[*] posted on 23-11-2015 at 02:37
Iron-Chlorine secondary cell - conceptually?


I've had this idea for an Iron Chlorine rechargeable cell for a while now and would like to run it by the folks here to get an idea on it's feasibility.

I have attached a basic diagram of the cell.

The intended half reactions for this cell are:

Discharge:

Anode: Fe -> Fe^3+ + 3e^- (+0.04V)
Cathode: 2Cl^- -> Cl2(g) + 2e^- (+1.36V)

Cell Voltage is 1,4V

(ref: https://en.wikipedia.org/wiki/Standard_electrode_potential_%...)

FeCl cell.PNG - 5kB

This cell employs an anhydrous deep eutectic combination of Ferric chloride and Calcium chloride whereby the excess Ferric chloride formed during discharge would remain in and form part of the electrolyte.
(referring to my post here: https://www.sciencemadness.org/whisper/viewthread.php?tid=10...)

The Cathode is a porous carbon electrode with a nickel mesh current collector hopefully in order to effectively collect and diffuse chlorine gas during cycling.

The cell/cell stack would be constructed inside a chlorine resistant pressure vessel that would store the chlorine gas produced after charging under pressure.

According to the phase diagram this cell should operate well within it's parameters at around 30 degC provided the molar proportion is maintained.

I know there are people here with way more electrochemical experience than I have and would like to hear their views on the concept along with any advice or suggestions.




We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3947
Registered: 8-2-2015
Member Is Offline


shocked.gif posted on 23-11-2015 at 05:27


I would consider the volume x pressure of chlorine gas required for your required A.h capacity
Then consider that quantity in a consumer environment.
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 23-11-2015 at 12:02


Hey froot, nice to see a thread by you and an idea for an invention to boot, keep them coming!

Now down to the business. Whenever you have gas and phase change as one of your half reactions, chances are that you will need a catalyst to get decent amounts of power out of the system. For chlorine, this is quite easy, it so happens that ruthenium dioxide is a fantastic chlorine catalyst, so DO use RuO2 MMO titanium anodes. In SA there's a great company that makes them, NMT electrodes. They are also even cheaper than China!

Secondly, your cell voltage might not be 1.4V because that's defined for a 1M Cl- solution as electrolyte in water, but it would probably be close to that anyhow.

Next, I've experimented with DES electrolytes for batteries and found their performance wanting, sadly! Specifically, they have much lower conductivity compared to traditional good electrolytes like concentrated KOH or H2SO4 solutions in water. The mobility of the ions seems to be low. Again, it'll give a voltage, but don't expect power densities anywhere near conventional batteries.

Running hot on the other hand helps A LOT in this regard. But then you might as well run a hot molten salt battery.



[Edited on 23-11-2015 by deltaH]




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6475
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 23-11-2015 at 12:57


Two problems I see.
One is that the eutectic needs to be maintained to within certain specifications -- which means that the amount of FeCl3 used or liberated must be kept relatively small. This means that it is not going to be a deep-cycling battery.
Secondly, it does not look like an entirely user-friendly idea. Free chlorine in a consumer product is something generally to avoid.

I'll let the experts chime in in the chemistry of it all.
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 23-11-2015 at 13:19


There are better ways to skin a mule.

http://www.google.com/patents/US5422197
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 23-11-2015 at 13:20


Feel free to balance this equation
Fe + FeCl3 --> FeCl2
then explain what will stop it happening in the cell.
View user's profile View All Posts By User
froot
Hazard to Others
***




Posts: 347
Registered: 23-10-2003
Location: South Africa
Member Is Offline

Mood: refluxed

[*] posted on 25-11-2015 at 03:14


Unionised that was one of my concerns and suspected this would be a favorable reaction in those conditions but this got me thinking - baseless speculation as follows:
Anhydrous FeCl2 is an amorphous solid it may be possible that it forms a 'passivation' layer on the iron anode preventing further reaction with FeCl3 in anhydrous conditions. Now would this inhibit electrochemical functionality of the cell or could it improve it?
Half reactions from wiki I mentioned above:

1) Fe^3+ +  e^− -> Fe^2+ +0.77V
2) Fe^2+ + 2^ e− -> Fe(s) −0.44V

If my 'passivation' theory is correct and equation 1 occurs then this is proof that Cl^- ion mobility occurs. How the +0,77V, being on the electrolyte side of the 'passivation' layer affects the bigger picture and if it determines the favourability of this reaction is a bit beyond my understanding and am hoping for some input on this. Furthermore equation 2 would suggest an increased overall cell voltage.

If I'm making a fool of myself it's worth the 1 in 1000 chance that I'm onto something.

j_sum1 If you look at the phase diagram I may be reading it wrong but as the FeCl3 molarity increases it remains liquid but with solid FeCl3 suspended in it so one may be able to achieve an acceptable cycle depth from it.
As for the chlorine hazard I would encase this cell chamber in a second low pressure chamber with an inch of ammonia solution at the bottom which would neutralise any chlorine that happened to leak from the cell chamber.

