[*] posted on 10-1-2017 at 15:50


Could be useful for loading charges, but probably not for the manufacture itself. Kneading it is bound to reintroduce air, so wouldn't any increase in density is lost unless you handle the product very deliberately with a minimum of reshaping?



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
Dornier 335A
Hazard to Others
***




Posts: 231
Registered: 10-5-2013
Location: Northern Europe
Member Is Offline

Mood: No Mood

[*] posted on 10-1-2017 at 15:51


The data was calculated with a rather simple (only 1000 lines of code...) program of mine. It guesses the reaction, calculates temperature and finally other detonation parameters using a few empirical equations. It has surprising accuracy, almost approaching that of expensive programs like EXPLO5. A complete JCZ3 implementation is on its way though...

Anyway, at 40% wax (OB = -146%) the VoD is calculated to 5450 m/s and P to 132 kbar at 1.28 g/cm3. More than that and the temperature starts to drop too low for my model.
View user's profile Visit user's homepage View All Posts By User
DubaiAmateurRocketry
National Hazard
****




Posts: 841
Registered: 10-5-2013
Location: LA, CA, USA
Member Is Offline

Mood: In research

[*] posted on 11-1-2017 at 00:27


dornier you havent posted a video in a while ;)
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 11-1-2017 at 09:52


Quote: Originally posted by Bert  
Having seen vacuum degassing used to eliminate or at least minimize bubbles and voids when casting composite rocket fuel grains, I wonder if anyone has tried adapting vacuum processing to plastic explosive manufacture?

This would be indeed an effective way to reduce the air incorporation...but the all kneeding system must be under vaccuum.

Since following the perfect gas law: p*V=n*R*T
--> then reducing the pressure will proportionnally reduce the quantity of air incorporated.

If 10% air is incorporated into a normal process at ambiant pressure; then into identical conditions but the pressure, reducing the pressure by 2, 5 or 10 will reduce the air incorporation to 5%, 2% or 1% respectively (vs the initial 10%).

Theorically if pressure can be set to 0 mm Hg (or close because 0 is unreachable) then the air incorporation will be negligible.

Practically of course one has to work with non/least volatile HE, plasticizer and oils...considering the fact any solid has a vapour pressure...lowering the overal pressure will increase the apparent/relative volatility of all the ingredients: so even PETN or ETN may start to sublime from the kneeder compartiment to other unsuitable parts of the system and reduce the % of ingredients of the kneeded mass based on their respective vapour pressure.




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 11-1-2017 at 09:56


Quote: Originally posted by Dornier 335A  
The data was calculated with a rather simple (only 1000 lines of code...) program of mine. It guesses the reaction, calculates temperature and finally other detonation parameters using a few empirical equations. It has surprising accuracy, almost approaching that of expensive programs like EXPLO5. A complete JCZ3 implementation is on its way though...

Anyway, at 40% wax (OB = -146%) the VoD is calculated to 5450 m/s and P to 132 kbar at 1.28 g/cm3. More than that and the temperature starts to drop too low for my model.

Nice program and project. Thank you for the calculation at 40% wax.

Sadly I don't have such programming abilities (although I understand the concept behind code lines and iterative calculations), so I work more on feeling, raw datas comparison and extrapolation from graphics.

But as I can see, I'm not too bad since it took me less than 1 minute to guestimate/extrapolate the VOD and pressure at 40% wax ;):P

I wish that one day you will do like Engager and let the forum benefit from your ingenious calculation program.

[Edited on 11-1-2017 by PHILOU Zrealone]




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1045
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2017 at 10:03


Some nagging thoughts I have had for a while.

I don't know chemistry well enough to answer this, but is there any other plastizer options that can get the job done with only 1-3% inerts?

Or another option that I have confidence in, increase the grain size so less inerts are needed, like this...

https://www.walmart.com/ip/Educational-Insights-Play-Foam-Co...

View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1045
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2017 at 10:04


I have played with this product (children's toy) and the air gaps can be compressed quite well.
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 11-1-2017 at 10:35


Quote: Originally posted by MineMan  
Some nagging thoughts I have had for a while.

I don't know chemistry well enough to answer this, but is there any other plastizer options that can get the job done with only 1-3% inerts?

