Author: Subject: Odd chromium chemistry - making sodium chromate
The Plutonium Bunny
Harmless
*




Posts: 21
Registered: 22-4-2015
Location: On an actinide asteroid
Member Is Offline

Mood: Fissile

[*] posted on 8-4-2017 at 17:09
Odd chromium chemistry - making sodium chromate


So I've been trying to get sodium chromate and potentially chromium oxide for thermite from stainless steel, and I've observed something rather unexpected. I dissolved the stainless in HCl and precipitated it with NaOH before using bleach to make a Na2CrO4 solution. This product is contaminated with bleach and salt, however.

I thought I would add HCl to push the equilibrium to the Na2Cr2O7 which I could then reduce with methanol - a method referenced on other chromate threads. The reduced chromium could be precipitated and calcined. To avoid chlorine production, I added a splash of household ammonia to convert the residual bleach to chloramines, which I boiled off. To the cooled solution I added HCl, but instead of turning orange, it fizzed and changed to green! This would appear to be a Cr (III) chloride solution.

Can someone explain what might be happening? This was just a small scale test, so I didn't measure anything. If, however, I could get some idea of what is going on, I could replicate this to make a bunch of Cr (III) to precipitate and use in thermite.

Alternately, a way of purifying the sodium chromate would be greatly appreciated. I attached a picture of the green solution and my contaminated chromate solution.

IMG_2502.JPG - 178kB




Deadlier than the Rabbit of Caerbannog
YouTube: https://www.youtube.com/channel/UCKA03pwhIrC9l7xP2rEb-VA
View user's profile Visit user's homepage View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 8-4-2017 at 17:34


I recently tried doing this and found that sodium chromate was kind of a pain to purify when it contained bleach. I found that it was actually pretty easy to get the sodium chloride to crystallize out but the other impurities didn't seem to separate as cleanly. You could precipitate some calcium chromate by adding concentrated calcium chloride solution. Calcium chromate is a bit of a pain to recrystallize unless you happen to know a better method for doing it than dissolving it in a calculated minimum amount of water, filtering and boiling off most of the water, but doing that isn't incredibly difficult. You could convert it to sodium chromate by adding a stoichiometric amount of sodium carbonate, or adding it very slowly and carefully as long as a chalky precipitate is produced.

I would think that bleach would react with ammonia to produce hydrazine, which decomposes and reduces chromates, but it's hard to say for sure exactly. Perhaps the bleach hadn't been reduced yet and formed hypochlorous acid with HCl which reacted more quickly with the ammonia, producing hydrazine, which reduced your product?

One idea I had that I didn't try was to decompose the chlorates by heating them in a crucible. I'm not really sure how dangerous that is, so I wouldn't attempt it on a large scale without trying it with a small amount first. Chromates can withstand pretty high temperatures as long as they aren't in a reducing environment.



[Edited on 9-4-2017 by JJay]




View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 8-4-2017 at 17:44


Oh and I wasn't personally trying to make thermite, but I would think that the iron sludge produced when preparing dichromates from stainless steel would probably have some utility there.



View user's profile View All Posts By User
tsathoggua1
Hazard to Others
***




Posts: 335
Registered: 8-1-2017
Location: Beyond the pale
Member Is Offline

Mood: Phosphorescent

[*] posted on 9-4-2017 at 12:15


You could potentially purify the chromium content as chromyl chloride. Salt would be an ideal impurity to have there. This would require removing the water (CrO2Cl2 is sensitive to H2O, and a powerful oxidizing agent, the synthesis is one that requires great care, because the mixture in the distillation flask will be extraordinarily corrosive, since it is composed of a mixture of a dichromate salt, NaCl and concentrated sulfuric (98% will do it)

But CrO2Cl2 is a distillable liquid, colored like unto bromine, it fumes in air, reacting with the traces of H2O, although it is not air-sensitive per se, just to the water content. The fumes are hydrogen chloride gas. The hypochlorite should be decomposed via the instability of hypochlorous acid, although given the strong dessicant nature of H2SO4, it would be wise to test this on a small scale, due to the exposive nature of the corresponding anhydride.
View user's profile View All Posts By User
The Plutonium Bunny
Harmless
*




Posts: 21
Registered: 22-4-2015
Location: On an actinide asteroid
Member Is Offline

Mood: Fissile

[*] posted on 9-4-2017 at 18:30


Thank you for your detailed and helpful replies. I love this forum. :)

I dried out another sample of the chromate solution and heated it for a few minutes in a test tube with a propane torch. Interestingly, it turned an orange color with heat but reverted back to its yellow state on cooling.

