Electrolytic aluminum powder?
I was thinking if the electrolysis of a weak acid salt of aluminum like aluminum acetate can yield aluminum powder, but i was thinking that the water
can react further with the nano aluminium powder to make aluminum hydroxide. If this happens, can aluminum acetate disolved in some solvent like
ethanol
yield aluminum powder?
I can make a good amount of aluminum acetate from calcium acetate and aluminum sulfate.
Pd : I have a ball mill and i use it to make aluminum powder , but if this method works it would be much better because the aluminum is not cast and
will have a very small particle size , without the need of milling it.
And about the electrodes , i think that graphite cathode/anode will work.
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
To my knowledge, only group 1 metals form hydroxides in contact with water. Iron powder in water will produce iron oxide (rust). The same is likely
to occur with Al, with the formation of Al2O3.
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
ch3misc00l
Harmless
Posts: 16
Registered: 8-10-2015
Location: Costa Rica
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Detonationology  | | To my knowledge, only group 1 metals form hydroxides in contact with water. Iron powder in water will produce iron oxide (rust). The same is likely
to occur with Al, with the formation of Al2O3. |
And if i use ethanol/ some solvent in which aluminum acetate is soluble? I know that aluminum triethoxide exists , but it only forms when
aluminum-mercury amalgam reacts with ethanol , or boiling ethanol with aluminum powder and aluminum chloride, but i think that the ethanol will serve
as an inert solvent here.
[Edited on 28-1-2016 by ch3misc00l]
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
I am not sure I follow 100%, but if you are asking what I believe you are, electrolysis cannot be preformed in pure alcohols because they are
non-electrolytes. If you are familiar with aluminum powder, you are probably also aware of "dark aluminum powder." The reason it is dark is because
charcoal is added to cover the aluminum and protect it from oxidizing. Oxidation is the biggest issue when it comes to making fine metal powders.
That's why charcoal is typically added during the ball milling process. It is likely that if very finely powdered aluminum wasn't covered in charcoal,
that it could prove to be pyrophoric
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
ch3misc00l
Harmless
Posts: 16
Registered: 8-10-2015
Location: Costa Rica
Member Is Offline
Mood: No Mood
|
|
Yes , i know that aluminum powder needs to be coated in charcoal to increase reactivity and lower its unstability. I have made fine aluminum powder
without charcoal with no accidents using ceramic grinding media , but the stuff is scary , and it can be light with just a spark from a lighter, and
it can burn spontaneously . I was so lucky that doesn't happened to me, and it was the first time i made aluminum powder. I heared of a lot of
accidents and dust explosions involving pure non charcoal-coated aluminum powder.
In resume, better i search another method of making aluminum powder or upgrade my tiny ball mill 
[Edited on 28-1-2016 by ch3misc00l]
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
Sorry, I didn't mean to insult your intelligence, I was just reiterating the reactivity of aluminum powder.
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
ch3misc00l
Harmless
Posts: 16
Registered: 8-10-2015
Location: Costa Rica
Member Is Offline
Mood: No Mood
|
|
No , i was wrong about this , i am beginner at chemistry , don't worry. But i will continue researching , maybe i found something interesting.
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Detonationology  | That's why charcoal is typically added during the ball milling process. It is likely that if very finely powdered aluminum wasn't covered in charcoal,
that it could prove to be pyrophoric |
No. Carbon-free Al powders are very common. Al passivates in air immediately and isn't pyrophoric in the slightest.
https://en.wikipedia.org/wiki/Passivation_(chemistry)#Aluminium
It's also extremely hard to make it burn, for the same reason.
Electro-deposition of electro-positive metals like Al from water is basically impossible. So Al powder can't be produced electrolytically, from
aqueous solutions.
|
|
|
ch3misc00l
Harmless
Posts: 16
Registered: 8-10-2015
Location: Costa Rica
Member Is Offline
Mood: No Mood
|
|
I am still thinking that some water-free solvent in which an aluminum salt is soluble , when electrolysed will produce aluminum powder. Also aluminum
isopropoxide electrolysis could produce aluminum powder, but it would be impractical due to aluminum isopropoxide rare availability and expensiveness.
[Edited on 28-1-2016 by ch3misc00l]
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by ch3misc00l  | I am still thinking that some water-free solvent in which an aluminum salt is soluble , will produce aluminum powder. Also aluminum isopropoxide
electrolysis could produce aluminum powder, but it would be impractical due to aluminum isopropoxide rare availability and expensiveness.
[Edited on 28-1-2016 by ch3misc00l] |
Good luck. A $1000 tells me you won't succeed were so many have failed before. Al isopropoxide isn't even a real salt: MP about 140 C!