DeltaH I'd be interested in your experiments and findings from working with DES electrolytes. I've always speculated that anhydrous electrolytes would perform far better than aqueous electrolytes especially from a charge efficiency and ion vs electron conductivity perspective. Thanks for the info on the chlorine electrode.

Thanks for the input.




We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 25-11-2015 at 11:56


I have tried the choline chloride + metal chloride 'flavour', not anhydrous (75% choline chloride solution was used), nevertheless, conductivity was dramatically poorer compared to acid in water and KOH in water.

It may be mixture specific, but I think the trend will hold. Few things come close to the ease with which protons hop between water molecules.







Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 25-11-2015 at 12:19


Quote: Originally posted by deltaH  
Few things come close to the ease with which protons hop between water molecules

Why is that so ?

Kinetics ?

If so, the notion of how it all works may be influenced by something as simple as agitation of the electrolyte.

A purely chemical system might not work, wheras a hybrid might.

Edit:

Odd feeling.

2 years in and i'm suggesting mechanical vibration as a catalyst in an electrochemical reaction.

Very odd indeed.

[Edited on 25-11-2015 by aga]




View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 25-11-2015 at 20:34


Yes it's a kinetic effect born out of a special mechanism of ionic flow, called the Grotthuss mechanism and you can read a nice introduction about it here and also see a nifty animation:

https://en.wikipedia.org/wiki/Grotthuss_mechanism

From the article:

Quote:
The Grotthuss mechanism, along with the relative lightness and small size of the proton, explains the unusually high diffusion rate of the proton relative to that of other common cations (Table 1), which is due simply to random thermal motion, i.e. Brownian motion. Quantum tunnelling becomes more probable the smaller the mass of the cation is, and the proton is the lightest possible stable cation. Thus there is a minor effect from quantum tunnelling also, although it dominates at low temperatures only.


Also from the article:

Table 1 values:

K+ 0.762×10−3 Mobility / cm2 V−1 s−1
H+ 3.62×10−3 Mobility / cm2 V−1 s−1

To put that into perspective (provided I am interpreting that table correctly) if you used potassium sulfate as electrolyte in your car battery instead of sulfuric acid of the same molarity, instead of bursting out say 340A during starting, it would produce a feeble ~72A initially, 4.75 times less!

What's more, those ionic mobilities are for solutions in water...

I know that for the electrolyte of lithium ion batteries, it's common to use a solvent combination of ethylene carbonate and dimethoxy methane, as an anhydrous solvent for lithium ions, specifically.

Nafion membranes, being a polymer of a super-acid, has a very high proton conductivity, but it's price is insane!

[Edited on 26-11-2015 by deltaH]




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 26-11-2015 at 00:55


Either an alternative or pricing will come down on the nafion membranes if flow cell technology will come online. Distributed power storage, everyone needs one in the garage.
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 26-11-2015 at 01:55


I have seen cheaper hybrid anionic membranes sold commercially at much lower prices than Nafion, however, on closer inspection, their conductivity is rather pathetic and those with high conductivity cost nearly as much as Nafion :mad:

[Edited on 26-11-2015 by deltaH]




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 26-11-2015 at 06:36


Would surely be nice to be able to manufacture your own membranes, but I'm probably dreaming there. Anyone have any idea whats involved?

Maybe it's not so far fetched. Can anyone access this article? Looks interesting.

Now we just need a supply of rejects.

http://www.sciencedirect.com/science/article/pii/S0013468604...

And another one of interest.

http://www.sciencedirect.com/science/article/pii/S0167273898...

[Edited on 26-11-2015 by hyfalcon]

[Edited on 26-11-2015 by hyfalcon]

[Edited on 26-11-2015 by hyfalcon]
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 26-11-2015 at 06:54


The hybrid types are potentially possible in the amateur context, but the downside is they're not very conductive, I think something in the order of 300A/m^2 of membrane (the pro ones), which is pretty poor.

I haven't looked into it, but my understanding is that you start from ordinary cheap ion exchange resin, mill it, then mix with an inert polymer ?like LDPE? and then extrude as thin a sheet as possible.

A very crude version might be hacked in an amateur context, press a melt from glue-gun sticks and ionic resin in a smooth vice with waxed paper (used in baking) squeezed between two hot metal plates?




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
Geekineer
Harmless
*




Posts: 12
Registered: 21-12-2015
Member Is Offline

Mood: No Mood

[*] posted on 21-12-2015 at 13:59
3D printing ionic membranes


What about taking the milled ionic resins and extruding it into 1.75mm filament for 3D printing - not sure if you'd have to mix in some PLA ...... but there are a lot of additives out there today and why not try one more.