You'll have sodium and/or potassium bisulfate if the pH is low enough and enough sulfuric acid is present... not sure exactly how that will make a difference....



This is my YouTube channel: Extreme Red Cabbage. I don't have much posted, but I try to do nice writeups once in a while.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1109
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 4-4-2018 at 15:51


That's an excellent point, and both of these are far more soluble than the sulfates. I think it's worth a shot.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 2924
Registered: 15-10-2015
Location: Western Hemisphere
Member Is Offline

Mood: :cool:

[*] posted on 4-4-2018 at 22:58


I'm thinking about dissolving some impure calcium chromate in water and dripping in sulfuric acid until I see no precipitate, filtering, and then adding an excess of sulfuric acid to see if I can get any chromium trioxide to precipitate. This seems like it might be a fairly dangerous experiment (especially if there are a lot of chlorides present), and I think a lot of sulfuric acid may be required, but I am pretty sure it will work....



This is my YouTube channel: Extreme Red Cabbage. I don't have much posted, but I try to do nice writeups once in a while.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1109
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 4-4-2018 at 23:49


Don't see why not. I don't see any reason for "titrating" the calcium, a slight excess of acid should be enough. With 10% sulfuric acid the precipitation was quite slow, producing a very dense ppt that was easy to filter off.
I would also concentrate the solution before trying to produce the trioxide, chromic acid is far more soluble than calcium chromate. This should remove more dissolved salts and reduce the amount of acid required.




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1109
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 6-4-2018 at 07:52


I give up. After acidifying it with sulfuric acid I added potassium carbonate in hope of precipitating potassium dichromate. No such luck. I did get a whiteish precipitate, but now the solution has turned an odd brown-green color. I don't know what I have anymore or how to deal with it, so I'm mothballing the project for now.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
Peterae
Harmless
*




Posts: 1
Registered: 24-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 24-4-2018 at 11:53


I've been following the process from here
http://lanthanumkchemistry.over-blog.com/article-how-to-sepa...

I'm at the Bleach stage which is incredibly slowwwww.

I'm getting a nice yellow though, with yellow crystals of Sodium Chromate on evaporation mixed with Sodium Chlorate from the bleach, maybe a little Sodium Chloride from the electrolysis process.

I need some ammonium hydroxide and have Ammonium Sulphate, I electrolytically made some Sodium hydroxide and will combine this with the Ammonium Sulphate and bubble the Ammonia gas through water and add this to my dried filtrate to get Nickle Amine.

[Edited on 24-4-2018 by Peterae]

[Edited on 24-4-2018 by Peterae]