Downs cell + MgCl2
Hi,
I am setting up Downs cell and got a question related to electrolyte.
In industrial process mix of NaCl and CaCl2 is used, however my CaCl2 is heavily contaminated with Mg. Think of Dolomite ...

Does anyone have any experience/knowledge if MgCl2 would interfere with cell operation ?
I've googled around heavily and haven't found the answer.
Regards
|
|
|
IrC
International Hazard
   
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
I would think since the reduction potential of Mg is lower than that of sodium then you have a problem. I could be wrong but I think your answer is
that simple, and I'm guessing the lower than Na it is the bigger the problem. Not being a chemistry guru myself, perhaps Woelen or another member can
give a better opinion.
Na+(aq) + e– Na(s) -2.714
Ca2+(aq) + 2 e– Ca(s) -2.87 higher
Mg2+(aq) + 2 e– Mg(s) -2.37 lower
"Science is the belief in the ignorance of the experts" Richard Feynman
|
|
|
pesco
Hazard to Self

Posts: 95
Registered: 19-11-2015
Member Is Offline
Mood: No Mood
|
|
Good point, thx.
I guess I better drop the MG(OH)2 with Ca(OH)2 or buy some clean CaCl2
|
|
|