Or another option that I have confidence in, increase the grain size so less inerts are needed, like this...

https://www.walmart.com/ip/Educational-Insights-Play-Foam-Co...


Everything is a matter of scale.
You may enter the field of nanomaterials if the film of plasticizer becomes too thin, it will loose part of its macroscopic properties (stretching ability, elastic ability or sticking ability) because to keep those you need to keep several molecular radius of like molecules.

You are right that increasing the particle size will reduce the surface of particle to coat with the plasticizer (active surface will be less) and thus the quantity of it...
but it may:
1°) become less kneedable (increased viscosity)
2°) become more breakable.
3°) become more sensitive because the weakest link remains the large crystals of HE (ETN, RDX and HMX for example)
--> To test.

Sole alternative would be to foccus on active binders/plasticizers...that are dense and contribute to the explosive properties.
--> Nitrocellulose and non volatile explosive gellifiers for example.
--> Other known technical compounds, glycidyl azide/ nitrate polymers, ...
--> Other unknown polymeric compounds (I have a lot of ideas because polymers usually induce higher densities and better stability (heat and shock) than monomers)




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
greenlight
National Hazard
****




Posts: 765
Registered: 3-11-2014
Member Is Offline

Mood: Energetic

[*] posted on 11-1-2017 at 10:42


I don't think its possible to get a moldable plastic explosive with <3% inerts. The lowest I have seen is C4 with 9% inerts.
All the new explosives testing seems to be focusing on PBX's which are bonded with a plastic polymer and have as little as 5% inerts.

Large grain size would be hard to obtain and they would probably get broken down in size a lot while incorporating the binder with rolling and kneading.
It looks like that playfoam is small rubber balls coated in some sort of binder that makes them stick to each other so I am guessing air gaps would be a problem.





View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1045
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2017 at 10:48


Philou,

To avoid the sensitivity problem I was going to form large grains from small crystals with smokeless powder and acetone. TACP if a perfect candidate because of the small crystals, low sensitivity and positive OB! The children's product is quite mold able, maybe I can dissolve that in acetone... but the foam might dissolve also...

Laboratory of Liptakov... this could be your claim to fame! I want to experiment with this but I can not find any PIB tape in the US...

And Dornier, I am legitimately jealous of you, remember me when you go places ...and when you are a chief engineer....
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 11-1-2017 at 12:53


Quote: Originally posted by MineMan  
Philou,

To avoid the sensitivity problem I was going to form large grains from small crystals with smokeless powder and acetone. TACP if a perfect candidate because of the small crystals, low sensitivity and positive OB! The children's product is quite mold able, maybe I can dissolve that in acetone... but the foam might dissolve also...

Laboratory of Liptakov... this could be your claim to fame! I want to experiment with this but I can not find any PIB tape in the US...

Beware that the TACuP may be storage inadvisable into contact with smokeless powder and/or aceton.
TACuP is a complex of NH3 and as such the NH3 is held by the Cu(ClO4)2 but not at 100%...
so the NH3 may react:
1°) with the aceton to make aceton-imin and dark polymerisation tars (only if exposed for long)
2°) most of all, with the nitric esters to hydrolyse or amonolyse it...

The children product you referenced is said to be non-sticky. (At first I thought it was magnetic core, with rubber arround)
--> So i guess the coating is stiking to itself but not to other stuffs.
--> I wonder what it is

No PIB tape...
I'm sure bird repellent/rat glue should work just fine but you have to find the right process and order of addition of the ingredients...
--> When working at Procter&Gamble on silicon additive to allow for wrinkle resistance of clothes and easy post wash ironing...
We did make an aqueous 50% silicon solution from 80% silicon into ethanol (about 5000 cps)...allowing the 80% to fall into water resulted into immediate precipitation and hard (very viscous) plastic chewing-gum totally unworkable (>100000 cps); reversely when allowing the water to fall drop by drop into the 80% silicon ethanolic solution, despite a transitory moderate increase of viscosity (not unworkable at all 15000), we ended up with a very thin liquid only 10 centipoise (thus about 10 times as viscous as water) composed of sub-micron-sized silicon beads into a water-ethanol mix.

