Best way to Synthesize Zinc Sulfide


I made a video on making Zinc Sulfide (glow in the dark powder) but my results of it is actually pretty bad... only a few bits glowed and thet was from intensive lighting with a black light... the method i used was Zn + S = ZnS... but is this this the best way? im thinking of placing a Sulfide salt in HCl, make H2S gas and bubble it though a Soluble Zinc compounds (sulfate for example... this would produce ZnS + H2SO4 if im correct) Would the Sulfuric Acid produce react with the Zinc Sulfide produced? is this a good way on making a good batch of glow in the dark powder or is there a better way to get zinc sulfide?

Below is my Zinc Sulfide Video

http://www.youtube.com/watch?v=9zEDtYPcAjc




View user's profile Visit user's homepage View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 4-9-2011 at 04:44


By your own admission your stuff is heavily contaminated. Your initial mix didn't even look particularly well mixed to me. Permanganate/glycerol introduced more contamination.

I believe there are some threads on this forum on ZnS. Search and yee shall find!

It can also be made by precipitating it from a Zn2+ solution with a water soluble sulphide. Maybr that's easier to control than a flash powder? The 'wet method' requires good control of pH, otherwise your product will hydrolyse (redissolve).


[Edited on 4-9-2011 by blogfast25]




View user's profile View All Posts By User
Endimion17
International Hazard
*****




Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline

Mood: speeding through time at the rate of 1 second per second

[*] posted on 4-9-2011 at 04:52


Why not merging those threads? The topic is essentially the same.



View user's profile Visit user's homepage View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 4-9-2011 at 04:55


http://www.sciencemadness.org/talk/viewthread.php?tid=9490#p...

... for starters.




View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 7-9-2011 at 18:51


One cited preparation of ZnS is by passing H2S into a buffered zinc salt solution adjusted to a pH of 3. It forms a white precipitate.

Example:

ZnCl2 + H2S --> 2 HCl + ZnS (s)
View user's profile View All Posts By User
Chemistry Alchemist
Hazard to Others
***




Posts: 403
Registered: 2-8-2011
Location: Australia
Member Is Offline

Mood: No Mood

[*] posted on 7-9-2011 at 19:45


How do i control the pH? i dont have anything to use? I thought Zinc Sulfide was Yellow?



View user's profile Visit user's homepage View All Posts By User
IrC
International Hazard
*****




Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline

Mood: Discovering

[*] posted on 7-9-2011 at 21:15


Quote: Originally posted by Chemistry Alchemist  
How do i control the pH? i dont have anything to use? I thought Zinc Sulfide was Yellow?


http://en.wikipedia.org/wiki/Zinc_sulfide

"Zinc sulfide is a white to yellow-colored powder or crystal."

You really need to spend more time doing research. It will save you much unneeded work and questions.

Forgot to add but study adding silver as an activator to make some nice scintillation screens for Gamma radiation. Old tech but cool to watch in the dark.


[Edited on 9-8-2011 by IrC]




"Science is the belief in the ignorance of the experts" Richard Feynman
View user's profile View All Posts By User
Chemistry Alchemist
Hazard to Others
***




Posts: 403
Registered: 2-8-2011
Location: Australia
Member Is Offline

Mood: No Mood

[*] posted on 7-9-2011 at 23:14


Yeah i apologise about that, soon after i posted it, i went onto wiki ans read about it, i spend ALOT of time doing research actually, sometimes doing it all day just on one topic




View user's profile Visit user's homepage View All Posts By User
The WiZard is In
International Hazard
*****




Posts: 1617
Registered: 3-4-2010
Member Is Offline

Mood: No Mood

[*] posted on 8-9-2011 at 09:29


Quote: Originally posted by Chemistry Alchemist  
Yeah i apologise about that, soon after i posted it, i went onto wiki ans read about it, i spend ALOT of time doing research actually, sometimes doing it all day just on one topic


I would suggest expanding you research beyond the back
of cereal box's, and searching in a language which you are
proficient in.


1 — Try these
http://tinyurl.com/Zink-sulphide-Popular-Science
http://tinyurl.com/Zink-sulphide-Henry
2 — Put your check in the mail please.
View user's profile View All Posts By User
TheNaKLaB
Hazard to Self
**




Posts: 51
Registered: 18-9-2011
Location: Australia
Member Is Offline

Mood: Elastic

[*] posted on 19-9-2011 at 03:40


I would mix stoichiometric amounts of sulfur and zinc and put it in a test tube. Heat for about 10 minutes so that the sulfur melts and reacts with the zinc.
It could be quite dangerous if the mixture ignites though.




http://www.youtube.com/user/TheNaKLaBScience

"Aerodynamically, the bumble bee shouldn't be able to fly, but the bumble bee doesn't know it so it goes on flying anyway" - Mary Kay Ash
View user's profile Visit user's homepage View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 19-9-2011 at 11:58


Quote: Originally posted by TheNaKLaB  
I would mix stoichiometric amounts of sulfur and zinc and put it in a test tube. Heat for about 10 minutes so that the sulfur melts and reacts with the zinc.
It could be quite dangerous if the mixture ignites though.

That's odd because I'd not try heating a mixture fairly commonly used as rocket fuel in a glass container.
Once the reaction starts it will ignite- rather vigorously

I'd prefer this sort of thing
http://www.naasjournal-ng.org/files/2009/pdf/239-244(vol10_no3_2009).pdf
though I accept that you need to be careful with the thiourea.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 19-9-2011 at 12:39


Quote: Originally posted by unionised  
That's odd because I'd not try heating a mixture fairly commonly used as rocket fuel in a glass container.
Once the reaction starts it will ignite- rather vigorously



An expendable ceramic teacup or similar, embedded in (a small bucket of) dry sand, will do. Thermal shock will crack the 'crucible' but won't (obviously) melt it, Gently prize it out of the sand and recover the product. That's how I do all my thermites.




View user's profile View All Posts By User
TheNaKLaB
Hazard to Self
**




Posts: 51
Registered: 18-9-2011
Location: Australia
Member Is Offline

Mood: Elastic

[*] posted on 19-9-2011 at 21:22


I've done this experiment many times and had much success. Zinc and Sulfur don't spontainasly combust like flash powder, but act more like a thermite reaction.





[Edited on 19-09-2011 by TheNaKLaB]




http://www.youtube.com/user/TheNaKLaBScience

"Aerodynamically, the bumble bee shouldn't be able to fly, but the bumble bee doesn't know it so it goes on flying anyway" - Mary Kay Ash
View user's profile Visit user's homepage View All Posts By User

  Go To Top