[*] posted on 22-6-2012 at 14:20


Well, the sodium nitrate is going to evaporate over the course of a week or two... (I should really make a dessicator bag, but I used all my remaining NaOH for this reaction...)



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 23-6-2012 at 06:22


Quote: Originally posted by elementcollector1  
Well, the sodium nitrate is going to evaporate over the course of a week or two... (I should really make a dessicator bag, but I used all my remaining NaOH for this reaction...)


You mean it's going to dry? I have force dried it [NaNO3] on a low light on a gas stove in a defunct stainless steel pan, no problems. Just keep stirring to avoid sticking and it's a 10 - 15 min job.

Another one that works really well is CaSO4 + 8/3 Al === > CaS + 4/3 Al2O3. CaSO4 is of course... wallfiller! This mixture can also be ignited with an Mg ribbon and burns like hell, possibly even hotter than chlorate/nitrate. It's best to dehydrate (by oven heating, 200 C does the trick) the wallfiller (it's a hemihydrate) to anhydrous CaSO4 but for ignition mixes that might not even be strictly necessary.

[Edited on 23-6-2012 by blogfast25]




View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 11-7-2012 at 14:25


Should I dehydrate the MnO2, or leave it as the brown hydrated form? (supposedly this is more active).



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 12-7-2012 at 04:57


Dry it at 150 - 200 C. No need to calcinate. But it must be quite dry for aluminothermy...



View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 12-7-2012 at 20:58


Well, it's drying fairly well in the open sun, so I could leave it to dry for two weeks while I'm in New York...



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
rannyfash
Hazard to Others
***




Posts: 113
Registered: 21-2-2012
Member Is Offline

Mood: No Mood

[*] posted on 13-7-2012 at 19:12


i have tried CuO/Mg thermite as a 'kewl' experiment, a possible source for atomised copper particles, can anyone explain why it deflagrates? Mg + CuO ==> MgO + Cu there is no difference in moles which usually causes the pressure difference in explosive reactions, does the extreme enthalpy change cause the air around it to expand? or am i overlooking something simple
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 13-7-2012 at 19:33


Copper thermites are known for being explosive. >:D



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 14-7-2012 at 17:15


How long should the MnO2 be in the oven? Golden brown? XD
But seriously, how many hours at about 150 C?




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 15-7-2012 at 05:35


Quote: Originally posted by elementcollector1  
How long should the MnO2 be in the oven? Golden brown? XD
But seriously, how many hours at about 150 C?


Depends a bit on how wet it was to start with, of course. A nicely dripped dry filter cake: about 1 - 2 hours, I'd say.




View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 26-8-2012 at 22:42


I heard mention of a molten MnCl2 - KCl eutectic a while back. What temp does this melt at? (Below 654 C is easily doable with a blowtorch, and electrolysis is only mildly hard with that setup).



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-8-2012 at 04:05


Quote: Originally posted by elementcollector1  
I heard mention of a molten MnCl2 - KCl eutectic a while back. What temp does this melt at? (Below 654 C is easily doable with a blowtorch, and electrolysis is only mildly hard with that setup).


The eutectic MP will be in that neighnourhood.




View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 27-8-2012 at 14:37


Well, I gave the Mn-thermite another go.
Attempt one: Ignition with blowtorched plaster of paris and aluminum. Failed.
Attempt two: Ignition with magnesium. Failed, just burned on the top without igniting anything.
Attempt three: Ignition with blowtorch. Partial success?
I got bits and pieces of the powder to ignite and melt together, and I did get one particularly good-sized, gray lump. The other lumps are all brittle-looking, gray to brown things, while this one looked more spherical while molten.
What should I do to reclaim a good-looking manganese sample (if the manganese is in there) from this mixture of Al2O3, Mn2O3, MnO2, Al, and hopefully Mn?

EDIT: Ah, nope. Just crumbly gray powder. I washed it in bleach to remove some of the aluminum (I think), but I think I'll just discard this particular experiment.

