liquidlightning
Hazard to Self
**




Posts: 66
Registered: 10-5-2012
Location: Washington
Member Is Offline

Mood: Witty

[*] posted on 16-9-2012 at 12:21
Platinized Asbestos


I just got a 10 grams of platinized asbestos. Know of anything interesting I can do with it? 5% Platinum, looks like steel wool. It is definitely real, it ignites my butane torch.

[Edited on 16-9-2012 by liquidlightning]
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3849
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 16-9-2012 at 12:34


You could use it to oxidise SO<sub>2</sub> and prepare oleum!
View user's profile View All Posts By User
Lambda-Eyde
International Hazard
*****




Posts: 855
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 16-9-2012 at 12:44


You could, but Pt is easily poisoned. Vanadium pentoxide catalyst is a better choice for that reaction and also should be quite interesting to prepare. See Fleakers thread on oleum. Preparation of SO<sub>3</sub> is not something to be taken lightly and should under no circumstances be done without a fume hood.



This just in: 95,5 % of the world population lives outside the USA
You should really listen to ABBA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
View user's profile View All Posts By User This user has MSN Messenger
Endimion17
International Hazard
*****




Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline

Mood: speeding through time at the rate of 1 second per second

[*] posted on 16-9-2012 at 13:40


Quote: Originally posted by Lambda-Eyde  
You could, but Pt is easily poisoned. Vanadium pentoxide catalyst is a better choice for that reaction and also should be quite interesting to prepare. See Fleakers thread on oleum. Preparation of SO<sub>3</sub> is not something to be taken lightly and should under no circumstances be done without a fume hood.


It's not a nerve gas, for god sake. Pretty much anything can be done withoud a fume hood, if the apparatus is properly designed and assembled, and if the excess gasses are being taken care of properly by series of tubes leading outside.

Now, if someone is working with soda bottles and drinking glasses, it's easy to get poisoned. If one uses old fashioned corks and bungs, the poisoning is less likely, but if one has a ground glass joint apparatus with Keck clips and joint lubrication, nothing happens.

Sulphur trioxide can be readily condensed and solidified, and excess sulphur dioxide can leave the apparatus through a tube.
There are way more dangerous experiments people do. SO3 synthesis is not one of them.




View user's profile Visit user's homepage View All Posts By User
plante1999
International Hazard
*****




Posts: 1937
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 16-9-2012 at 13:55


Few days ago I also received 10g of 5% platinized asbestos. Many use can be mane from it but its mostly good for oxidation reaction. I'm also working on something pretty interesting that should be revealed in a month or two.



I never asked for this.
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1248
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 16-9-2012 at 14:10


Make nitric acid via the ostwald process?



-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1937
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 16-9-2012 at 14:25


Quote: Originally posted by phlogiston  
Make nitric acid via the ostwald process?
Ok I'm a bit obligated to reveal the project I'm working on. I started it a month ago I already made some experimenting with the Ostwald process but I do not have anymore ammonia (the reason for the post I need ammonia fast). At the time the process is very successful.

Here a picture of my setup:
The right bottle is for ammonia and the upper tube for air. The tube can be lowered or raised to increase or decrease ammonia concentration as such it act as a carburetor. then there is the catalyst tube and tree water absorption bottle. the last tube is for gas analysis, air is used in excess. The reason for this is that when the nitrogen dioxide dissolve in water it make nitrogen monoxide, the monoxide is oxidized with the excess air in upper of the absorption bottle and is ready for next absorption bottle.

.

[Edited on 16-9-2012 by plante1999]




I never asked for this.
View user's profile View All Posts By User
liquidlightning
Hazard to Self
**




Posts: 66
Registered: 10-5-2012
Location: Washington
Member Is Offline

Mood: Witty

[*] posted on 16-9-2012 at 14:31


That's pretty interesting, do you heat the catalyst tube?
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1937
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 16-9-2012 at 14:38


I do but only for starting an ammonia poor air combustion, then the catalyst glow dull red from the oxidation reaction, but I can also use ammonia rich gas then the catalyst automatically become yellow-white, and then I lower the ammonia concentration. Ammonia rich gas mix make mostly nitrogen but ammonia poor make a lot of nitrogen oxides.



