Author: Subject: Titanium compounds out of TiO2
papaya
National Hazard
****




Posts: 615
Registered: 4-4-2013
Member Is Offline

Mood: reactive

[*] posted on 26-6-2014 at 09:04
Titanium compounds out of TiO2


Hi everyone,
I own an amount of pure TiO2 powder, that for no surprise is very inert - it will not dissolve in boiling HCL, HNO3, etc (quite concentrated), which is confirmed by addition of hydrogen peroxide to solution (no coloration observed). The only thing that worked a LITTLE so far was melting with NH4HSO4 - after dilution with water the H2O2 gave intense orange-red coloration, but still only small fraction of TiO2 reacted. The goal is to prepare some water soluble, stable to hydrolysis Ti salts, is titanium (IV) or titanyl nitrate a possibility ? If this works I plan to use it in anode coating experiments.
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 26-6-2014 at 10:02


It won't be very easy, but it is possible. It does react with hot (boiling) sulfuric acid, as well as hydrofluoric acid:

TiO2+ 2 H2SO4 → Ti(SO4)2 + 2 H2O

Or:
TiO2 + H2SO4 → TiOSO4 + H2O

And:
TiO2 + 6 HF → H2TiF6 + 2H2O

http://product.lookchem.com/item/24/properties-of-titanium-d...

[Edited on 26-6-2014 by Zyklon-A]




View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 972
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 26-6-2014 at 10:25


With the help of some of our other posters here, I dissolved TiO2 into molten NaHSO4.H2O in a test tube. The test tube survived for at least several runs.

In short, 0.4g of TiO2 dissolved into 3.2g of molten NaHSO4.H2O to form a transparent yellow melt. Upon dissolution into cold water, no residue was noted.

http://www.sciencemadness.org/talk/viewthread.php?tid=27624&...
View user's profile View All Posts By User
papaya
National Hazard
****




Posts: 615
Registered: 4-4-2013
Member Is Offline

Mood: reactive

[*] posted on 26-6-2014 at 12:21


What soluble product exactly did it form, WGTR? Can I really use NH4HSO4 instead? Also - if I manage to dissolve it, is it possible to get it back as a hydrated oxide or even carbonate with NaHCO3 solution, since I want to prepare nitrate, will it be gel like or powder that can be filtered?
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 972
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 26-6-2014 at 12:49


In the presence of water, it's more like TiOSO4. If a weak solution is refluxed for a hour or two, the salt hydrolyzes, precipitating out some amorphous hydrated form of titania. This wet precipitate will still have some sulfate in it, but will generally be easier to react with other concentrated acids than your (likely) dead-burned powder. Good luck trying to filter it. It needs to be precipitated out, either with a centrifuge, or by letting it sit for a day or so. If it doesn't settle out, then perhaps dialyzing the solution and/or heating it gently will help: http://www.sciencemadness.org/talk/viewthread.php?tid=27624&...

I have no idea whether ammonium bisulfate will work or not. I got the sodium bisulfate at a pool supply store. I'm really a one-trick pony when it comes to titanium chemistry. I haven't done much with it.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 26-6-2014 at 12:49


@papaya:

Dissolving TiO2 is a hard nut to crack, although it depends a lot on what grade it is.

My latest batch of food grade Anatase didn't dissolve even the slightest little bit on 3 hours of boiling with 98 % H2SO4!

Other grades will be slightly more amenable to dissolution with H2SO4. HF is of course out of the question for most amateurs.

Fusion with NaHSO4 will work with some grades. It will work better than NH4HSO4.

With my stubborn Anatase I resorted to fusing with twice the weight in KOH. This forms potassium titanate, which after cooling and on treatment with plenty of water then hydrolyses to TiO2:

K2TiO3(s) + H2O(l) === > 2 KOH(aq) + TiO2(s)

But this freshly prepared TiO2 (Ti(OH)4?) is much, much more soluble in H2SO4.

The salts of Ti(IV) are all titanyl salts, as far as I now: titanyl sulphate for instance is TiOSO4 = TiO<sup>2+</sup> + SO<sub>4</sub><sup>2-</sup>. These salts are very prone to hydrolysis and I'm not sure they can even be isolated from their solutions by straightforward methods (like evaporation).