[Edited on 11-1-2017 by PHILOU Zrealone]




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 13-1-2017 at 10:01


No PIB tape #2

This is a question I've been asking myself everytime someone said that they cant find PIB:
Why dont you guys try to get it from somewhere else ?

Gloves first come to mind. You all have rubber gloves right?
And for those living in the land of the chewing gum and Ford you probably can find some chewing gum at your local convenience store.
Or go tear some tires to get at the bladder that holds the air.
Dont cut your gasmask to pieces though ;)

It probably is as easy to get PIB from those sources as from bird/rat traps.
Am I failing to see something?
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 13-1-2017 at 11:29


Quote: Originally posted by Herr Haber  
No PIB tape #2

This is a question I've been asking myself everytime someone said that they cant find PIB:
Why dont you guys try to get it from somewhere else ?

Gloves first come to mind. You all have rubber gloves right?
And for those living in the land of the chewing gum and Ford you probably can find some chewing gum at your local convenience store.
Or go tear some tires to get at the bladder that holds the air.
Dont cut your gasmask to pieces though ;)

It probably is as easy to get PIB from those sources as from bird/rat traps.
Am I failing to see something?

Bird/Rat glue I have bought is only PIB (90-80%) and solvent like hexane (10-20% by weight) nothing else...for 2,5-3,5€/100 g into brico shop...you can't hardly make it easier to get.
The product is also immediately mixable as such with mineral oil or organic solvent.

I was also thinking to chewing-gum (after use/chewing so you get rid of most sugar, aroma) or to Multi-fix by Pritt/Henkel for Poster (glue/paste without solvent containing Polybuten but with a mineral charge).




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
Hennig Brand
International Hazard
*****




Posts: 1284
Registered: 7-6-2009
Member Is Offline

Mood: No Mood

[*] posted on 23-1-2017 at 20:37


I haven't done anything HE related in about a year probably, but,

I never accurately measured the crystal density of the solid HE used or the density of the polymer it was mixed with to form a plastic/putty type explosive. However, using the published data for densities of both and calculating an average density based on proportions used always came out to very, very, close to the product density found using good scales to determine mass and a decent graduated cylinder and careful volume measurement using the water displacement method.

From what I saw, more kneading generally resulted in a density closer to what the calculated average density was. I have not used the solvent method in a while. I settled on bird repellent (91% PB IIRC, I looked for the highest percentage I could find) and mineral oil. I use a bit of heat (a previously heated, with hot water to ca. 50C, then insulated to slow heat loss, rolling board, glass cutting board for instance) and a glass rolling pin (can be bought for baking, there are also really light (not glass) Teflon coated rolling pins that would likely work really well, or even just a suitable glass bottle).

If I had air in most of my putty explosives, when well kneaded, it was a very small amount (I think).

BTW, good to read some of what you characters are writing about and see what you are up to again. :) I have actually been tied up lately applying some of my science & engineering skill to an R & D project where we are making synthetic diesel from wood.


[Edited on 24-1-2017 by Hennig Brand]




"A risk-free world is a very dull world, one from which we are apt to learn little of consequence." -Geerat Vermeij
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1453
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 24-1-2017 at 06:35
diesel from wood


:oMaking synthetic diesel from wood is my dream for all life. ......:cool:



Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1045
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 24-1-2017 at 13:04


I thought the bird repellent was not that good because it is a short molecular chain as LL stated.

It is hard to beat the ease of NM and Nitrocellulose. Are there any agents that would slow down the NM evaporation? Petroleum jelly helps, but it seems a high amount is needed, which resulted in no detonation....
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1453
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 24-1-2017 at 13:14


Camphor is pretty available, solid material and soluble in esters. Next is possibility use microtene bag.



Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 24-1-2017 at 14:27


NM with NC is a bit like using MN (Methyl nitrate) with NC.
Better use EGDN or NG with ETN and NC instead.

Or the more exotic 1,2-dinitroethan ...denser, less volatile, but less available and harder to do.




