Bert
Super Administrator
       
Posts: 2822
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
Fumed silica has been used with NM
Attachment: Nitromethane and amine explosives gelled with fumed silica.pdf (2MB) This file has been downloaded 872 times
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
|
DrManhattan
Harmless
Posts: 32
Registered: 24-1-2015
Member Is Offline
Mood: No Mood
|
|
Fumed silica worked a treat in a ratio of 25% AL, 4% Fumed Silica, 71% PLX.
|
|
|