When I dissolved the cooled yellow powder, adding just a touch of HCl made it turn a nice bright orange (pictured below). Success! I added a splash of methanol and heated in some hot water, causing the color to change from orange to yellow and then to a blue-ish green (also seen below).

I added some NaOH, then not seeing any precipitate, added some HCl (thinking I had redissolved my chromium hydroxide as chromite). I added Na2CO3 and after a bit I saw a light blue almost cloud-color precipitate. This filtered off without problems to give the purple-ish stuff pictured below.

This ought to be pure chromium hydroxide, right? Am I correct in thinking that I could add this to a calculated amount of NaOH to make pure sodium chromate?

IMG_2505.JPG - 155kB IMG_2507.JPG - 298kB IMG_2508.JPG - 295kB




Deadlier than the Rabbit of Caerbannog
YouTube: https://www.youtube.com/channel/UCKA03pwhIrC9l7xP2rEb-VA
View user's profile Visit user's homepage View All Posts By User
woelen
Super Administrator
*********




Posts: 8102
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 10-4-2017 at 23:43


This purple stuff most likely is a basic complex of chromium(III) and formiate ion. In the oxidation of methanol you end up with formic acid, which in alkaline conditions is converted to formiate (HCOO(-)), which forms a complex with chromium(III). If you heat up this material to red hot, then I expect it to turn green, leaving Cr2O3 behind. I do not expect the purity of this material to be very good. Precipitates of this kind usually need thorough washing to get rid of all kinds of ions, trapped in the precipitate (in your case chloride and sodium ions).

This purple stuff is not chromium(III) hydroxide. The latter is green/grey.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
The Plutonium Bunny
Harmless
*




Posts: 21
Registered: 22-4-2015
Location: On an actinide asteroid
Member Is Offline

Mood: Fissile

[*] posted on 11-4-2017 at 18:25


Thank you for your informative insights. Would evaporating the reduced solution at room temperature or by heating work to get rid of the methanol oxidation products (thus preventing complexing)?

Also, is formation of the chloro complexes temperature dependent like the formation sulfato complexes? Would a chloro complex still precipitate chromium hydroxide on Na2CO3 addition? Ideally I would like to end up with chromium (III) oxide, and the Internet seems to know very little about these complexes.




Deadlier than the Rabbit of Caerbannog
YouTube: https://www.youtube.com/channel/UCKA03pwhIrC9l7xP2rEb-VA
View user's profile Visit user's homepage View All Posts By User
woelen
Super Administrator
*********




Posts: 8102
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 12-4-2017 at 05:13


Chromium forms coordination complexes very easily with many ligands. Once a ligand is attached, it is attached quite firmly and then you need prolonged heating or a lot of patience to have the ligand replaced again.

Temperature certainly has a strong influence on formation of complexes. In your case, removal of methanol oxidation products by heating does not work. Chromium most easily forms new complexes at the moment it changes oxidation state. For formation of certain complexes, the starting point is not a chromium(III) salt, but a chromium(VI) salt, which is reduced in the presence of the desired ligand. This is an advantage for many industrial processes, but in your case it is a disadvantage.
I think that the best option is to rinse precipitates you get as well as possible, and then calcine the precipitate to make reasonably pure Cr2O3.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Amos
International Hazard
*****




Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline

Mood: No

[*] posted on 12-4-2017 at 12:25


woelen, I've used sodium carbonate solutions to precipitate chromium(III) on many occasions, and the trend I've noticed is that the precipitate is initially pale blue or purple but with time (weeks) turns to a uniform light grey and seems to be accompanied by fluffy white particles. My theory after reading what you had to say in this thread might be that the complex eventually loses its ligands and yields chromium hydroxide and some sort of salt. Do you think I might even be remotely correct here?
View user's profile View All Posts By User
The Plutonium Bunny
Harmless
*




Posts: 21
Registered: 22-4-2015
Location: On an actinide asteroid
Member Is Offline

Mood: Fissile

[*] posted on 12-4-2017 at 18:46


Thank you all for the help! I am preparing some sodium chromate to test these things on as I am writing this post.