I never asked for this.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2012 at 15:11


I'll be interested to see what yields you're able to get without the higher temperatures and pressures that are used industrially.

Also, cobalt oxide has come into use as a catalyst in the Ostwald process. It was the result of a lot of effort to find a cheaper catalyst than platinum.
View user's profile View All Posts By User
Lambda-Eyde
International Hazard
*****




Posts: 855
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 16-9-2012 at 16:14


Endimion, I think you are underestimating the power of Murphy's Law. And the health effects of SO<sub>3</sub>. From GC's thread:
Quote: Originally posted by garage chemist  

If you choose to make SO3, please make yourself aware of the dangers of this substance first.
The warning "Extremely corrosive" does not really express the dangers appropriately. Oleum destroys many plastics, like PE and PP, that are completely resistant to 98% H2SO4- only glass and fluoropolymers like PTFE are really safe.

The reaction of SO3 with water is explosively violent. SO3 must only be diluted with concentrated H2SO4!

SO3 and Oleum also create an extremely dense fog when handled in open air, due to reaction of gaseous SO3 with aerial moisture forming droplets of H2SO4. If using a fume hood, be aware that all this thick fog will come out the exhaust! Most filters are incapable of precipitating H2SO4 fogs!


And Fleaker's thread on the V<sub>2</sub>O<sub>5</sub>-catalyzed method:
Quote: Originally posted by Fleaker  
[...] It also requires high temperatures and is hazardous as well. Sulfur trioxide is extremely aggressive at high temperatures and will attack most all things organic. It forms thick, corrosive acid fogs that can blind or cause pulmonary edema.


Quote: Originally posted by Endimion17  

It's not a nerve gas, for god sake. Pretty much anything can be done withoud a fume hood, if the apparatus is properly designed and assembled, and if the excess gasses are being taken care of properly by series of tubes leading outside.

What will you do when one of the tubes begins to leak? A seal fails? A bubbler clogs? A flask breaks? Reaction gets out of hand? How will you transfer SO<sub>3</sub>/oleum outside of a fume hood without breathing in a cloud of an extremely corrosive gas? A fume hood isn't a replacement for good apparatus design and offgas handling, it's a failsafe for when (not if) things go wrong!

Quote: Originally posted by Endimion17  
Now, if someone is working with soda bottles and drinking glasses, it's easy to get poisoned. If one uses old fashioned corks and bungs, the poisoning is less likely, but if one has a ground glass joint apparatus with Keck clips and joint lubrication, nothing happens.

People working with soda bottles, drinking glasses, mason jars and caulk shouldn't be involved in amateur chemistry in the first place. If you're not willing to spend money on real lab equipment you are trading away your safety. It's not about being able to afford it, it's about priorities.

Quote: Originally posted by Endimion17  
Sulphur trioxide can be readily condensed and solidified, and excess sulphur dioxide can leave the apparatus through a tube.

Solid sulfur trioxide is still very volatile, producing mists of sulfuric acid.

Quote: Originally posted by Endimion17  
There are way more dangerous experiments people do. SO3 synthesis is not one of them.

I beg to differ. The syntheses of sulfur trioxide I have seen here on SM are among the most dangerous ones as well, together with preparation and distillation of bromine and the phosphorus halides. Of course, I haven't read all the posts on the board and my memory may fail me, so please show me something that you think deserves the title of "dangerous" more than SO<sub>3</sub>.

Quote: Originally posted by watson.fawkes  

Also, cobalt oxide has come into use as a catalyst in the Ostwald process. It was the result of a lot of effort to find a cheaper catalyst than platinum.

Do you have any more info on this? Specifically, which cobalt oxide, any special way of preparing it, other potential uses as a catalyst etc.? I would appreciate it.

