Titanium nitrate synthesis
I want to prepare Titanium nitrate tetrahydrate using titanium oxide
Pls help me ! I have tried it conc. Nitric acid but im not sure how much titanium nitrate has form pls help
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by mohd jalal  | I want to prepare Titanium nitrate tetrahydrate using titanium oxide
Pls help me ! I have tried it conc. Nitric acid but im not sure how much titanium nitrate has form pls help |
Most commercial TiO2 grades are completely insoluble in nitric acid, regardless of concentration or temperature of the acid.
Titanyl sulphate - (TiO)SO4 - can be obtained by fusing TiO2 with NaHSO4 (anh). Ti(+4) compounds in water are always
titanyl compounds.
Ti powder dissolves fairly well in hot HCl (37 w%) or hot H2SO4 (50 w%) to form the respective deep blue Ti(+3) salts.
Ti powder with nitric acid forms insoluble TiO2.
|
|
|