[*] posted on 6-12-2007 at 10:55
about Pt reduction


I wonder whether H2PtCl6 can be totally reduced to metal Pt when treated by Hydrogen only at room temperature?
and also what about Platinum acetylacetonate treated by hydrogen at room temperature?

any comments are welcome!
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 6-12-2007 at 11:25


At STP, no and no.



Neither flask nor beaker.