And plante, your project sounds interesting. I expect a report in Prepublications when you're done, I bet it will be an interesting read. ;)




This just in: 95,5 % of the world population lives outside the USA
You should really listen to ABBA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
View user's profile View All Posts By User This user has MSN Messenger
cyanureeves
International Hazard
*****




Posts: 722
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2012 at 16:51


interesting plante, now if you put glowing charcoals instead of that wool you got there then you could produce hydrogen cyanide couldn't you? how much heat can those stoppers take? did you bend your own glass? are you saying that the platinum catalyst automatically glows and creates heat? or does it just change colors in the presence of ammonia? do you need ammonium nitrate and sodium hydroxide to create the ammonia gas or will 20% plus ammonium hydroxide work? how are you gonna keep the ammonia from pulling air towards it instead of pushing out?

[Edited on 17-9-2012 by cyanureeves]
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1937
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 17-9-2012 at 02:32


I know that carbon monoxide and ammonia on platinized asbestos wool form hydrogen cyanide, so I guess a good calculated ammonia/air ratio passed on charcoal and then on platinized asbestos it should work too. Yes I have bend these myself, and the catalyst tube is made from a test tube with a cut bottom. The stoppers can take about 200 degree Celsius but the gas mix cool down quite fast and I don'T have any problem with them. The platinum become very hot because the oxidation of ammonia occur on its surface and oxidation reaction release energy. At the time I have used 30% ammonia and it work very well. In fact I use an air pump on the right tube and ammonia cannot overcome the pressure of the pump. (The pump is not in the picture).



I never asked for this.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 17-9-2012 at 03:03


Quote: Originally posted by Lambda-Eyde  
Specifically, which cobalt oxide, any special way of preparing it, other potential uses as a catalyst etc.?
I did a fair bit of reading on this a few years ago, but all my notes are on a computer that's half-broken. I found it looking at patent literature. One such (first patent link on search) is US3962138 Cobalt-oxide-based catalytic substances for the oxidation of ammonia. The keywords for searching are "cobalt oxide", "ammonia", and "catalytic oxidation". One of the reasons I asked about yield was that a theme of this literature is the possibility of oxidizing ammonia all the way to N2. This isn't just a theoretical catalyst; as of the time of my reading, the first production plant using this catalyst had gone live, in Canada as I recall.
View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10334
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 17-9-2012 at 10:19


Interesting Plante. What's the source of ammonia?



View user's profile Visit user's homepage View All Posts By User
Endimion17
International Hazard
*****




Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline

Mood: speeding through time at the rate of 1 second per second

[*] posted on 17-9-2012 at 11:57


Quote: Originally posted by Lambda-Eyde  
Endimion, I think you are underestimating the power of Murphy's Law. And the health effects of SO<sub>3</sub>.

What will you do when one of the tubes begins to leak? A seal fails? A bubbler clogs? A flask breaks? Reaction gets out of hand? How will you transfer SO<sub>3</sub>/oleum outside of a fume hood without breathing in a cloud of an extremely corrosive gas? A fume hood isn't a replacement for good apparatus design and offgas handling, it's a failsafe for when (not if) things go wrong!


You can work by an open window with a fan. Why, for god sake, would synthesis of SO3 be limited with people who own a whole fume hood? It's a huge, expensive overkill that can be avoided if one knows good alternatives. Anyone who doesn't shouldn't perform this at the first place! It's not like anyone is going to make liters of it. We're talking about small apparatus here.
Tubes should be inspected before doing an experiment. Ground glass joint seals don't fail like corks. Bubblers don't clog because of nonprecipitating reactions. Annealed flasks without cracks don't burst for no reason. SO3 synthesis can't get out of hand. We are not talking about reactions in liquid medium stored in reaction vessels that need to be constantly stirred and cooled down. This is mixing of two gases over a catalyst and passing that through a cooled vessel. There is no possibility of a runaway reaction here. You're exaggerating.


Quote:
People working with soda bottles, drinking glasses, mason jars and caulk shouldn't be involved in amateur chemistry in the first place. If you're not willing to spend money on real lab equipment you are trading away your safety. It's not about being able to afford it, it's about priorities.


