Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Stabilization of iron(II) by acids
SnailsAttack
Hazard to Others
***




Posts: 175
Registered: 7-2-2022
Location: The bottom of Lake Ontario
Member Is Offline


[*] posted on 24-2-2023 at 04:09
Stabilization of iron(II) by acids


I've read that acids are supposed to inhibit the air oxidation of iron(II) salts. Can someone explain how that's supposed to work?

For instance, iron(II) sulphate should oxidize in water by the following formula:

12FeSO₄ + 2H₂O + 3O₂ -> 4Fe₂(SO₄)₃ + 4FeO(OH)

Aside from redissolving the iron oxyhydroxide as iron(III) sulphate, why would the presence of sulphuric acid prevent this reaction from occurring?




View user's profile Visit user's homepage View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1252
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 24-2-2023 at 10:05


I think because of electrode potentials.

Fe3+ + e- <--> Fe2+ E°= 0,771 V

Fe(OH)3 + e- <--> Fe(OH)2 + (OH)- E° = -0,56 V

Fe2+ solutions doesn't contain Fe(OH)2, but there is still some hydrolysis in which some basic salt is formed. Acid prevent hydrolysis.

Acid however doesn't stop oxidation of Fe2+. Acidic Fe2+ solutions are still sensitive to air.
View user's profile View All Posts By User
SnailsAttack
Hazard to Others
***




Posts: 175
Registered: 7-2-2022
Location: The bottom of Lake Ontario
Member Is Offline


[*] posted on 25-2-2023 at 02:18


Quote: Originally posted by Bedlasky  
I think because of electrode potentials.

Fe3+ + e- <--> Fe2+ E°= 0,771 V

Fe(OH)3 + e- <--> Fe(OH)2 + (OH)- E° = -0,56 V

Fe2+ solutions doesn't contain Fe(OH)2, but there is still some hydrolysis in which some basic salt is formed. Acid prevent hydrolysis.

Acid however doesn't stop oxidation of Fe2+. Acidic Fe2+ solutions are still sensitive to air.
So what you're saying is that the acid just redissolves any hydrolyzed iron(II) salts? Like this:

FeSO₄(aq) + 2H₂O(l) <-> H₂SO₄(aq) + Fe(OH)₂(s)

Also, I found a relevant post about this: https://chemistry.stackexchange.com/questions/31243/what-is-...

[Edited on 2/25/2023 by SnailsAttack]




View user's profile Visit user's homepage View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 25-2-2023 at 03:44


Quote: Originally posted by SnailsAttack  
I've read that acids are supposed to inhibit the air oxidation of iron(II) salts. Can someone explain how that's supposed to work?

For instance, iron(II) sulphate should oxidize in water by the following formula:

12FeSO₄ + 2H₂O + 3O₂ -> 4Fe₂(SO₄)₃ + 4FeO(OH)

Aside from redissolving the iron oxyhydroxide as iron(III) sulphate, why would the presence of sulphuric acid prevent this reaction from occurring?


It's largely driven by the extreme insolubility of Fe(OH)3.nH2O: Ksp approx. 10-39 (!)

This causes the oxidation II to III to be favoured in neutral/alkaline conditions.

It also explains why Mohr's salt is much more stable than FeSO4, the latter which oxidises even in the solid (dry) form.




View user's profile View All Posts By User
teodor
International Hazard
*****




Posts: 1142
Registered: 28-6-2019
Location: Netherlands
Member Is Offline


[*] posted on 25-2-2023 at 05:11


Practically it is possible to store Fe(II) salts solutions for years without oxidation if you don't open the bottle too often and use something lile ParaFilm.
I have Fe(SCN)2 test solution which was kept in a bottle for 1 year and it is still colorless. It turns pink on air very quickly, so you probably can use this reagent to check how effective different ingibitors could work. And yes, the soluition contains HCl, and it doesn't inhibit oxidation much.

Update: for preparation of Fe(II) salt solution you can make it acidic and filter to the storage bottle through Zn powder. Addition of Fe(SCN)2 can help to check the solution if not spoiled.