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 940
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 25-1-2017 at 13:48


Concerning inert binder/plasticizer systems, and trouble with finding PIB:

I am presently conducting a series of experiments on a silicone (poly-dimethylsiloxane) system. It consists of curable silicone rubber caulking for construction (the kind you buy for DIY projects) and silicone oil (bought the same places for lubricating rubber seals and such, or at the pharmacy for lubricating... different things). It produces a mouldable product with superior mechanical properties at about 85 % inerts and seems quite forgiving of variations in the binder/plasticizer ratio (in a range around the 50/50 mark). 85 % active ingredients seems low, but bear in mind that silicone has a higher density than PIB/diester. If you compute the volume fraction of inerts, it is actually quite close to the value obtained for C4.
At present, I have only tried it with a non-energetic filler, in order to investigate the mechanical properties and behaviour after prolonged storage (I'm at the 2 month mark tomorrow, and so far there has been no change).
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1453
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 26-1-2017 at 00:18
silicone plasticizer


Plasticizer on silicone based, poly-dimethylsiloxan oil + classic transparent silicone rubber. Results after 30 minute preparation. By 60 Celsius.

PLF.jpg - 231kB
........:cool:.........LL




Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 940
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 27-1-2017 at 14:39


today I heated a sample of the inert plastique at 85 C for 3 hours to see if I could replicate your results. However, in my case, the sample did not exhibit any signs of change in the physical properties. The kind of transparent silicone rubber I used was neutral curing (no smell of vinegar), how about yours? Also, did you use any solvents in the preparation?
View user's profile View All Posts By User
Uriel
Harmless
*




Posts: 14
Registered: 28-1-2017
Member Is Offline

Mood: No Mood

[*] posted on 28-1-2017 at 14:12


Hello guys !
(it's my first message on this forum)
I've made research in plastic ETN.
- Motor Oil + ETN 25/75 it quitte good (23 or 24% are too few and 24 at 30 are perfect... but less powerfull of course)
- 9 Motor Oil + 1 Lecithine plastizer, about 17/18% with ETN give a plastic but that flows. Under it is powder, over it's flowing... (but good density).
- PIB/PB (rat glue and I don't know de proportions of each) 14/15% is quite good : there is my video here :
https://www.youtube.com/watch?v=s3K67Cqzm-I

- And about 11%PIB + 4% motor oil is such good and density is better !
- I've found that the PIB can be mix under water, so, I've put ETN/Water and PIB and it's quite easy to knead, it is the method of the real C4. I let drys many days. The density is a little better. (So better detonation pressure).
I'm pretty proud of myself on this development ;-)

For the moment, my conclusion is : if you haven't PIB you can use motor oil at about 25% (and less if you can use some Lecithine but the adhesion falls and the plastic can flow)
If you can have PIB : about 15% is a good compromise but the density is not perfect, because there are tiny air zones (but can be improved by adding oil, like 11%PIB + 4% oil).
I'll probably make a video of standard tests in the future.




[Edited on 28-1-2017 by Uriel]
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1453
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 28-1-2017 at 15:32
plastic


Good attempt. Hardcore video. Your plate I estimate on 8 mm. But 30 grams a High Quality brizant plastic, should by making this:


brz.jpg - 13kB
And middle quality homemade should by making hole 10 mm.




Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User
Uriel
Harmless
*




Posts: 14
Registered: 28-1-2017
Member Is Offline

Mood: No Mood

[*] posted on 19-3-2017 at 12:25


Hello guys !

I've made the tests !
My two plastic contains about 14% PIB by mass.
I wanted to compare ETN plastic with PETN plastic to have an idea.
As the ETN cristals are biggers, the density of ETN is quite lowest.
As ETN cristals had a density of 1.827 (1.6 is for liquid) against 1.77 for PETN, I was hoping to reach better density, but no.
I've reach a density of 1.32 for ETN and 1.36 for PETN (37mm high and 35.5/36mm for PETN)

30g in both charge with plasticizer additional.

IMGP3635.JPG - 510kB IMGP3639.JPG - 478kB IMGP3641.JPG - 490kB IMGP3643.JPG - 486kB IMGP3646.JPG - 486kB

As you can guess, the first one, the weakest, is ETN ans the most brisant is PETN.
Both are in the same tube of paper of exactly 30mm internal.
(And the steel plate is 10x40mm of section).





[Edited on 19-3-2017 by Uriel]
View user's profile View All Posts By User
 Pages:  1    3

  Go To Top