I have done some thorough searching, and think I've (maybe) found a solution to these complicated separations from stainless steel. Could the chloride solution from HCl dissolution simply be evaporated to get crystals and then dissolved in ethanol?

Please confirm if I am right or wrong, but I believe the nickel and iron chlorides would dissolve while the chromium chloride would stay as a solid. The ethanol would have to be free of water, of course.

[Edited on 13-4-2017 by The Plutonium Bunny]




Deadlier than the Rabbit of Caerbannog
YouTube: https://www.youtube.com/channel/UCKA03pwhIrC9l7xP2rEb-VA
View user's profile Visit user's homepage View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 12-4-2017 at 20:32


That's an interesting idea. I wonder if a Soxhlet extractor would work well for removing the nickel and iron chlorides.

I've been wondering about the best way to purify the nickel salts as well... it seems like such a shame to put nickel carbonates and hydroxides in the trash.




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8102
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 12-4-2017 at 23:15


Quote: Originally posted by Amos  
woelen, I've used sodium carbonate solutions to precipitate chromium(III) on many occasions, and the trend I've noticed is that the precipitate is initially pale blue or purple but with time (weeks) turns to a uniform light grey and seems to be accompanied by fluffy white particles. My theory after reading what you had to say in this thread might be that the complex eventually loses its ligands and yields chromium hydroxide and some sort of salt. Do you think I might even be remotely correct here?

Your observation is quite right. I have similar observations with chromium complexes. Ligands can be exchanged, but things go very slowly.
One nice experiment is the following:
- Dissolve some chrome alum or chromium(III) sulfate in distilled water. You get a purplish/blue solution of hexa-aqua chromium(III) ions.
- Heat the solution to near boiling: The liquid turns deep green. A very nice and beautiful color I must say.
- Allow the liquid to cool down. It remains green.
- Allow the liquid to stand at room temperature in a sealed bottle. Over time, the liquid slowly turns back to the purplish/blue color.
The green color is the color of a mixed sulfato/aqua-complex of chromium(III) and over the days or even weeks, the sulfate ligands are replaced by water ligands.

Similar experiences I also have seen with other ligands. E.g. when you add a precipitate of hydrous Cr(OH)3 (which also is a coordination complex, but a neutral one) to 10% or so ammonia, then over the days, the liquid turns purple/red, due to formation of ammine-complexes of chromium(III). This reaction also is very slow.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
woelen
Super Administrator
*********




Posts: 8102
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 12-4-2017 at 23:18


Quote: Originally posted by The Plutonium Bunny  
Thank you all for the help! I am preparing some sodium chromate to test these things on as I am writing this post.

I have done some thorough searching, and think I've (maybe) found a solution to these complicated separations from stainless steel. Could the chloride solution from HCl dissolution simply be evaporated to get crystals and then dissolved in ethanol?

Please confirm if I am right or wrong, but I believe the nickel and iron chlorides would dissolve while the chromium chloride would stay as a solid. The ethanol would have to be free of water, of course.

[Edited on 13-4-2017 by The Plutonium Bunny]

Ferric chloride is deliquescent and won't form crystals, the same is true for hydrated chromium(III) chloride. Nickel chloride may separate, but I'm not sure.
If you boil down the liquid, then you end up with basic chlorides.
I do not think this is going to work.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
The Plutonium Bunny
Harmless
*




Posts: 21
Registered: 22-4-2015
Location: On an actinide asteroid
Member Is Offline

Mood: Fissile

[*] posted on 13-4-2017 at 16:31


It seems like the main problem in getting pure chromates is the sodium chloride from the bleach step. Bypassing that would be a good choice.