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
Solid pieces or sheets of aluminum are indeed capable of passivation; however, metal powders under 5 microns tend to become more reactive. There
isn't much room for passivation when the particles are that small.
Here is some references too:
https://en.wikipedia.org/wiki/Pyrophoricity
http://cameochemicals.noaa.gov/chemical/14570
http://www.ehs.pitt.edu/assets/docs/combustible-metals.pdf
http://www.dtic.mil/dtic/tr/fulltext/u2/b270510.pdf
http://ehs.unl.edu/sop/s-pyrophoric_%26_substances.pdf
[Edited on 1-28-2016 by Detonationology]
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
ch3misc00l
Harmless
Posts: 16
Registered: 8-10-2015
Location: Costa Rica
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by blogfast25  | Quote: Originally posted by ch3misc00l  | I am still thinking that some water-free solvent in which an aluminum salt is soluble , will produce aluminum powder. Also aluminum isopropoxide
electrolysis could produce aluminum powder, but it would be impractical due to aluminum isopropoxide rare availability and expensiveness.
[Edited on 28-1-2016 by ch3misc00l] |
Good luck. A $1000 tells me you won't succeed were so many have failed before. Al isopropoxide isn't even a real salt: MP about 140 C!
|
I forgot to say , it would only work with MOLTEN aluminum isopropoxide.Molten salts are the only routes to aluminum metal as i am searching. But i
think that melting a flammable solid that reacts with water is not a good idea, and electrolyzing it would be worse. So , some organoaluminum room
temperature melting point compound could be the "safe" way to get aluminum powder without ballmilling / powderizing the metal.
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
Quote: Originally posted by blogfast25  | Al passivates in air immediately and isn't pyrophoric in the slightest.
https://en.wikipedia.org/wiki/Passivation_(chemistry)#Aluminium |
| Quote: |
Pure aluminium naturally forms a thin surface layer of aluminium oxide on contact with oxygen in the atmosphere through a process called oxidation
|
However...
Powdered aluminum...
| Quote: |
Can be ignited under almost all ambient temperature conditions.
|
| Quote: |
Finely divided metals (iron,[3] aluminium,[3] magnesium,[3] calcium, zirconium, uranium, titanium, bismuth, hafnium, thorium, osmium,
neodymium)
|
...are pyrophoric.
| Quote: |
In
finely divided powder or dust form, aluminum and its alloys are combustible in air and
present a serious combustion explosion hazard.
|
So...
| Quote: |
Please be more careful when citing, in the future. You pulled that seriously out of context.
|
[Edited on 1-28-2016 by Detonationology]
[Edited on 1-28-2016 by Detonationology]
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
deltaH
Dangerous source of unreferenced speculation
   
Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline
Mood: Heavily protonated
|
|
Aluminium metal can be deposited in a mirror form from chloroaluminates dissolved in an anhydrous choline chloride deep eutectic solvent. See
pp.13,14 in this long presentation and it's reference for more info:
https://wet.kuleuven.be/english/summerschools/ionicliquids/l...
It does not, however, produce powder... nor do I think it could be made to do so easily, yet it is interesting as an example of room temperature
electrolysis that forms aluminium metal.
I do not think that molten aluminium isopropoxide would be conductive due to lack of ionisation.
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
I don’t think it’s accurate to describe Al powder as pyrophoric in the strict sense of the word:
| Quote: | | A substance that ignites spontaneously in air at temperatures below 55 C (Celsius) |
Instead I think there’s conflation going on, leading to an inaccurate ‘reputation’:
• Pyrophoric Al compounds do exist: see alkyl aluminium
• Al powder reacts very strongly with strong oxidisers, 'burning' past the MP of alumina
• Used in fireworks
I’ve used various grades of Al powder, including some of the finest and purest, all my life. I’ve also mixed it with KClO3,
KNO3, NaNO3, S and even KClO3 + S, without the slightest incident.
With something like MnO2 you get close to a flash powder but not without heating it strongly (igniting with hot source). And smooth running
MnO2 thermite formulations I’ve also created (with CaF2 or CaO).
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
Somebody should go to and tell those 3 sources I posted that they have been publishing false info.
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
For one, I didn't say 'false', I said inaccurate. They're not the same thing.
And Al compounds do not equate to Al powder.
Much as I use and respect, e.g. Wikipedia, it's full of errors and poor cut'n paste jobs. Not everything you read on the Net is true. And not
everything you read should be taken literally.
[Edited on 28-1-2016 by blogfast25]
|
|
|
ch3misc00l
Harmless
Posts: 16
Registered: 8-10-2015
Location: Costa Rica
Member Is Offline
Mood: No Mood
|
|
http://www.materialstoday.com/metal-finishing/features/depos...
Interesting..
|
|
|