I don't agree. You can do amateur chemistry without expensive equipment, but you have to know the limits. If your equipment is based on bottles and jars, pretty much every synthesis is unreachable, but you can nevertheless have a great time if you're just starting.
I don't know, maybe you were one of those rare, lucky kids who got a ground glass joint equipment as a kid. I didn't. It was before the era of online markets and I was a poor little fuck. I had to work my way up, starting with shitty equipment and shitty experiments, gradually turning to cored corks and rubber bungs. Today I own custom made ground glass joint equipment, tailored for my needs. Unfortunately, now I lack the time to do everything I want, but that's a different story.


Quote:
Solid sulfur trioxide is still very volatile, producing mists of sulfuric acid.


And it stays in the apparatus.

Quote:
I beg to differ. The syntheses of sulfur trioxide I have seen here on SM are among the most dangerous ones as well, together with preparation and distillation of bromine and the phosphorus halides. Of course, I haven't read all the posts on the board and my memory may fail me, so please show me something that you think deserves the title of "dangerous" more than SO<sub>3</sub>.


I did all that without a fume hood without getting poisoned even slightly. I worked by an open window equipped with a fan, and I had few tubes going outside. If I haven't chased away my cat, it would look at me sitting on the shelf, not giving a fuck about the traces of smell.

More dangerous? Isolation of alkali metals using electrolysis of their molten salts, synthesis of mercury salts, synthesis of all kinds of sensitive, explosive compounds, synthesis of volatile organic compounds with high acute toxicity, just to name few.
Sulphur trioxide is a little cub if tamed in an apparatus. If a tiny plume of oleum escapes and drifts through the room, it's nothing compared to getting mercury salt somewhere on your skin or floor, ready to be stepped on and carried into the kitchen.

Of course SO3 will turn into a cruel beast if you smash the apparatus, but hey... A car could kill you tomorrow even if you're on a sidewalk. Will that make you walk around in a large bubblewrap sphere?

[Edited on 17-9-2012 by Endimion17]




View user's profile Visit user's homepage View All Posts By User
plante1999
International Hazard
*****




Posts: 1937
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 21-9-2012 at 14:23


Quote: Originally posted by blogfast25  
Interesting Plante. What's the source of ammonia?


30% ammonia. I hop that I will be able to make some nitric acid soon. I will still have to increase the 40% acid to 68% to get a goo conc. acid since 40% is the maximum % I can get without pressure when dissolving the nitrogen oxides.




I never asked for this.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 21-9-2012 at 16:21


Quote: Originally posted by Endimion17  
SO3 synthesis can't get out of hand. We are not talking about reactions in liquid medium stored in reaction vessels that need to be constantly stirred and cooled down. This is mixing of two gases over a catalyst and passing that through a cooled vessel. There is no possibility of a runaway reaction here.
True, but also a bit misleading on what some of the actual problems are.

First some physical data. The oxidation SO2 + 1/2 O2 --> SO3 is strongly exothermic, about 100 kJ / mol SO3. The catalyst bed heats up in a contact process plant and requires explicit temperature control that includes cooling coils and dumping waste heat. (Mind you, the hydration of SO3 is also exothermic, about 130 kJ / mol SO3. Contact process plants throw off lots of process heat.) The reason for cooling the catalyst bed is that catalytic activity strongly decreases with temperature. The knee in the curve (the curvature inflection point, and near the 50% yield point) is about 950 &deg;C. The V2O5-based catalyst has to become liquid on the surface of its carrier to become active; that happens around 680 - 700 &deg;C. And then it's typical for the gas feed temperature to rise from 700 &deg;C to 900 &deg;C in one pass through the catalyst bed.

The point is that this is a lot of &Delta;T, both within the apparatus itself as well as between the apparatus and the environment. Strain in glass is directly proportional to the temperature gradient, and even well-constructed glassware will be at risk. Borosilicate glass just isn't best suited for this environment. The recommended temperature range for borosilicate glass in extreme service is only 500 &deg;C. It's softening point is around 820 &deg;C, which is possible to exceed in an exhaust gas stream, even assuming the catalyst bed is in ceramic. (Vycor would work for this, incidentally, with only a bit of care. Fused quartz wouldn't even notice.)
View user's profile View All Posts By User

  Go To Top