Mood: No Mood

[*] posted on 5-12-2014 at 19:50


That all sounds pretty good. I would probably dilute the acid to avoid it reacting too quickly, but it is likely fine as is. Be careful not to add too much carbonate to your acid at once or it will foam over.

Also, if ground joint glassware is available to you, you may consider adding the acid via addition funnel to a slurry of the carbonate in a 2/3 neck flask to contain the barium-rich aerosol as much as possible. Just something to consider.
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 734
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 5-12-2014 at 20:11


Thanks, I do have ground joint glassware so I will try it with a two-neck round bottom flask and addition funnel.
View user's profile View All Posts By User
Justin Blaise
Hazard to Self
**




Posts: 82
Registered: 5-10-2011
Location: Parts Unknown
Member Is Offline

Mood: No Mood

[*] posted on 6-12-2014 at 07:23


Woelen has some great notes on making barium salts here;

http://woelen.homescience.net/science/chem/exps/BaCl2_2H2O/i...

There will be some amount of solid that won't dissolve no matter how much acid you add, if you're using pottry grade material. I found that letting it settle for a long time was the easiest solution, rather than trying to filter the extremely fine particles.
View user's profile View All Posts By User
otonel
Hazard to Self
**




Posts: 84
Registered: 9-4-2005
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2014 at 13:24


Squall you can make barium nitrate by boiling barium carbonate with calcium nitrate like in this patent http://www.google.com/patents/US2010046
I have two question:
- if I make electrolysis of a solution of barium sulfate can obtain barium hidroxide?
-can obtain barium nitrate by electrolysis a solutions of barium sulfate and calcium nitrate?
I want to resolve that misery theoretical first because I don`t have much time to make that kind of experiments and i ask about decomposition of barium sulphate electrolytically because thermal decomposition need high temperature and barium sulfate is available for me as radiocontrast agent
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2538
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 29-12-2014 at 13:47


Barium sulfate is highly insoluble, so you won't be able to dissolve it for the electrolysis.



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
nezza
Hazard to Others
***




Posts: 324
Registered: 17-4-2011
Location: UK
Member Is Offline

Mood: phosphorescent

[*] posted on 30-12-2014 at 00:38


Barium sulphate is difficult to convert to other barium salts. It can be converted to Barium carbonate in an equilibrium by repeated boiling with alkali carbonate, filtering, washing and reaction with acid to dissolve the barium carbonate formed.
View user's profile View All Posts By User
Squall181
Harmless
*




Posts: 46
Registered: 21-2-2011
Member Is Offline

Mood: No Mood

[*] posted on 30-12-2014 at 05:44


It's interesting to see such an old post of mine again. I've learned a lot since those days .

Greenlight your posted procedure is how I make my barium nitrate these days too.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 30-12-2014 at 06:19


Quote: Originally posted by nezza  
Barium sulphate is difficult to convert to other barium salts. It can be converted to Barium carbonate in an equilibrium by repeated boiling with alkali carbonate, filtering, washing and reaction with acid to dissolve the barium carbonate formed.


Or glow it with an excess carbon at red heat for a prolonged time:

BaSO4 + 2 C === > BaS + 2 CO2




View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 734
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 30-12-2014 at 07:45


Squall, do you use 62% nitric acid as well?
Does anyone know how to purify the Barium nitrate so it can be used effectively in green colour compositions?
I read on a patent that you can wash it with ice cold (0.degrees) low concentration nitric acid solution, would this work or is there a better way?
View user's profile View All Posts By User
Justin Blaise
Hazard to Self
**




Posts: 82
Registered: 5-10-2011
Location: Parts Unknown
Member Is Offline

Mood: No Mood

[*] posted on 30-12-2014 at 08:41


Barium nitrate solubility in water shows decent temperature dependence, so you could try the conventional recrystallization once you let the fine solids settle out.
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 30-12-2014 at 10:05


Please remember to handle carefully! Check toxicity, Barium carbonate was used as RAT POISON.

Avoid using any Sodium compounds if you want this for green flames, small traces of Sodium yellow/orange will ruin a Barium green.

Start with a very pure Barium compound, Strontium is present in most technical grade materials. Sr is quite difficult to chemically separate from Ba- and will also ruin green flames in surprisingly mall amounts.

If cost was no object, I would choose reagent grade Barium carbonate & nitric acid.

Also consider Barium peroxide as a colorant and oxidizer-

http://www.privatedata.com/byb/pyro/pfp/tracers.html#Tracers...