[Edited on 26-6-2014 by blogfast25]




View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 26-6-2014 at 12:53


Quote: Originally posted by blogfast25  
These salts are very prone to hydrolysis and I'm not sure they can even be isolated from their solutions by straightforward methods (like evaporation)

CHRIS25 can do this. Oh yes. I'm a Believer.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 26-6-2014 at 12:58


And I need proof.



View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 26-6-2014 at 13:06


Can't prove or disprove a Belief, which is VERY convenient (for me) !



View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1120
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 26-6-2014 at 13:49


Damn aga you sure know how to go offtopic sometimes. And yes I know my post doesn't help that at all.
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 972
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 26-6-2014 at 14:03


Papaya, this should answer your questions:

Analytical chemistry, Volume 1, Frederick Pearson Treadwell, William Thomas Hall - J. Wiley & sons, inc., 1921



Ti_1.jpg - 164kB Ti_2.jpg - 195kB Ti_3.jpg - 129kB Ti_4.jpg - 199kB Ti_5.jpg - 151kB Ti_6.jpg - 188kB Ti_7.jpg - 154kB Ti_8.jpg - 164kB Ti_9.jpg - 99kB
View user's profile View All Posts By User
papaya
National Hazard
****




Posts: 615
Registered: 4-4-2013
Member Is Offline

Mood: reactive

[*] posted on 26-6-2014 at 14:26


Thanks WGTR, quite informative. So it appears that after fusion one gets titanium sulfate, but then
https://www.sciencemadness.org/whisper/files.php?pid=335947&...
it's transformed inti titanyl in solution?
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 27-6-2014 at 05:23


Quote: Originally posted by papaya  
it's transformed inti titanyl in solution?


It seems the Ti(IV) salts can only exist in solution as titanyl salts (solutions of). Pure TiCl<sub>4</sub> is a covalent, liquid (STP) compound, not an ionic solid.

Ti(III) salts like TiCl<sub>3</sub> and Ti<sub>2</sub>(SO<sub>4</sub>;)<sub>3</sub> do appear to exist as salts of [Ti(H<sub>2</sub>O)<sub>6</sub>]<sup>3+</sup>. Some can be isolated, or so I've read. The (III) sulphate forms alums with Cs and Rb, possibly with NH4.

[Edited on 27-6-2014 by blogfast25]

[Edited on 27-6-2014 by blogfast25]




View user's profile View All Posts By User
sasan
Hazard to Self
**




Posts: 92
Registered: 22-2-2014
Location: TEHRAN / IRAN
Member Is Offline

Mood: Radiative

[*] posted on 28-6-2014 at 03:13



Maybe it can be useful:http://titanium.atomistry.com/titanium_dioxide.html
Its about titanium dioxide and other titanium compounds that you can't find anywhere else.

[Edited on 28-6-2014 by sasan]
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2014 at 03:36


Would Ammonium Bi-Fluoride be strong enough for a route to the fluoride salt and then be further displaced to whatever salt you're trying to form?
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2014 at 05:51


Quote: Originally posted by hyfalcon  
Would Ammonium Bi-Fluoride be strong enough for a route to the fluoride salt and then be further displaced to whatever salt you're trying to form?


That's a good question. NH4HF2 isn't very suitable for fusions because of it low MP and tendency to decompose (into NH4F + HF!) when heated. It's certainly something that should NEVER be attempted outside of a good fume hood.

So that leaves using it in concentrated solution. I've used 50 w% NH4HF2 solutions to dissolve freshly prepared Zr(OH)4 and that's not easy either despite the fact that zirconium (IV) forms a strong complex with fluoride ions (hexafluoro zirconate anions). That dissolution requires some excess of NH4HF2 and modest heating.

For that reason I think attacking hard calcined TiO2 with NH4HF2 will probably not work so well. I could be wrong on that.

Freshly prepared hydrated titania ("Ti(OH)4") however would be quite responsive to NH4HF2, yielding (NH4)2TiF6 (or variants thereof). The problem is then to displace the fluoride ions with whatever you fancy: as the hexafluoro titanate complex is a strong one, that will not be easy either.

