else could it be. I cant make the composition yet as i'm working to make Nitrocellulose Lacquer next. I cant really test it as everything I do is also made into a video for youtube. I will just have to wait until it is time to make it
View user's profile Visit user's homepage View All Posts By User

  Go To Top