[Edited on 25-2-2023 by teodor]
View user's profile View All Posts By User
SnailsAttack
Hazard to Others
***




Posts: 175
Registered: 7-2-2022
Location: The bottom of Lake Ontario
Member Is Offline


[*] posted on 26-2-2023 at 00:55


Quote: Originally posted by teodor  
Practically it is possible to store Fe(II) salts solutions for years without oxidation if you don't open the bottle too often and use something lile ParaFilm.
I have Fe(SCN)2 test solution which was kept in a bottle for 1 year and it is still colorless. It turns pink on air very quickly, so you probably can use this reagent to check how effective different ingibitors could work. And yes, the soluition contains HCl, and it doesn't inhibit oxidation much.

Update: for preparation of Fe(II) salt solution you can make it acidic and filter to the storage bottle through Zn powder. Addition of Fe(SCN)2 can help to check the solution if not spoiled.

I'm actually more interested in this behavior for its geochemical implications. This summer I observed that a sample of acid-rich volcanic fumarole salts seem to contain iron(II) despite being exposed to air for months or even years.

Additionally, iron-oxidizing bacteria rely on the presence of iron(II).




View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6462
Registered: 4-10-2014
Location: At home
Member Is Online

Mood: Most of the ducks are in a row

[*] posted on 26-2-2023 at 04:26


Something like this?




View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4729
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Seeking gainful employment

[*] posted on 26-2-2023 at 08:09


In that scenario, I would guess it has a lot to do with the local atmosphere produced by the volcanic activity. Fumaroles are constantly belching out gases that are not oxygen. The major gases released are either reducing agents, like H2S and SO2, or inert to redox, like CO2 and water. It’s forming an area that is locally devoid of oxygen, making it a reducing atmosphere rather than the oxidizing atmosphere we are accustomed to!



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
SnailsAttack
Hazard to Others
***




Posts: 175
Registered: 7-2-2022
Location: The bottom of Lake Ontario
Member Is Offline


[*] posted on 27-2-2023 at 06:06


Quote: Originally posted by j_sum1  
Something like this?

Well, that looks a lot cooler than where I was but yeah I think it's geologically similar. The fumarole was underneath a street, leaking salts onto the sidewalk (see attached pictures). Tasted extremely acidic. Still analyzing the sample I took.
Quote: Originally posted by Texium  
In that scenario, I would guess it has a lot to do with the local atmosphere produced by the volcanic activity. Fumaroles are constantly belching out gases that are not oxygen. The major gases released are either reducing agents, like H2S and SO2, or inert to redox, like CO2 and water. It’s forming an area that is locally devoid of oxygen, making it a reducing atmosphere rather than the oxidizing atmosphere we are accustomed to!

Yeah, the majority of a fumarole system is highly reduced except where it breaches the surface. In my case though, the iron(II) salt I looked at was already aboveground for... maybe a few weeks, at least, fully exposed to the air.

With the sample I took, the iron salts only began to precipitate after I neutralized the acid component with copper hydroxycarbonate.

Fumarole_shop.png - 778kB Ground_salts.png - 1.1MB




View user's profile Visit user's homepage View All Posts By User
SnailsAttack
Hazard to Others
***




Posts: 175
Registered: 7-2-2022
Location: The bottom of Lake Ontario
Member Is Offline


[*] posted on 27-2-2023 at 06:22


Maybe the oxidation of iron(II) salts proceeds through iron(II) hydroxide (more abundant in absence of acids due to hydrolysis) rather than the direct oxidation of the iron(II) salt itself.

FeSO₄(aq) + 2H₂O(l) <-> Fe(OH)₂(aq) + H₂SO₄(aq)

4Fe(OH)₂(aq) + O₂(aq) -> 4FeO(OH)(s) + 2H₂O(l)

2FeO(OH)(s) + 3H₂SO₄(aq) -> Fe₂(SO₄)₃(aq) + 4H₂O(l)

Net reaction:
12FeSO₄(aq) + 2H₂O(l) + 3O₂(aq) -> 4Fe₂(SO₄)₃(aq) + 4FeO(OH)(s)

Iron(II) hydroxide does appear to oxidize almost immediately in air, so I think this would make sense.

Note that basic sulphate species (e.g. 'Fe(OH)SO₄') may also be present according to some sources.

[Edited on 2/27/2023 by SnailsAttack]




View user's profile Visit user's homepage View All Posts By User