[Edited on 28-6-2014 by blogfast25]




View user's profile View All Posts By User
papaya
National Hazard
****




Posts: 615
Registered: 4-4-2013
Member Is Offline

Mood: reactive

[*] posted on 28-6-2014 at 07:39


HF and similar things, though available to me, aside from being toxic are inconvenient since you must forget about GLASS vessels when working with them (or not? )
I retried fusion with NH4HSO4, this time I held it longer at high T - it's shitty, the melt bubbles and decomposes after(!) addition of TiO2 with white fumes and strong AMMONIA(!) odor (at lower temp it turns to solid). At the end I obtained yellow colored hard porous chunk, that partially dissolved in cold water and most if not all TiO2 precipitated at once. H2O2 test gives yellow color this time (not red :O ), but I think 99% of TiO2 is not dissolved. I don't have any NaHSO4 to do it right way for now...

Btw. red peroxide compound formed with Ti4+ solution seems very stable - it's still the same color after few days - any information about known Ti peroxo complexes ? is it similar to CrO8 (3-) anion? Would be a nice goal to prepare and isolate such a compound in free state.

[Edited on 28-6-2014 by papaya]
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 28-6-2014 at 07:46


Quote: Originally posted by papaya  
At the end I obtained yellow colored hard porous chunk, that partially dissolved in cold water and most if not all TiO2 precipitated at once. H2O2 test gives yellow color this time (not red :O ), but I think 99% of TiO2 is not dissolved. I don't have any NaHSO4 to do it right way for now...


I've no idea whether any titanium/titanyl sulphate formed in your experiment but if it did then dissolving the frit in water is not a good idea: it causes any titanium (IV) to promptly hydrolyse (to hydrated titania). Ti (IV) compounds need a very low pH to stay in solution (except for hexafluoro titanates).

Try once more but this time try and dissolve the frit in 30 % H2SO4.

You could also try and treat that first precipitate with conc. H2SO4 to see if you get any dissolution.

[Edited on 28-6-2014 by blogfast25]




View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 972
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 28-6-2014 at 19:41


Quote: Originally posted by papaya  

I retried fusion with NH4HSO4, this time I held it longer at high T - it's shitty, the melt bubbles and decomposes after(!) addition of TiO2 with white fumes and strong AMMONIA(!) odor (at lower temp it turns to solid). At the end I obtained yellow colored hard porous chunk, that partially dissolved in cold water and most if not all TiO2 precipitated at once. H2O2 test gives yellow color this time (not red :O ), but I think 99% of TiO2 is not dissolved. I don't have any NaHSO4 to do it right way for now...
[Edited on 28-6-2014 by papaya]

I couldn't find the same sort of information on titania, but here is what happens when magnesia is reacted with molten
ammonium pyrosulfate (which is what you have when you heat up your ammonium bisulfate ). Note that ammonia is given off:

ammonium_pyrosulfate.jpg - 55kB

Encyclopedia of the Alkaline Earth Compounds,
Richard C. Ropp
Newnes, Dec 31, 2012

Potassium pyrosulfate (or bisulfate) is recommended over sodium pyrosulfate, as it appears that the sodium salt gives off
SO3 more readily on overheating. However, either one can be used it care is taken when heating. I used the
sodium salt when fusing TiO2 in a test tube, and it worked fine. Sodium bisulfate is used to lower pH in pools, and
can be found in practically every hardware or pool supply store. It dehydrates to sodium pyrosulfate after fusion.
Attachment: Vries69thermal.pdf (259kB)
This file has been downloaded 616 times

Whatever salt you use, when dissolving the TiO2 the melt should be gently heated until all the titania dissolves to a
clear, transparent melt. If this doesn't happen, there is probably not enough extra pyrosulfate salt in the melt. Titanium
sulfate melts at a very high temperature (not sure of the exact number), and extra pyrosulfate is needed to ensure that
everything stays molten at a sufficiently low temperature.

Also, titanyl sulfate does tend to hydrolyze in water, but I didn't notice it happening too quickly at room temperature. This may
have been the result of the excess bisulfate left over from the melt. I stored 10% stock solutions of the previously fused mass
into water. Over a period of weeks only mild decomposition was noticed.

