Sticky Foam
Any idea what this can be for the substance?
https://youtu.be/1daq1QMynG4
|
|
EilOr
Harmless
Posts: 20
Registered: 12-12-2017
Member Is Offline
Mood: No Mood
|
|
Looks like a usual polyurethane to me
https://en.wikipedia.org/wiki/Polyurethane
In my country you can buy such a sticky foam (which looks and sticks exactly like the foam in the video) in bottles ready for use in hardware stores,
though with less pressure It has a very low density and is stickier than most
glues, almost impossible to remove from skin, clothes etc.. After a few hours it hardens to a slightly fragile hard sponge which is great for thermal
insulation
Though I don't know which PU it is
[Edited on 24-12-2017 by EilOr]
|
|
unionised
International Hazard
Posts: 5107
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
The squirt cans of foam are based on methylene diphenyl diisocyanate.
That's a bit toxic, but I guess that if the alternative is a bullet...
|
|