Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: The catalytic converter (platinum & PM) paradox of converting NOx, SOx and NH3
RogueRose
International Hazard
*****




Posts: 1590
Registered: 16-6-2014
Member Is Offline


[*] posted on 22-8-2018 at 11:27
The catalytic converter (platinum & PM) paradox of converting NOx, SOx and NH3


Last week I was researching the thread about using platinized quartz wool (heated) to convert NH3 +O2 into NO/NO2 and eventually HNO3 based upon the ostwald process. I also researched the contact process which stated that platinum used to be used as the catalyst to convert SO2 into SO3, also with addition of O2 I believe - but now V2O5 is preferred due to cost.

Now when I researched the catalytic converters the main goal of these is to keep things like NOx and SOx and even NH3 out of the atmosphere by converting them to N2 + H2O

Two-way cat

Quote:

A 2-way (or "oxidation", sometimes called an "oxi-cat") catalytic converter has two simultaneous tasks: Oxidation of carbon monoxide to carbon dioxide:
-2 CO + O2 → 2 CO2

Oxidation of hydrocarbons (unburnt and partially burned fuel) to carbon dioxide and water:
-CxH2x+2 + [(3x+1)/2] O2 → x CO2 + (x+1) H2O (a combustion reaction)



This is the process of a three way cat:
Quote:

Reduction of nitrogen oxides to nitrogen (N2)
-2 CO + 2 NO → 2 CO2 + N2
-hydrocarbon + NO → CO2 + H2O + N2
-2 H2 + 2 NO → 2 H2O + N2

Oxidation of carbon monoxide to carbon dioxide
-2 CO + O2 → 2 CO2

Oxidation of unburnt hydrocarbons (HC) to carbon dioxide and water, in addition to the above NO reaction
-hydrocarbon + O2 → H2O + CO2


The only thing it did say was that there is a problem with fuels (LNG & diesel) which contain sulfur because during combustion it produces SO2 and then further catalyzed to SO3 in the cat, which leads to "acid rain". Now I've heard that when SO3 + H2O mix (which should happen in exhaust) a very large amount of heat is released, and this should take place behind the cat and I would suspect that there is acutally sulfuric acid exiting the exhaust if not H2SO3 if the SO2 didn't oxidize in the process (maybe not enough O2 for this to happen?). Either way, the H2SO3 would probably turn into H2SO4 in the moist air - is that a correct assumption or am I missing something.

Now this whole idea seems to be counter intuitive to what is going on in the ostwald process and I am wondering if the pressure in the reaction tube (in the members experiement) is causing low yields).

What I would really like to do is figure out a way to use ammonium sulfate as a source for NH3 and SO2/SO3 and pass it through a reactor (platinum for the NH3 and V2SO5 for the SOx) as the decomp point of amm sulf is about 280F (relesaes NH3) and then about 660F (nice high temp to start the reaction in the reactor!) as the bisulfate where it releases NH3 and SOx (IDK if it is SO2 or SO3 it releases, if SO3 then no need for V2O5 I guess!). In addition I would like to use an O2 concentrator where a pipe flows behind the reactor (to pre-heat the O2 and cool the NO2 as it exits catalyst) and then is fed into the NH3 stream prior to the catalyst. If anyone sees problems with this, please let me know.

As a collection method for the gases I was thinking of a vertical stainless pipe (~2.5-3" diameter & 18-36" tall) filled with fiberglass insulation - the puffy stuff - and then have a mister spraying down on top of the glass wool with re-circulating water/acid. This should give a lot of surface area for the gases to contact as they rise through the column. I guess a cap could be inserted on this to feed any gasses to a bubbler but IDK how much more NOx/SOx would be present - maybe use H2O2 in the bubbler?

In the end you would have a mixture of sulfuric and nitric acid which would have to be distilled but I don' think that is the hardest part in most areas.

AS for the catalyst i'm working on a few ideas for support structure and have thought about using large grain Al2O3, the course stuff used in sand blasting to coat it with platinum and also V2O5 though I'm researching the best method for this. The Al2O3 seems to have a crystal structure (very rough) that may help support the catalyst where the pure SiO2 I've looked at seems very smooth and IDK how much can be supported without it flaking off especially at higher temps. Both of these are available in a range if sizes from pottery stores for very little $$.

Here are some compounds with very high melting points that are available at most pottery shops (or they can order them), most are very inexpensive. All temps are listed in F even if not noted.

MgO (5,200)
Fe3O4 (2,940F)
Fe2O3 (2832F)
Dolomite - (4700 - 8420F)
Calcium Silicate - (3,900F)
TiO2 - (3,350F)
SiO2 (pure quartz sand) - (3,115)
Al2O3 - (3,762F)
Silica gel (3,115)
Calcium magnesium Silicate (CaMgSiO4) - insulation temp rating of 2380F melts MUCH higher - great pourosity & comes in flexible insulation sheets -
Forsterite (Mg2SiO4) 3850F MP


https://en.wikipedia.org/wiki/Catalytic_converter

https://en.wikipedia.org/wiki/Ostwald_process

https://en.wikipedia.org/wiki/Contact_process
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 22-8-2018 at 11:52


I'm about to try something similar. I'm currently test firing some alumina mixed with about 10% bentonite clay. Both came from the local pottery store. The clay body looks very white. The alumina dilutes out the iron content of the bentonite.

It's a bit tough to handle when dry, as it remains rather fragile, but I was able to shape it with a knife. A sharp blade shaves it like butter. I'm firing it at 800°C for now, to see whether or not enough strength is gained at this temperature. I could go up as high as cone 10, but this is hard on the heating elements.

I'm actually awaiting the arrival of a pound of Veegum T. My pottery store ordered it for me. At $15/lb it's a bit pricey, but is used only in small quantities. The aforementioned link shows different articles made from alumina or zircon with only about 3% Veegum. So it's possible to make a ceramic with almost 100% alumina that is plastic enough to be thrown on a wheel and shaped. Interesting.

Two key terms that may be of use to you are selective catalytic reduction (SCR) and selective catalytic oxidation (SCO).




View user's profile View All Posts By User
nux vomica
Hazard to Others
***




Posts: 267
Registered: 18-7-2013
Member Is Offline

Mood: No Mood

[*] posted on 22-8-2018 at 16:15


I dont know if ether of you have seen these ceramic honeycomb blocks it might make things easier .


https://www.ebay.com/itm/80mm-SOLDERING-BOARD-CERAMIC-HONEYCOMB-SOLDER-BOARD-HEATING-/271640811782?_ul=AU

s-l400.jpg - 24kB




My YouTube channel Nux's channel
View user's profile View All Posts By User
Chemetix
Hazard to Others
***




Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 22-8-2018 at 17:24


The ostwald process seems to work at oxidising nitrogen rather than reducing it because there's no carbon in the mix. I'm unsure as to how the Ostwald scheme would work with SOx in the feed.

I postulated that SO2 in contact with NO2 should turn to SO3 and NO, where it would then re oxidise with excess air. The result should be a nitric sulphuric acid mix. A one stop acid plant producing the two most valuable acids would have to be of benefit to many out there.
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 22-8-2018 at 21:14


Quote: Originally posted by nux vomica  
I dont know if ether of you have seen these ceramic honeycomb blocks it might make things easier .


https://www.ebay.com/itm/80mm-SOLDERING-BOARD-CERAMIC-HONEYCOMB-SOLDER-BOARD-HEATING-/271640811782?_ul=AU



Looks like there are a lot of these floating around on eBay:
https://www.ebay.com/itm/25-TWENTY-FIVE-Ceramic-Honeycomb-Pi...


s-l1600.jpg - 191kB




View user's profile View All Posts By User

  Go To Top