Edit:
On the other hand, if you can dissolve TiO2 into a sufficient excess of molten ammonium pyrosulfate, perhaps the excess
ammonia could be removed more easily than the extraneous metal salts could, perhaps by extended heating above 400-500C
(Attachment: t091a25-1.pdf (258kB)
This file has been downloaded 613 times).



[Edited on 6-29-2014 by WGTR]
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 29-6-2014 at 04:14


Quote: Originally posted by WGTR  
[
Also, titanyl sulfate does tend to hydrolyze in water, but I didn't notice it happening too quickly at room temperature. This may
have been the result of the excess bisulfate left over from the melt. I stored 10% stock solutions of the previously fused mass
into water. Over a period of weeks only mild decomposition was noticed.



Yes, with excess bisulphate left the pH will have been kept low. Also, 10 % TiOSO4 is fairly low. In the older sulphate process, titania was precipitated from titanyl sulphate/ferrous suphate solutions essentially by strongly diluting with water: dilute the acid reserve and the hydrated titania drops out.

Your remarks on potassium pyrosulphate remind me of another reaction reported here by 'plante' and 'garage chemist': heating a mixture of TiO2, NaCl and potassium pyrosulphate yields vapours of TiCl4!




View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4729
Registered: 11-1-2014
Location: Salt Lake City
Member Is Online

Mood: Seeking gainful employment

[*] posted on 29-6-2014 at 10:22


And if you were to produce TiCl4, you could reduce that with aluminum or preferably hydrogen to make TiCl3, which would be an easy feedstock for other titanium compounds.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 29-6-2014 at 13:16


Quote: Originally posted by zts16  
And if you were to produce TiCl4, you could reduce that with aluminum or preferably hydrogen to make TiCl3, which would be an easy feedstock for other titanium compounds.


TiCl4 is very hard to handle though: all moisture has to be avoided or you've got a smoke bomb on your hands.




View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4729
Registered: 11-1-2014
Location: Salt Lake City
Member Is Online

Mood: Seeking gainful employment

[*] posted on 29-6-2014 at 13:41


Yeah, I guess you'd have to dry your reaction vessel extremely well and then channel the TiCl4 gas into another vessel where it reacts with hydrogen, and then TiCl3 would crystalize in there. At least I think that would be a possible way to go about it. It's all purely speculative on my part. It would be VERY cool to see two colorless gases combine and form a purple solid.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 30-6-2014 at 04:33


Actually, in spite of claims on how hard it is to attack TiO2, the protective layer on Titanium metal, some exciting research that suggests otherwise!

Per this source, a noted manufacturer of resistance Titanium alloys (see this source https://www.google.com/url?sa=t&source=web&rct=j&... ), there are a couple of paths that even an a home chemist may wish to explore.

First, and most exciting, if one were to scrap (that is, mechanically damage) some mildly heated Ti metal in an atomsphere of very dry (and mostly oxygen free) chlorine gas, the metal may even start to burn! To quote from material prepared by Titanium Metals Corporation:

"Dry chlorine can cause rapid attack on titanium and may even cause ignition if moisture content is sufficiently low (Table 2).(3)However, one percent of water is generally sufficient for passivation or repassivation.."

A cooled area of a vessel in which this ignition occurs could collect, most likely, anhydrous Titanium chloride, but I am not sure how practical this is really for the home chemist or for any large scale work.

Based on essentially the same chemical reaction and electrochemistry (my guess, some galvanic corrosion also) concentrated aerated solutions of AlCl3 and ZnCl2 appear to corrode the metal as well.

I must explore some of these paths when I acquire the metal.

[Edited on 30-6-2014 by AJKOER]
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 30-6-2014 at 04:50


AJ:

The metal dissolves in hot 37 % HCl and similar concentration hot H2SO4 quite easily, as I've demonstrated on this forum a few times. For the Ti(III) sulphate concentrations of 30 w% and higher can be achieved (personal experience) in a matter of 30 mins to 1 hour. But that says NOTHING about highly calcined commercial TiO2 and how it responds to acids.

Anhydrous TiCl4 is hard to handle, no matter how you prepare it.

Titanium powder ('sponge' as it's called) is readily available from eBay sellers, not expensive either. Pyros use it to produce white sparks of burning Ti particles. Direct union with oxygen or chlorine is probably possible at higher than RT temperatures.




View user's profile View All Posts By User