Idiocy in action; don't be me


Well, i printed a .25 calibre starter pistol. NO SAFETY. dumb dumb dumb. Loaded some HOT blanks--black powder fortified with magnalium--really pretty at night by the way.

Fast Forward.

My dog died, alcohol WAS involved along with grief, and I got to screwing with my blanks. Bear in mind, I'm almost sixty and been messing with dangerous things all my life and KNOW BETTER. Hear me youngsters....

My wonky trigger let loose with my fingertip in the wrong place. OOPS

Lost about 3/4 inch. Even with the sharpie mark.



finger.jpg - 990kB




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4484
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Online

Mood: Semi-victorious.

[*] posted on 18-12-2022 at 10:15


Yikes! I am so sorry for your loss- both your dog and your finger.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
ManyInterests
International Hazard
*****




Posts: 1024
Registered: 19-5-2019
Member Is Offline


[*] posted on 18-12-2022 at 11:19


Holy shit! the worst I have is a small scar on my hand and picric acid stains on my fake wood floor. This stuff is dangerous.

And I'm a gun guy and I want to make homemade smokeless propellants and priming compounds.

Stories like these make me feel really wary of what might happen.
View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 18-12-2022 at 11:30


Kinda why I posted this.............at least not as bad an outcome as "Life after detonation". If I can save one kids life that reads this I've done well.



"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 18-12-2022 at 11:34


Ouch, really sorry to hear this. I hope it heals cleanly, quickly and without too much discomfort.
Very brave of you to share.
View user's profile View All Posts By User
ManyInterests
International Hazard
*****




Posts: 1024
Registered: 19-5-2019
Member Is Offline


[*] posted on 18-12-2022 at 11:37


The worst thing is just how sudden these things happen. You think everything is going OK then... BAM! It happens! This is what happened when a single drop of red fuming nitric acid fell on my hand and I wasn't wearing gloves. I didn't even trust the vinyl gloves that should protect against fuming nitric acid (I trust them now that I've tested them) and I have a scar I need to look at every time I see my hand.

This is a scary thing.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4484
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Online

Mood: Semi-victorious.

[*] posted on 18-12-2022 at 11:43


Hopefully your Secret Santa hadn't sent you new gloves....



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Energetics-testin
Hazard to Self
**




Posts: 53
Registered: 7-6-2022
Location: Canada,Quebec
Member Is Offline


[*] posted on 18-12-2022 at 12:05


I've had an accident similar to your story..I had bought 100 rounds of .25 Ramset blanks...I was taking out the smokeless powder first then I would put them on the side to extract the priming compound(lead styphnate I think)..

After like 30 rounds I became tired and decided to go have a drink and finish after..

After my break,I was a litlle drunk and scrapped the priming compound with a metal pick..it detonated in my face...thankfully no injuries..but my eyes burned for 2 days straight after that..

Ever since,I've stopped ''playing'' with blanks..And now I use them carefully and with respect.

Thanks for sharing your story.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 18-12-2022 at 12:36


All the best and speedy recovery!



View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6462
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 18-12-2022 at 14:00


Quote: Originally posted by DraconicAcid  
Hopefully your Secret Santa hadn't sent you new gloves....


Or socks.
View user's profile View All Posts By User
MadHatter
International Hazard
*****




Posts: 1369
Registered: 9-7-2004
Location: Maine
Member Is Offline

Mood: Enjoying retirement

[*] posted on 18-12-2022 at 14:25
Sorry


Arky, as we discussed earlier I'm lucky I only lost my eyebrows to Armstrong's
mixture. Could have been much worse. Be safe for the holidays my friend.
Sorry to hear about the loss of your dog. Nobody likes losing long time pets.
For me it was a chocolate Labrador earlier this year. He was my buddy.




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 18-12-2022 at 14:57


Quote: Originally posted by B(a)P  

Very brave of you to share.


Other people need to hear this stuff. Complacency sets in EASY.




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
Hey Buddy
Hazard to Others
***




Posts: 444
Registered: 3-11-2020
Location: Bushwhacker Country
Member Is Offline


[*] posted on 18-12-2022 at 23:18


I hate safeties. Sorry to hear about your dog.
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2900
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 19-12-2022 at 10:32


Arkoma,

Sorry to hear about the finger, and the dog. Hope it heals OK and you can find a new dog as well. Merry Christmas.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8149
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 19-12-2022 at 23:51


Arkoma, I find it brave that you shared this with us. Thumbs up for sharing and warning!
I wish you a good recovery! I wish you a good Christmas, despite this nasty event!




