Hello everyone! I found I have had an old dead car battery which is labeled Calcium-Calcium. First, I opened the top cap of the battery, used a syringe to take some of the liquid ( I collected about 50 mls in around 1 min.). I poured it over NaHCO3 and NaCl and reactios took place in both cases. Then I brought it to a boil with the idea to concentrate it. I was expecting this, but something weird happened - the liquid evaporated and I was left with a white solid on the bottom of the beaker. I have no idea why this happened, so that's why I'm asking here.

P.S. I did this on a normal hotplate, without any special chambers or distillations.

[Edited on 28-12-2015 by johncena]
View user's profile View All Posts By User
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 28-12-2015 at 12:13


Yes, I have had that result as well.

Solubility of PbSO4 is = 0.00443 g/100 mL (20 °C)
Solubility of CaSO4 is = 0.24 g/100ml (20 °C)




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
johncena
Harmless
*




Posts: 13
Registered: 23-12-2015
Member Is Offline

Mood: No Mood

[*] posted on 28-12-2015 at 13:23


So is there a way of cleaning it? Maybe a kind of a distillation or..?

[Edited on 28-12-2015 by johncena]
View user's profile View All Posts By User
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 28-12-2015 at 13:52


I would require vacuum distillation to distill the sulfuric acid itself.
Doing it at atmospheric pressure causes the H2SO4 to break down into SO2.

Also, you have to start with distillation at 1 atm to distill away most of the water and old car battery acid has a lot of water.




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User

  Go To Top