rollercoaster158
Harmless
Posts: 34
Registered: 21-4-2012
Location: Looking through your window
Member Is Offline
Mood: Compiling...
|
|
Chlorine released?
I had some thin iron rods, and no use for them. I decided to make some iron oxide, so I stuck them in a salt (NaCl) solution. A week later, there was
plenty of orange/red iron oxide in the container, but the faint smell of chlorine. Does iron/iron oxide cause NaCl to decompose into sodium and
chlorine? It's not a lot of chlorine, but a detectable amount that I am curious about.
|
|
|
hissingnoise
International Hazard
   
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Something in the water?
|
|
|
CrEaTiVePyroScience
Hazard to Self

Posts: 71
Registered: 14-4-2012
Location: Belguim
Member Is Offline
Mood: Explosive
|
|
Well I think I can answer this question , because I have also made iron oxide that way and got some youtube videos about but anyways back to topic.
You added NaCl to the water to increase its conductivy because you are running electric current through it.
There are several reactions happening:
1. 2 H2O -> 2 H2 + O2 the water is splitting up in two gasses, hydrogen and oxygen due to electrolysis the oxygen causes the iron nails which are
acting as cathodes and anodes to rust. (Rusting is nothing more then something being exposed to oxygen Fe + 3 O2 --> 1 Fe2O3.) So the O2 gas is
escaping on the nail and running over it , causing it to rust.
2. NaCl is splitting up in chlorine gas due to the electrical current and will produce chlorine gas, the amounts of the gas should not be
underestimated. At the start most of the gas will dissolve in the water, creating bleach but when the water is saturated with the gas, the gas will
escape.
SOLUTION: To make the iron oxide you don't have to use NaCl to increase the conductiviy of the water but you can also add somethingelse , I am sorry I
can't remember the name of the product that I added because its too long ago but you can google it!
[Edited on 6-5-2012 by CrEaTiVePyroScience]
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Creative: rollercoaster makes no mention of a current (even though that is a common hobbyist way of making ferric oxide).
I have a much simpler explanation: anyone who has handled solutions of ferric compounds will attest to a specific odour, I’m not sure what causes
it. But it’s somewhat reminiscent of faint chlorine and could be easily mistaken for it. Unless you have other evidence that you’re observing
actual chlorine, that is the most likely explanation…
Chlorine solutions can be detected by adding them to potassium iodide solution with some soluble starch mixed in: 2 I<sup>-</sup> +
Cl<sub>2</sub> == > I<sub>2</sub> + 2 Cl<sup>-</sup>. Starch forms a deep blue complex with iodine, detectable
even at low iodine concentrations.
|
|
|
CrEaTiVePyroScience
Hazard to Self

Posts: 71
Registered: 14-4-2012
Location: Belguim
Member Is Offline
Mood: Explosive
|
|
@Blogfast25 Oh that's right looks like I read to fast ,sorry for that.
@rollercoaster158 But its quite awkward to make iron oxide with a NaCl solution and without current? I mean if you use current your yield would be
ALOT higher. Just adding 4.5v will atleast tripple your yields perhaps even more.
Another way to find out is to add just normal food coloring or ink to the water before you let it stand for a week. If after a week, the solution has
lost (some) color, it indicates that chlorine gas was produced. (Even small amounts of chlorine gas will make the water lose it's color)
[Edited on 6-5-2012 by CrEaTiVePyroScience]
|
|
|
bbartlog
International Hazard
   
Posts: 1139
Registered: 27-8-2009
Location: Unmoored in time
Member Is Offline
Mood: No Mood
|
|
Although no voltage was applied, there may still be a small internally generated current. Iron is attacked by atmospheric oxygen, O2. The oxygen in
tearing the electrons from the iron might generate enough of a potential that in some places Cl- would in turn lose an electron, being oxidized to Cl.
Certainly there has to be some reduction or oxidation of Na+ and/or Cl- taking place, else what role would it be playing in accelerating this
reaction?
The less you bet, the more you lose when you win.
|
|
|
rollercoaster158
Harmless
Posts: 34
Registered: 21-4-2012
Location: Looking through your window
Member Is Offline
Mood: Compiling...
|
|
Yes, I know that I can assist production by adding a current. However, I had a lot of time to do it and decided to skip that. I have no means to tell
whether it's chlorine, it just smells like chlorine. It could have been the iron oxide, who knows. By the looks of it it's red iron oxide
(Fe2O3).
|
|
|
AndersHoveland
Hazard to Other Members, due to repeated speculation and posting of untested highly dangerous procedures!
   
Posts: 1986
Registered: 2-3-2011
Member Is Offline
Mood: No Mood
|
|
I am very doubtful that any chlorine was produced in your reaction. But it is not entirely beyond the realm of possibility. Fe+2 ion solvated
in water could potentially react with oxygen from the air to transiently form complexed superoxide as an intermediate. It could be possible that this
superoxide is oxidizing some of the chloride ions to chlorine.
If this is actually correct, the formation of chlorine would only be a very small part of the overall reaction. Most of the chlorine would just
rapidly oxidize the iron, and be reduced back to chloride, but some of it might be able to escape.
|
|
|
woelen
Super Administrator
       
Posts: 8146
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I'm absolutely sure that no chlorine was formed in this reaction, not even a trace. Chlorine is very reactive and certainly is not formed
spontaneously under the conditions you describe. It might be some impurity in the iron, the salt or the water, which gives a similar smell.
An interesting test may be to make a very small amount of real chlorine and compare its smell with your salt/iron smell. Take 1 big drop of bleach and
one big drop of acid (e.g. dilute hydrochloric acid) and add these to each other in a glass or plastic cup and carefully smell the cup. DO NOT USE
MORE THAN SINGLE DROPS. You'll notice the chlorine, even from this single drop. Compare this with the smell from your salt/iron setup. Are they really
the same?
[Edited on 7-5-12 by woelen]
|
|
|
hissingnoise
International Hazard
   
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Bromate?
|
|
|