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Phosphor-ing
Hazard to Others
***




Posts: 254
Registered: 31-5-2006
Location: Deep South, USA
Member Is Offline

Mood: Inquisitive

[*] posted on 20-12-2022 at 13:30


Sorry about your finger. I too recently lost my dog. I can relate to the alcohol/grief stupor you speak of. Fortunately I don’t dabble in energetics.
Wishing you a quick recovery.




"The nine most terrifying words in the English language are: 'I'm from the government and I'm here to help.'" -Ronald Reagan
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1497
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline

Mood: Good

[*] posted on 20-12-2022 at 19:06


See if they'd just go ahead and let people use fireworks for Christmas season... You wouldn't have been messing around with a dragon's breath pistol. Well maybe you would have IDK. Point is, bottle rockets sound fun and hard to set off on accident. Sounds like a blinding revelation of what can go wrong. Levity aside, ouch! I hope your a good sport with the ribbing.

Rough go loosing the tip of your finger. Wishing you a speedy recovery Arky. About your loss, well that will heal, just more slowly. We've said goodbye to a lot of furry friends over the years. Down to one grumpy cat, 16+ YO. I feel ya there man.
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1641
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 21-12-2022 at 07:20


Sorry for the lose, some wounds cut very deep and losing a loved one is deff a very very deep one.

The real issue here was the alcohol in the end, it asks for a huge price that is rarely worth the fleeting temporary cold comfort it offers.

I hope you heal well, on all fronts.
View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 21-12-2022 at 23:11


Quote: Originally posted by violet sin  
e I hope your a good sport with the ribbing.


Yes, I'm good with it, in fact it is EXPECTED.

The thing is, in Ark-In-Saw, you can practically buy dynamite over the counter for Fourth of July and New Year's Eve.




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
specialactivitieSK
Hazard to Self
**




Posts: 94
Registered: 21-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 25-12-2022 at 09:00


https://www.facebook.com/reel/821389625983945?s=yWDuG2&f...
View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 10-1-2023 at 16:37


condolences - on the bright side, microneedling can help to make scarred skin look normal within weeks- depending. has crackling balls never been fired out of a gun before?



~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 993
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 10-1-2023 at 18:01


Be grateful for a lesson learned.
Im thankful you shared this with the world,
I am hoping it will protect others

It does not matter
how many times you have done something
nor how skilled you are
or how well prepared you may be
This may have a high price, but it's cheap compared to
the "what could have been"
December 25, 2014. 10:43am
Doing something ive done 1000s of times.
BOOM
PPE saves lives.

My arc flash suite was peppered with molten copper and steel
Shrapnel from my hard hat penetrated 1/4in thick steel cabinets behind me
face shield was atomized, safety glasses melted to my head
fireproof shirt charred and fell apart
zipper was welded shut and my paints on fire under my apron.
gloves burnt off my hands
Cell phone was melted in my pocket, bluetooth melted in my ear
contact lenses melted and surgicly removed from my eyes
1st degree across the entire front of my body, and i mean EVERYTHING
3rd to my face and hands.
35 days of pain management, 19 months of physical addiction and detox
Still burns to this day
I am blessed to say im alive.
20141228_075159 (1).jpg - 1.6MB




"You can't do that" - challenge accepted
View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 11-1-2023 at 15:44


Oh wow. That was pretty catastrophic Rainwater. I'm sure your friends and family do indeed think it is Madness (pun intended...) that you are still involved in this avocation.

Yes, I DO HOPE that this post breaks through at least one persons complacency. Thanks for your addition to it, Wow,

Edit

Healing well.



20230111_174724.jpg - 326kB

[Edited on 1-11-2023 by arkoma]




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6462
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 11-1-2023 at 16:15


So, you lost all the way down to the first knuckle? Or is there some fingertip bone left?



View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 11-1-2023 at 21:55


To here:



20230111_235401.jpg - 753kB




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
 Pages:  1  

  Go To Top