[Edited on 28-8-2012 by elementcollector1]




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 27-8-2012 at 17:26


Well, I had a potentially stupid but potentially game-changing idea. I read somewhere on this forum a while back (couldn't find OP even with search) that if one melted aluminum, topped it up with manganese dioxide, added more aluminum, added more MnO2, added more aluminum and so on, they would eventually have a container of manganese metal. (and aluminum, I suppose.) Is this a better idea? I have the materials to melt aluminum easily - I just don't think my powdered aluminum works, and it takes forever to make new stuff. (Old stuff was made from Al foil, notoriously bad source of aluminum.)



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 28-8-2012 at 05:01


Quote: Originally posted by elementcollector1  
Well, I had a potentially stupid but potentially game-changing idea. I read somewhere on this forum a while back (couldn't find OP even with search) that if one melted aluminum, topped it up with manganese dioxide, added more aluminum, added more MnO2, added more aluminum and so on, they would eventually have a container of manganese metal. (and aluminum, I suppose.) Is this a better idea? I have the materials to melt aluminum easily - I just don't think my powdered aluminum works, and it takes forever to make new stuff. (Old stuff was made from Al foil, notoriously bad source of aluminum.)


Well, it's worth a shot. Remember that the reduction reaction MnO2 + 4/3 Al === > Mn + 2/3 Al2O3 is very exothermic and now you'll carry out this reaction at > 660 C! Chances are that your Mn will form in the vapour phase!

Add your MnO2 really slowly, pinch by pinch, to see how you get on and be well prepared in terms of fire and heat protection.

You'll also need to look up 'Al Mn alloys', to figure out what will happen to any formed Mn: will it dissolve in the Al bath? At first glance it seems Mn solubility in Al is somewhat limited.



[Edited on 28-8-2012 by blogfast25]




View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 28-8-2012 at 08:22


Although I believe MnAl (an intermetallic) was mentioned a while back as well. I think that if I add enough MnO2 slowly, then the Al will react with that instead, leaving the Mn alone.



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 28-8-2012 at 09:00


EC1:

Whatever you do with this, be really careful. Assuming the MP of Al is high enough to get the reaction going every time some MnO2 hits the Al melt, then each time you will get a burst of enthalpy being released. Vaporous Mn is a real possibility!

Another problem is the slag (alumina): will it form in the molten state? Of course it will then solidify as its MP (2,054 C, IIRW) is much higher than the MP of Al.

All in all this could be a really interesting experiment but with serious potential danger to the experimenter. Add the aliquots of MnO2 using a long armed ladle or something like that.




View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 28-8-2012 at 12:03


Ja, I know. That's why I mentioned the idea being possibly stupid. However, it would ensure a reaction, which is better than what I've been getting.
Also, tried electroplating of manganese again today. Surprise! A silvery coating formed. It's thin, but I think it could get thicker if I'm careful about it.
Setup:
9V battery
Beaker 1: Dilute MnCl2 (anolyte)
Beaker 2: Saturated MnCl2 (catholyte)
Anode: 60/40 solder
Cathode: Copper PCB, unetched
I have to keep brushing it every few minutes, otherwise it builds up an oxide coating, but yay!




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 28-8-2012 at 19:57


So, how do I build up enough Mn to rip it off? (More importantly, how do I remove the copper foil from the PCB blank without etching?)



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 29-8-2012 at 04:31


Hmmm... geting the experimental conditions for viable plating correct isn't so easy. Are you sure the build up is actually oxide? Search for patents in that field, I'd say.



View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 29-8-2012 at 10:09


I searched, and found that a concentrated catholyte is good, a cold solution is better, etc.
The plate is for the most part, bright, shiny silvery metal. Some black is visible, but that's to be expected.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 30-8-2012 at 04:22


Quote: Originally posted by elementcollector1  
I searched, and found that a concentrated catholyte is good, a cold solution is better, etc.
The plate is for the most part, bright, shiny silvery metal. Some black is visible, but that's to be expected.


Very nice. Buff it or polish it and put it in your collection. Recovering it would be hard, I guess industrially they obtain thick coatings/crystals and somehow scrape off the metal, then ingot it.




View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 30-8-2012 at 11:17


Well, I really just need to remove it from the PCB board.



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
 Pages:  1  2

  Go To Top