If I precipitated the acid-dissolved SS with sodium carbonate and heated them to ensure they were oxides, could I make chromate from the oxides using just sodium hydroxide (no nitrate - this would add impurity just like the bleach)? Would this need to be fused or could I just use a hot concentrated solution?

On a side note, anyone have ideas for electroplating out chromium metal starting with a NaCl-contaminated chromate solution? Electrolyzing the solution resulting from methanol reduction of chromate with a graphite anode and copper cathode at ~3V did not seem to work (besides making bubbles and a chlorine smell).




Deadlier than the Rabbit of Caerbannog
YouTube: https://www.youtube.com/channel/UCKA03pwhIrC9l7xP2rEb-VA
View user's profile Visit user's homepage View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 14-4-2017 at 07:44


Elch Science on YouTube posted a video that showed a method that started with chromates and hydrogen peroxide. This seems unlikely to cause issues with chlorides.

It appeared to me when attempting to make sodium chromate from impure calcium chromate that that the sodium chloride separated cleanly at around 100 C before everything else. The solution also contained some sodium carbonate, which was much harder to separate. I did not rigorously verify that the solution contained no sodium chloride after seeing it separate, and indeed, the solution likely did contain small amounts, but recrystallization appeared to be a viable way of removing it. The chromyl chloride test could be used to check sodium chromate for chlorides.




View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 23-5-2017 at 07:37


i must pipe in and say calcium chromate has reverse solubility curve, its something like 4g/100mL at 0*C where its 0.8 at .. 80*C? (100*C probably less, presumably)

i dont see why you would have problems with seperating sodium chromate from bleach and sodium chloride, sodium chlorides solubility curve -- given that you work in reasonable amounts makes it quite easy to seperate

if you want to reduce, you could try ascorbic acid, it has some reducing potential, i wont promise you hole in one however




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 23-5-2017 at 07:57


Bleach will degrade to sodium chlorate, which is looks like it is probably kind of hard to remove.

Also, I don't think calcium chromate actually has a reverse solubility curve, despite what Wikipedia may say on the subject, although what data I have seen suggests that the hydrated form is much easier to dissolve than the anhydrous form. Most sources on the topic indicate that the dihydrate is more soluble at higher temperatures and less soluble at lower temperatures. I don't have very detailed data on its solubility, but if anyone does, you might want to fix the Wikipedia solubility table article.

[Edited on 23-5-2017 by JJay]




View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 24-5-2017 at 00:00


maybe fractional crystallization is whats required to seperate the chromate from chlorate, it seems like they really like to stick together
maybe one could turn the chromate into copper chromate, which isnt very soluble, in which chlorate variety of copper is, i recall the precipitate as being spongy blue-green, but as its copper it shouldnt take too long to seperate through gravity filtration as copper salts tend to be heavy

by crystallization i mean that you may be able to crystallize the chromate and chlorate very slowly and pick the large crystals apart, chromate and chlorate has somewhat similar solubilities even in potassium form, sadly




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 24-5-2017 at 00:18


Calcium chromate and chlorate have very different solubilities, but you're going to have a hard time using fractional crystallization to split potassium or sodium chlorate and chromate. I think you can destroy chlorates at high temperature if necessary.





View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 1-6-2017 at 01:06


just got to think of something
ehm, so we have 5% NaClO, one third of this, translating into 1.65% theretically from 5% bleach solution, IF IT DOES BREAK DOWN INTO CHLORATE -- and isnt used up in oxidizing the chromium carbonate to chromate
that isnt a whole lot
now i kinda get the point that you intend to use calcium hypochlorite, which is a bit more of hypochlorite, but for common bleach 1.65% chlorate isnt very much of a problem, and especially not when you are unlikely to first up break all of it down, secondly supposedly 50% of it isnt broken down into NaClO3, im thinking maybe a reducing agent could be added to take care of the chlorate, although it does seem to be decently stable in solution, it could mayhabs be acidified and reacted with a fuel although +30% chloric acid solutions are accidents waiting to happen, 30% concentration is far fetched when coming from bleach still i'd say




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User