Separate hydrocarbons from polyuerethane ?
How to separate hydrocarbons from polyurethane(PU) ? the hydrocarbons are naphtha, c5-c12. I got a 70% PU and 30% naphtha, viscous liquid from a paint
shop, i wanted use PU for something i want, so i just bought it thinking that i can purify it somehow by removing the naphtha, however i searched on
the web for like half an hour and did not find anything like boiling point of PU so... my plan to boil away the naphtha still not sure, i think PU
might thermally decompose but theres little info, any one have any ideas or links ?
many thanks.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Where is this naphtha supposed to be? In uncured PU component liquids? In polymerised PU? As a chain extender?
I've never heard of naphtha in a PU context.
|
|
KonkreteRocketry
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 165
Registered: 12-11-2012
Location: Dubai
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by blogfast25 ![](images/xpblue/lastpost.gif) | Where is this naphtha supposed to be? In uncured PU component liquids? In polymerised PU? As a chain extender?
I've never heard of naphtha in a PU context. |
It is mixed with PU cus its Polyurethane Varnish.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Is it a one component system?
|
|