[*] posted on 9-2-2017 at 15:19
Unique silver compounds


Silver nitrate is combined with these salts

Sodium oxalate
Sodium citrate
Sodium ascorbate
Sodium metabisulfite
Sodium acetate
Sodium chlorocyanurate
Sodium borate....
Sodium silicate...
Magnesium sulfate
Sodium hypochlorite

Insouble yellow silver oxalate

Silver citrate formed is soluble

Sodium ascorbate forms black solid?

Sodium metabisulfite forms pink solid?

Insoluble white silver acetate

Sodium chlorocyanurate forms white percipitate?

silver sulfate slight white cloudyness

silver hypochlorite forms white percipitate
And a little black precipitate


Side notes
Reactions with copper foil
Also if anyone needs copper foil
I extracted mine from a lithium ion battery

Silver acetate
Big chunks spall off the copper foil
Silver citrate
Strongly adheres to the copper foil
Silver sulfate
Percipitate forms on copper surface


[Edited on 9-2-2017 by symboom]

[Edited on 10-2-2017 by symboom]

[Edited on 10-2-2017 by symboom]
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4308
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 9-2-2017 at 15:22


The black solid formed by the reaction with ascorbate is probably metallic silver. Ascorbic acid is a reducing agent.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
myristicinaldehyde
Hazard to Others
***




Posts: 166
Registered: 23-4-2016
Location: .͐͌ ͛҉̻̫̰̻̖E̮ͮ̐́̚ ̢̗̅̉ͩ͂̒̌.̯̻̺̯̀̎͂̄ͩ̚
Member Is Offline

Mood: сорок пять

[*] posted on 9-2-2017 at 16:02


I would guess the pink precipitate is silver sulfite, which apparently decomposes very readily on exposure to light- this would be the pink color. I am basing the color source off my experience with silver chloride.

A proof of decomposition causing the pink color rather than the salt itself would be to make some fresh in dim light, then put it in the sun or a UV light. If it is sulfite, then if you wash it very thoroughly (out of the light) and add a little bit to acid, SO2 should be given off.




If we don't study the mistakes of the future we're doomed to repeat them for the first time.
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 10-2-2017 at 08:22


Quote: Originally posted by DraconicAcid  
The black solid formed by the reaction with ascorbate is probably metallic silver. Ascorbic acid is a reducing agent.


Why not silver(I) oxide?




there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8003
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 10-2-2017 at 11:29


Not silver(I) oxide. Silver(I) oxide, when formed in water, is not black, but dirty brown. This is hydrous silver(I) oxide. And indeed, ascorbate is a sufficiently strong reductor to reduce silver(I) to metallic silver. It also is capable of reducing copper(II) to copper(I).

With bleach you get silver(I) chloride, but you can get a black compound, silver(I) silver(III) oxide, AgAgO2. Hypochlorite is a very strong alkaline oxidizer and it is capable to oxidize silver to its +3 oxidation state. In this oxidation state it hydrolyses at once and forms a mixed oxidation state oxide.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 10-2-2017 at 13:01


Quote: Originally posted by woelen  
Not silver(I) oxide. Silver(I) oxide, when formed in water, is not black, but dirty brown. This is hydrous silver(I) oxide. And indeed, ascorbate is a sufficiently strong reductor to reduce silver(I) to metallic silver. It also is capable of reducing copper(II) to copper(I).

With bleach you get silver(I) chloride, but you can get a black compound, silver(I) silver(III) oxide, AgAgO2. Hypochlorite is a very strong alkaline oxidizer and it is capable to oxidize silver to its +3 oxidation state. In this oxidation state it hydrolyses at once and forms a mixed oxidation state oxide.

Silver (III) can be stabilized in water if complexed with ethylenebis(biguanide) and forms then a [ethylenebis(biguanide)silver(III) cation that can fix nitrate or perchlorate anion
--> [Ag(H2L)]3+ + 3 NO3(-) or 3 ClO4(-)...
Probably energetic ;):):cool::P




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 10-2-2017 at 14:21


Quote: Originally posted by woelen  

With bleach you get silver(I) chloride, but you can get a black compound, silver(I) silver(III) oxide, AgAgO2. Hypochlorite is a very strong alkaline oxidizer and it is capable to oxidize silver to its +3 oxidation state. In this oxidation state it hydrolyses at once and forms a mixed oxidation state oxide.


Thank you for the response
I read that silver hypochlorite is formed and disproportionates to silver chloride and silver chlorate

Edit(woelen): Fixed layout issue.

[Edited on 13-2-17 by woelen]
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8003
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 13-2-2017 at 00:06


I don't think that silver hypochlorite can form from bleach. Bleach is quite alkaline and under such conditions, you will get silver oxide. Even with pure hypochlorite, not containing chloride, I expect formation of the black mixed +1/+3 oxide.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
phlogiston
International Hazard
*****




Posts: 1378
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 13-2-2017 at 06:16


Can the slight turbidity observed with sulfate be explained by a slight contamination with lead?
What is the source of your silver nitrate?

When bleach is used to reclaim silver from the gelatine layer of x-ray film, one obtains a white precipitate of (what seems to me to be) silver chloride. When exposed to sunlight, it converts into a black powder. If kept in the dark, even though bleach is very alkaline it remains white for at least a few days. Addding concentrated NaOH converts the precipitate to a black powder 'instantly'.




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer