Bubbling


Hi,

Any idea if the mixture of DI Water, H2O2 and NH4OH with the ratio 20:3:1 respectively creat bubbles when the mixture is agitated and heated up to 50 degrees celcius?
View user's profile View All Posts By User
vulture
Forum Gatekeeper
*****




Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 23-8-2003 at 02:25


It probably will create bubbles (oxygen) due to the decomposition of the hydrogen peroxide.

Now seriously, you could have figured this out yourself very easily. I guess this is a chemistry homework or something?




One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
View user's profile View All Posts By User
pyrochem
Harmless
*




Posts: 21
Registered: 1-1-2006
Location: United States
Member Is Offline

Mood: No Mood

[*] posted on 1-6-2006 at 14:34


It will also probably release ammonia (NH3) from the NH4OH.
View user's profile View All Posts By User
DeAdFX
Hazard to Others
***




Posts: 339
Registered: 1-7-2005
Location: Brothel
Member Is Offline

Mood: @%&$ing hardcore baby

[*] posted on 1-6-2006 at 15:04


Water will also be released (evaporation) to an extent.
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1071
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 1-6-2006 at 16:31


If you consulted the literature you would have found hydrogen peroxide is destabilzed by high pH solutions. In the presense of metals the peroxide is unstable in even strongly acid solutions.



Fellow molecular manipulator
View user's profile View All Posts By User
guy
National Hazard
****




Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline

Mood: Catalytic!

[*] posted on 1-6-2006 at 22:54


I read that H2O2 can oxidize ammonia to ammonium nitrite which decomposes to nitrogen. Is this true?



View user's profile View All Posts By User
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 11-6-2006 at 00:35


No, its not possible as far as i know, under any conditions of reaction. I do know for sure that just adding a H2O2 solution to an ammonia solution WILL NOT just react with each other



Ammonium nitrite does decompose into nitrogen. but if it is nitrogen gas you are trying to get, then there are some ways you can do it.

the first one is:

NaNO2 + NH4Cl = NaCl + 2H2O + N2
this one is done pretty easily from what i understand, but i have never done it so i cant really say.

And the second one is from this nice little site with a few other chemistry stuff on it

http://www.douchermann.a0tu.com/General_Chemistry.html#n2

The main reaction in this one is simply 4NH3(aq) + 3Ca(OCl)2(s) ---> 2N2(g) + 3CaCl2(s) + 6H2O(l)




View user's profile Visit user's homepage View All Posts By User
Zinc
Hazard to Others
***




Posts: 472
Registered: 10-5-2006
Member Is Offline

Mood: No Mood

[*] posted on 10-7-2006 at 02:20


Quote:
Originally posted by kclo4
The main reaction in this one is simply 4NH3(aq) + 3Ca(OCl)2(s) ---> 2N2(g) + 3CaCl2(s) + 6H2O(l)


Be careful with this reaction as side products can form wich are toxic (chloroamine and dichloroamine).