How stable is TEMPO to heat?


Over the summer for a few days I stored some TEMPO in my shed while I was cleaning up the garage. It was pretty hot and melted the TEMPO into a solid mass. It has a lower MP, so it is expected.

What is the likelyhood that it has decomposed? It had a dark color reddish color to begin with, so not easy just with a visual inspection.
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 4-1-2017 at 08:41


There is a flash point recorded in SigmaAldrich MSDS at 67ºC so probably fine - maybe a very small percentage has decomposed but I wouldn't worry too much.

(either way it will be used in catalytic amounts :P )

[Edited on 4-1-2017 by Eddygp]




there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
DrP
National Hazard
****




Posts: 625
Registered: 28-9-2005
Member Is Offline

Mood: exothermic

[*] posted on 4-1-2017 at 08:45


I would guess that it is fine also... it is a 'stable' free radical... I used to use it a long time ago and ran reactions with it at about 120C. Although I stored it in the fridge. It is not like the older BPO which decomposed at 40C or so - it is relatively stable.

I would do a small scale test by polymerising some styrene with it at a controlled concentration to see if you get the right MW out of it before doing any serious work.