Hello fellow scientist!
I am trying to accurately measure particle sizes, I need to measure accurately to 10 microns (particles that are 10 microns).
The issue with an optical microscope is I would like to take pictures, and the cameras for them can be up to 100-200 dollars for a decent resolution.
I am guessing I will want 500X magnification at least? I see microscopes on Amazon for 200 that can do this, but everyone says the resolution sucks at
higher magnifications...
What should I do?
|
|
PHILOU Zrealone
International Hazard
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
This may help you:
Introduction Differential Sedimentation-particle size
and this too
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Texium
|
Thread Moved 14-2-2017 at 07:13 |
MineMan
National Hazard
Posts: 998
Registered: 29-3-2015
Member Is Offline
Mood: No Mood
|
|
Ah, interesting. Thank you
I do not have a centrifuge nor a detector though and I am afraid it might be hard to find a liquid where the chemicals (mostly oxidizer salts,
percolates and nitrates) are not soluble in.
|
|
PHILOU Zrealone
International Hazard
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
You can also simply allow a constant flow of solvant with the particles run horizontally from a tiny pipe and coming into a larger long and deeper
tank for sedimentation...finer particles will travel further while the larger ones will sedimentate faster...so you only need calibration with known
diameter particles (and density).
Fluid for oxidizer salts like perchlorates and nitrates...no problem use oil, benzine, naphta, white spirit, paraffin oil.
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
MineMan
National Hazard
Posts: 998
Registered: 29-3-2015
Member Is Offline
Mood: No Mood
|
|
Damn it Philou! why did you have to remind me of fluid dynamics.
|
|
PHILOU Zrealone
International Hazard
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Oups sorry .
When there is a specific and concise problem, there is often one or more solutions...now I agree that fluid flow dynamics is not the easiest matter,
but in this specific case it must be very handy...even if it calls for a memory refreshing and a travel back in time at the time of your studies .
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|