I have successfully produced very pure PGC by electrochemical preparation by using 40gpl of KCN as both the anode and cathode solution.

The anode was a 24k pure gold foil, the cathode was a 304 Stainless steel inside a porous cup. Voltage was around 12v.

Upon anode disintegration, the anode solution was boiled down to 25% volume, as the solution cools very white PGC precipitated. Washed with very cold water three times and was vacuum dried.

Now I wonder if the same procedure will work for Nickel, Copper and Silver? As their potassium cyanide salt form is not readily available in my country I have to prepare them myself.
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 30-11-2016 at 09:47


PGC? Potassium Gold cyanide?



PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
autumnwilow
Harmless
*




Posts: 2
Registered: 23-11-2016
Member Is Offline

Mood: No Mood

[*] posted on 4-12-2016 at 07:15


Quote: Originally posted by PHILOU Zrealone  
PGC? Potassium Gold cyanide?


Yes, exactly.
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1254
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 21-12-2016 at 09:10


Silver I think yes. I don't know about the others.



Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4508
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 21-12-2016 at 09:55


K2[Ni(CN)4] is easily made by reaction of KCN with nickel cyanide (itself easily made by reaction of any soluble nickel salt with two equivalents of potassium cyanide).



Please remember: "Filtrate" is not a verb.