[Edited on 30-12-2014 by Bert]




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
otonel
Hazard to Self
**




Posts: 84
Registered: 9-4-2005
Member Is Offline

Mood: No Mood

[*] posted on 30-12-2014 at 13:10


Cheddite Cheese You have right about barium sulfate solubility, what I think was to fiind an easy way to make barium nitrate .
I find another patent about making barium sulphide from barium sulfate using lower temperature then using just carbon or charcoal US4795625
Can be replaced barium nitrate with lead nitrate or calcium nitrate in some pyrotechnic recipes?
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 31-12-2014 at 08:12


Quote: Originally posted by otonel  
Can be replaced barium nitrate with lead nitrate or calcium nitrate in some pyrotechnic recipes?


Not if a bright green is what you're after.

Finely ground BaSO4 should also be reduced in a 'thermite-style' reduction with Al powder:

BaSO4 + 8/3 Al === > BaS + 4/3 Al2O3

This should burn very brightly at over 2,500 C (end temperature). The cooled, crushed mass would then be lixiviated with dilute HCl or HNO3 and filtered, to obtain the respective barium salt and much H2S. The annealed alumina doesn't dissolve in dilute acids.

This method avoids using a furnace altogether.

[Edited on 31-12-2014 by blogfast25]




View user's profile View All Posts By User
nezza
Hazard to Others
***




Posts: 324
Registered: 17-4-2011
Location: UK
Member Is Offline

Mood: phosphorescent

[*] posted on 31-12-2014 at 17:00


The best green colour flame is obtained with Barium chlorate. This is occasionally available on Ebay and gives a really deep green flame colour.
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 1-1-2015 at 14:17


Quote: Originally posted by Squall  
I have always wanted to distill my sulfuric acid to get the dye out of it

Seeing as the thread's been revived, i'll add that you can remove the colouring from drain cleaner H2SO4 by adding some 3% H2O2 and then boil until it fumes.

Well before it fumes, the colour has gone.

When it fumes, you have a clue as to the concentration of the acid.

No distillation aparatus required.

[Edited on 1-1-2015 by aga]




View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 1-1-2015 at 14:47


Quote: Originally posted by nezza  
The best green colour flame is obtained with Barium chlorate.


Oddly enough, men and women seem to differ on that perception. I recall that some blind tests of green star mixtures by a US pyrotechnic club showed men leaned towards the Barium chlorate greens, with women trending toward preferring the Barium nitrate greens.




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 18-1-2015 at 08:52


This is not the right thread for that question, in addition, use the edit button rather than posting again. To answer your question, while it technically is possible, there is no reasonable way to do this. It is possible however through a metathesis reaction with barium chloride and sodium chloride. This will leave a sodium contaminated product which will need to be purified if used for pyrotechnics.
View user's profile View All Posts By User
The Volatile Chemist
International Hazard
*****




Posts: 1981
Registered: 22-3-2014
Location: 'Stil' in the lab...
Member Is Offline

Mood: Copious

[*] posted on 18-1-2015 at 12:33


Quote: Originally posted by not_important  
Squall,
sounds a lot like the one here http://www.sciplus.com/category.cfm/subsection/4/category/42...

Distilling nitric acid takes a bit of care, rubber stoppers can make it tricky.

I use something similar to UI-3830 here http://www.uicoglass.com/distillingah.htm which minimizes the number of joints to deal with.

Isothermal distillation is slow, but gets you away from the need to heat stuff, and to worry about what hot nitric acid is going to do to your apparatus.

The best one sciplus sells is their one entitled 'essential oils' (they always have joke titles for their products), it's all-glass and usually $95, has a coil condenser, and some other nice stuff. Haven't purchased it, though.




View user's profile Visit user's homepage View All Posts By User
Deathunter88
National Hazard
****




Posts: 517
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 21-2-2015 at 23:56


Quote: Originally posted by Xenoid  
Quote:
Originally posted by Fleaker
@ Xenoid, would it not be easier to just dissolve BaCO3 in dilute HNO3 or am I missing something obvious?


Yeah! Good one! Whoops!

I naturally assumed he would not have nitric acid (the holy grail), I don't either!
Whereas hydrochloric acid is fairly readily available in most hardware stores.

Also, once you have your Ba in solution as the chloride, it's in a somewhat more useful form than the carbonate. I made up a large batch of concentrated solution, a fairly smelly procedure with pottery barium carbonate.

Regards, Xenoid

[Edited on 22-8-2007 by Xenoid]


Opposite for me, I can get concentrated nitric acid for a few dollars a pint. But I can't for the life of me get concentrated sulphuric and hydrochloric acid. Guess everyone has their own problems. lol