Anyone here tried to dissasemble NiMH battery?
I would like to obtain nickel from it and dissolve it but it seems rather scary to open it because I heard of them bursting into flames and fuming.
Anyone experienced with what I should expect and safety measures? I mean if it enflames should I put the whole battery into a jar of water?
These are two AA batteries that have lost their positive caps, probably their time has passed..
|
|
|
confused
Hazard to Others
 
Posts: 244
Registered: 17-3-2013
Location: Singapore
Member Is Offline
Mood: tired
|
|
MSDS for NiMH battery
http://data.energizer.com/PDFs/nickelmetalhydride_psds.pdf
short version:
contains mix of metals(possibly flammable) and corrosive metal hydroxides
try not to short out the battery when dismantling it
wear glove and goggles when dismantling
in case of fire or fumes flood the area with water(any suitable smothering agent, sand .etc) and let it burn out, ventilate the area.
i dont recomend picking it up when it starts to fume/burn, usually its pretty hot at that point...
[Edited on 19-8-2013 by confused]
|
|
|
Gooferking Science
Hazard to Self

Posts: 97
Registered: 17-7-2013
Location: Somewhere in Kansas, USA...
Member Is Offline
Mood: Halogenated
|
|
My advice would be to do the disassembly outside with good ventilation. You also need face, hand, and body protection. The main problem I've
encountered when disassembling batteries is accidentally shorting them out. This causes internal heating which may cause explosion and/or fire. Good
luck!
|
|
|
Random
International Hazard
   
Posts: 1120
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
I'll try to get face protection along with a bucket of water and a bucket of dillute acetic acid.
If battery gets on fire ill throw it in a bucket of water, if I get some metal hydride on myself I'm going to wash my hands and put them into vinegar.
Will report results.
|
|
|
Oscilllator
National Hazard
  
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
I have disassembled such a battery. I obtained what I think was nickel metal. It dissolved slowly in acid to give green solutions, but I imagine this
will be very impure. When you unroll the battery, there will be two tapes. One is a stainless steel mesh covered in gunk and the other is the nickel.
Be careful, because the electrode covered in gunk spontaneously catches on fire!
I found this to be an unsatisfactory source of nickel, so I purchased some nickel electrodes from here:
http://www.haines.com.au/index.php/electrodes-nickel-75-x-25...
Edit: These batteries are a bugger to open! Its almost as if they don't want people to get into them or something. I found the best way to open them
was a chisel and some judicial applications of kinetic energy.
[Edited on 27-8-2013 by Oscilllator]
|
|
|
eidolonicaurum
Hazard to Self

Posts: 71
Registered: 2-1-2014
Location: Area 51
Member Is Offline
Mood: Hydric
|
|
I have opened loads of these batteries, and they have never caught fire etc. They are difficult to get into though, but there a lot of nickel in some
form inside them. I dissolve up the innards in acid, then allow the nickel sulphate to crystallise out. What's left (eventually) is a bunch of rare
earth salts, which is what I was after in the first place. They are perfectly safe to open.
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
And I didn't even know that... live and learn.
|
|
|
MFrancoZ
Harmless
Posts: 1
Registered: 26-1-2014
Location: México
Member Is Offline
Mood: No Mood
|
|
Use fully discharged batteries.
Cut with a small saw.
the best source of nickel, are canadian coins 10 c. (1962-1981) 4.5g, and 25 cents. (1969-1999) 5g.
|
|
|
Zyklon-A
International Hazard
   
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
NiMH batteries contain: Lanthanum, cerium, neodymium, and praseodymium.
|
|
|